The modeling of epoxy polymers weathering by the color characteristics measurements

Startsev V.O., Nizina T.A.
Startsev V.O., Nizina T.A. The modeling of epoxy polymers weathering by the color characteristics measurements // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-10-10. URL: https://viam-works.ru/en/journal/2015/12/10
Keywords
epoxy polymer, weathering, color characteristics, ultraviolet.
Abstract

The epoxy polymer based on Ethal-247 resin and cycloaliphatic Ethal-45M curing agent was exposed to Gelendzhik and Saransk atmosphere. The color characteristics of the specimens were measured and it was shown that colorimetric property such as a color difference of the polymer surface is sensitive to initial stages of weathering. It was shown that the natural UV-radiation is a dominant factor for polymer degradation. The application of solar radiation doze provides more reliable results.

Reference list
  1. Chernin I.Z., Smehov F.M., Zherdev Yu.V. Epoksidnye polimery i kompozicii [Epoxy polymers and compositions]. M.: Himiya. 1982. 232 s.
  2. Berlin A.A., Volfson S.A., Oshmyan V.G., Enikolopov N.S. Principy sozdaniya kompozicionnyh polimernyh materialov [Principles of creation of composite polymeric materials]. M.: Himiya. 1990. 238 s.
  3. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy starenya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] //Deformaciya i razrushenie materialov. 2010. №11. S. 19–26.
  4. Nizina T.A. Zashhitno-dekorativnye pokrytiya na osnove epoksidnyh i akrilovyh svyazuyushhih [Decorative protective coverings on the basis of the epoxy and acrylic binding]. Saransk: Izd-vo Mordovskogo gos. un-ta. 2007. 258 s.
  5. Fairchild M.D. Color Appearance Models //Wiley. 2005. 408 p.
  6. Schanda J. Colorimetry: Understanding the CIE System //Wiley. 2007. 390 p.
  7. Sulejmanov A.M., Pomerancev A.L., Rodionova O.E. Prognozirovanie dolgovechnosti materialov proekcionnymi matematicheskimi metodami [Forecasting of durability of materials by projective mathematical methods] //Izvestiya KazGASU. 2009. №2 (12). S. 274–278.
  8. Ranby B., Rabek J.F., Photodegradation, Photo-oxidation and Photostabilization of Polymers. New York: Wiley-Interscience. 1975. 573 p.
  9. Olhov A.A., Ivanov V.B., Vlasov S.V., Iordanskij A.L. Klimaticheskoe ispytanie kompozicionnyh plenok na osnove PENP i poligidroksibutirata (PGB) [Climatic testing of composition films on the basis of PENP and poligidroksibutirata (PGB)] //Plasticheskie massy. 1998. №6. S. 19–23.
  10. Startsev O.V. Polymer Yearbook 11 /Ed. вy R.A. Pethrick. Glasgow: Harwood Academic Publishers. 1993. P. 91–109.
  11. Startsev O.V., Cincadze G.B., Vapirov Yu.M., Kiryushkin S.G. Polimernye opticheskie materialy [Polymeric optical materials]. Chernogolovka: IHF AN SSSR. 1989. S. 152–177.
  12. Startsev O.V., Krotov A.S., Golub P.D. Effect of Climatic and Radiation Ageing on Properties of Glass Fibre Reinforced Epoxy Laminates //Polymers and Polymer Composites. 1998. V. 6. №7. P. 481–488.
  13. Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PKM] //Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  14. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  15. Startsev O.V., Medvedev I.M., Kurs M.G. Tverdost kak indikator korrozii alyuminievyh splavov v morskih usloviyah [Hardness as the indicator of corrosion of aluminum alloys in sea conditions] //Aviacionnye materialy i tehnologii. 2012. №3. S. 16–19.
  16. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coal plastics and fibre glasses of new generation] //Trudy VIAM. 2013. №4. St. 09 (viam-works.ru).
  17. Titareva A.S., Kirillov V.N., Startsev O.V. Povedenie materialov v elementah konstrukcij aviacionnoj tehniki, izgotovlennyh s primeneniem PKM i sistem LKP v usloviyah umerenno teplogo klimata [Behavior of materials in structural components of aeronautical engineering, manufactured using PCM and PC systems under conditions of temperate thermal climate] //Aviacionnye materialy i tehnologii. 2013. №S2. S. 81–85.
  18. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  19. Stolyankov Yu.V., Ishodzhanova I.V., Antyufeeva N.V. K voprosu o defektah obrazcov dlya ispytanij ugleplastikov [On the question of carbon fiber reinforced plastics (CFRP) test specimen flaws] //Trudy VIAM. 2014. №10. St. 10 (viam-works.ru).