Insulating enamel coatings for modern electronics

Solncev S.St., Solovyova G.A., Denisova V.S.
Solncev S.St., Solovyova G.A., Denisova V.S. Insulating enamel coatings for modern electronics // Proceedings of VIAM. 2014. No. 9. DOI: 10.18577/2307-6046-2014-0-9-8-8. URL: https://viam-works.ru/en/journal/2014/9/8
Abstract

Possibility of development of insulating enamel coatings for substrates based on glass and ceramics is shown. The optimum compositions of insulating enamel coatings in phosphate and zinc borosilicate glass forming systems are chosen. Tests of chemical resistance have showed a high stability of the synthesized glasses. Enamels have high insulating properties. Maximum surface resistance of samples is 7.29·1014 Оhm•сm.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Solncev St.S., Rozenenkova V.A., Mironova N.A., Solov'eva G.A. Vysokotemperaturnye pokrytija dlja voloknistyh substratov [High temperature coatings for fibrous substrates] //Trudy VIAM. 2013. №10. St. 03 (viam-works.ru).
  5. Solncev S.S. Vysokotemperaturnye kompozicionnye materialy i pokrytija na osnove stekla i keramiki [High-temperature composite materials and coatings based on glass and ceramics] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 90–99.
  6. Solncev St.S., Rozenenkova V.A., Mironova N.A. Vysokotemperaturnye steklokeramicheskie pokrytija i kompozicionnye materialy [High-temperature glass-ceramic coatings and composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 359–368.
  7. Solncev S.S., Shvagireva V.V., Isaeva N.V., Solov'eva G.A. Armirovannye zharostojkie steklojemali dlja kamer sgoranija gazoturbinnyh dvigatelej [Reinforced heat-resistant glass enamel to the combustion chambers of gas turbine engines] //Aviacionnye materialy i tehnologii. 2010. №1. S. 26–29.
  8. Solncev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytija dlja uplotnitel'nyh materialov iz metallicheskih volokon [High-temperature thin-film coatings for sealing materials of metal fibers] //Aviacionnye materialy i tehnologii. 2012. №1. S. 30–36.
  9. Solncev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Keramicheskie pokrytija dlja zashhity vysokoprochnoj stali pri termicheskoj obrabotke [The ceramic coating to protect the high-strength steel during heat treatment] //Aviacionnye materialy i tehnologii. 2011. №4. S. 3–8.
  10. Solncev S.S., Rozenenkova V.A., Mironova N.A., Kas'kov V.S. Kompleksnaja sistema zashhity berillija ot okislenija [A comprehensive system of protection against oxidation of beryllium] //Aviacionnye materialy i tehnologii. 2010. №1. S. 12–16.
  11. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composites] //Rossijskij himicheskij zhurnal. 2010. T.LIV. №1.
  12. S. 20–24.
  13. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Carbon and fiberglass new generation] //Trudy VIAM. 2013. №4. (viam-works.ru).
  14. Shelbi Dzh. Struktura, svojstva i tehnologija stekla [The structure and properties of glass technology]: Per. s angl. M.: Mir. 2006. 288 s.
  15. Anand T. Krishnan, Sanghoon Bae, Stephen J. Fonash. Low temperature microcrystalline silicon thin film resistors on glass substrates //Solid-State Electronics. 2000. V. 44. №7. Р. 1163–1168.
  16. Ruqiang Bao, Carl M. Busta, Xiaofeng Su, Minoru Tomozawa, Douglas B. Chrisey. Microstructures, phases, and properties of low melting BaO–B2O3–ZnO glass films prepared by pulsed laser deposition //Journal of Non-Crystalline Solids. 2013. V. 371–372. P. 28–32.
  17. Hrovat M., Kielbasinski K., Makarovič K., Belavič D., Jakubowska M. The characterisation of lead-free thick-film resistors on different low temperature Co-fired ceramics substrates //Materials Research Bulletin. 2012. V. 47. №12. P. 4131–4136.
  18. Amelina O., Nesterov S. Vakuum-plotnaja korundovaja keramika na osnove ul'tradispersnyh poroshkov [The vacuum-tight alumina ceramic-based ultrafine powders] //Nanoindustrija. 2010. №5. S. 40–41.
  19. Shutov D.A., Sitanov D.V. Processy mikro- i nanotehnologij [Processes of micro-and nanotechnology]: Laboratornyj praktikum. Ch. 2. Ivanovo: GOUVPO Ivan. gos. him.-tehnol. un-t. 2006. 135 s.
  20. Appen A.A. Himija stekla [Chemistry glass]. L.: Himija. 1974. 352 s.
  21. Mohajerani A., Martin V., Boyd D., Zwanziger J.W. On the mechanical properties of lead borate glass //Journal of Non-Crystalline Solids. 2013. V. 381. P. 29–34.
  22. Nemilov S.V. Opticheskoe materialovedenie. Opticheskie stekla [Optical materials. Optical glass]: Ucheb. posob. SPb.: CPbGU ITMO. 2011. 175 s.
  23. Winterstein-Beckmann A., Möncke D., Palles D., Kamitsos E.I., Wondraczek L. Structure–property correlations in highly modified Sr, Mn-borate glasses //Journal of Non-Crystalline Solids. 2013. V. 376. P. 165–174.