Refining of scraps of Ni-base superalloy ZhS32-VI to eliminate silicon impurity under conditions of vacuum induction melting
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2014-0-9-1-1
Article PDF (Russian)
(660.04 KB)
How to cite
Min P.G., Sidorov V.V. Refining of scraps of Ni-base superalloy ZhS32-VI to eliminate silicon impurity under conditions of vacuum induction melting // Proceedings of VIAM. 2014. No. 9. DOI: 10.18577/2307-6046-2014-0-9-1-1. URL: https://viam-works.ru/en/journal/2014/9/1
Abstract
Possibility of reduction of the silicon content in ZhS32-VI alloy by combined intro-duction of AEE and REE additions followed by filtration of the melt through the ceramic foam filter with activated working surface from CaO. It was established that filtration rate influences the completeness of removal of nonmetallic inclusions from the melt. The effective use of yttrium for Ni-base melt refining from silicon impurity was demonstrated.
Reference list
- Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniju lityh prutkovyh (shihtovyh) zagotovok [Experience in processing of waste foundry alloy ZHS32-VI at the scientific-industrial complex for the production of cast VIAM of bar (charge) blanks] //Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
- Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
- Sidorov V.V., Rigin V.E., Kablov D.E. Organizacija proizvodstva lityh prutkovyh zagotovok iz sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Organization of production of cast bar stock of modern casting nickel-base superalloys] //Litejnoe proizvodstvo. 2011. №10. S. 2–5.
- Kablov D.E., Sidorov V.V., Min P.G. Vlijanie primesi azota na strukturu monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i razrabotka jeffektivnyh sposobov ego rafinirovanija [Influence of nitrogen impurities on the structure of single-crystal nickel superalloys ZhS30-VI and develop effective ways of refining it] //Aviacionnye materialy i tehnologii. 2012. №2. S. 32–36.
- Kablov D.E., Chabina E.B., Sidorov V.V., Min P.G. Issledovanie vlijanija azota na strukturu i svojstva monokristallov iz litejnogo zharoprochnogo splava ZhS30-VI [Investigation of the influence of nitrogen on the structure and properties of single crystals of cast superalloy ZhS30-VI] //MiTOM. 2013. №8. S. 3–7.
- Kablov D.E., Sidorov V.V., Min P.G. Zakonomernosti povedenija azota pri poluchenii monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i ego vlijanie na jekspluatacionnye svojstva [Of the behavior of nitrogen in the preparation of single crystals of heat-resistant nickel alloy ZhS30-VI and its impact on the performance of the] //MiTOM. 2014. №1. S. 8–12.
- Improved low sulfur nickel-base single crystal superalloy with ppm additions of lanthanum and yttrium: pat. 2415888 EU; publ. 14.10.2010.
- Zhuanggi HU, Hongwei SONG, Shouren GUO, Wenru SUN and Dezhong LU. Effects of Phosphorus on Microstructure and Creep Property of IN718 Superalloy //J. Mater. Sci. Technol. 2005. V. 21. Suppl. P. 73–76.
- Sidorov V.V., Rigin V.E., Filonova E.V., Timofeeva O.B. Strukturnye issledovanija i svojstva monokristallov splavov VZhM4-VI i VZhM5-VI, soderzhashhih povyshennye kolichestva fosfora [Structural studies of the properties of single crystals and alloys VZhM4-VI-VI and VZhM5 containing elevated levels of phosphorus] //Trudy VIAM. 2014. №3. St. 02 (viam-works.ru).
- Sposob poluchenija izdelija iz zharoprochnogo nikelevogo splava [A method of manufacturing a heat-resistant nickel alloy]: pat. 2215059 Ros. Federacija; opubl. 26.12.2001.
- Sidorov V.V., Rigin V.E., Gorjunov A.V., Kablov D.E. Vysokojeffektivnye tehnologii i sovremennoe oborudovanie dlja proizvodstva shihtovyh zagotovok iz litejnyh zharoprochnyh splavov [Enabling technologies and modern equipment for the production of charge billets casting of superalloys] //Metallurg. 2012. №5. S. 26–30.
- Sidorov V.V., Rigin V.E., Gorjunov A.V., Min P.G., Kablov D.E. Poluchenie Re–Ru-soderzhashhego splava s ispol'zovaniem nekondicionnyh othodov [Preparation of Re–Ru-containing alloy using unconditioned waste] //Metallurgija mashinostroenija. 2012. №3. S. 15–17.
- Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features single-crystal high-temperature nickel alloys, alloyed with rhenium] //Metally. 2006. №5. S. 47–57.
- Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah dlja lopatok gazovyh turbin (prodolzhenie) [Measurements in high-temperature nickel alloys for gas turbine blades (continued)] //Materialovedenie. 2000. №3. S. 38–43.
- Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh) zagotovok iz sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Production of cast semifinished (of charge) blanks of the modern casting nickel-base superalloys] /V sb. trudov nauch.-tehnich. konf., posvjashhennoj 310-letiju ural'skoj metallurgii i sozdaniju tehniko-vnedrencheskogo centra metallurgii i tjazhelogo mashinostroenija. T. 1. Ekaterinburg: «Nauka Servis». 2011. S. 31–38.
- Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of gas turbine engine blades with a single-crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements – materials for current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
- Sidorov V.V., Rigin V.E., Zajcev D.V., Gorjunov A.V. Formirovanie nanostrukturirovannogo sostojanija v litejnom zharoprochnom splave pri mikrolegirovanii ego lantanom [Formation of nanostructured state in casting superalloy with microalloying its lanthanum] //Trudy VIAM. 2013. №1. St. 01 (viam-works.ru).
- Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj [Nickel superalloys for blades casting with directional and single-crystal structure]. Ch. I //Materialovedenie. 1997. №4. S. 32–39.
- Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj [Nickel superalloys for blades casting with directional and single-crystal structure]. Ch. II //Materialovedenie. 1997. №5. S. 14–16.
- Sidorov V.V., Rigin V.E., Timofeeva O.B., Min P.G. Vlijanie kremnija i fosfora na zharoprochnye svojstva i strukturno-fazovye prevrashhenija v monokristallah ih vysokozharoprochnogo splava VZhM4-VI [Effect of silicon and phosphorus on the heat-resistant properties and structural phase transitions in single crystals of a highly heat resistant alloy VZhM4-VI] //Aviacionnye materialy i tehnologii. 2013. №3. S. 32–38.