Fireproof fabric material with an elastomeric covering for a sliding path of the saving ladder

Nesterova T.A., Platonov M.M., Nazarov I.A., Gerter J.A.
Nesterova T.A., Platonov M.M., Nazarov I.A., Gerter J.A. Fireproof fabric material with an elastomeric covering for a sliding path of the saving ladder // Proceedings of VIAM. 2014. No. 6. DOI: 10.18577/2307-6046-2014-0-6-11-11. URL: https://viam-works.ru/en/journal/2014/6/11
Abstract

The fabric material with an elastomeric covering is developed for a sliding path on the basis of a technical polyester fabric a sample 208 with the bilateral covering containing antipyrines and an electroconducting coating from the face. Physical, physicomechanical properties of a material are studied. The fabric material with an elastomeric covering on the main properties meets the requirements of the TSO-S69c standard and to requirements AP-25 the Part 1 Appendix F on combustibility. The material is at level foreign Air Cruisers Company firms of the USA an art. M-11673 on the weight of 1 sq. m and combustibility, but loses to it on explosive loading.

Reference list
  1. Kirin K.M. Perspektivnye pozharobezopasnye tekstilnye materialy dlya primeneniya v grazhdanskoy aviatsii [Prospective fireproof textiles for use in civil aircraft]: Avtoref. dis. na soiskanie uchyonoj stepeni k.t.n. M.: GOU VPO RosZITL. 2004. 16 s.
  2. Technical Standard Orbler TSO-C69с. publ. 18.8.1999. Р. 1–20.
  3. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tekhnologiy ix pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviatsionnie materialy i tekhnologii. 2012. №S. S. 7–17.
  4. Grashchenkov D.V., Chyrsova L.V. Strategiya razvitiya kompozitsionnykh fynktsionalnykh materialov [Development Strategy composite and functional materials] //Aviatsionnye materialy i texnologii. 2012. №S. S. 231–242.
  5. Barbot’ko S.L. Pozharobezopasnost’ aviatsionnykh materialov [Fire safety of aircraft materials] //Aviatsionnye materialy i texnologii. 2012. №S. S. 431–439.
  6. Federal’nye aviatsionnye pravila [Federal Aviation Regulations]. 6.03.1995.
  7. Aviatsionnye pravila. Ch. 25 Normy letnoy godnosti samoletov transportnoy kategorii [Aviation Regulations. Ch 25. Airworthiness standards transport category airplanes]. Prilozhenie F. M.: Aviaizdat. 2004.
  8. Tokoprovodyashchaya tkan’ [Conductive fabric]: pat. 2354766 Ros. Federatsiya; opybl. 10.05.2009.
  9. Еscape slides: pat. 1442711 GB; opubl. 14.07.1974.
  10. Escape device for aircraft: pat. 5542629 JP; opubl. 6.08.1996.
  11. Germetichnyy elastichnyy material [Sealed elastic material]: pat. 24443820 Ros. Fed-eratsiya; opybl. 27.02.2012.
  12. 12 Platonov M.M., Nazarov I.A., Nesterova T.A., Beyder E.Ya. Pozharobezopastnyy ma-terial na tekstilnoy osnove c poliuretanovym pokrytiem dlya naduvnoy obolochki spasatel’nogo trapa [Fireproof material textile-based polyurethane-coated shell for inflatable rescue ladder] //Aviatsionnye materialy i tekhnologii. 2013. №2. S. 50–54.
  13. Platonov M.M., Nesterova T.A., Nazarov I.A., Beyder E.Ya. Tkaneplenochnyy material VRT-9 dlya nadyvnoy obolochki aviatsionykh spasatel’nykh trapov [Tkaneplenochny material ART-9 aircraft shell for inflatable rescue ladders] //Trudy VIAM. 2013. №5. St. 05 (viam-works.ru).
  14. Kablov E. N. Ximiya v aviatsionnom materialovedenii [Chemistry aviation materials] //Rossiyskiy ximicheskiy zhurnal. 2010. Т. LIV. №1. S. 3–4.
  15. Ksantos M. Fynktsional’nye napolniteli dlya plastmass [Functional fillers for plastics]. SPb.: NОТ. 2010. S. 322–352, 205–223, 355–374.
  16. Barbot’ko S.L. Puti obespecheniya pozharnoy bezopasnosti aviatsionnykh materialov [Ways to ensure fire safety of aircraft materials] //Rossiyskiy khimicheskiy zhurnal. 2010. Т. LIV. №1. S. 121–126.
  17. Polimernaya teplootrazhayushchaya kompozitsiya dlya pokrytiya [Polymer heat-reflecting coating composition]: pat.2467042 Ros. Federatsiya; opybl. 07.06.2011.
  18. Samokhvalov E. Voprosy ognezashchity tekstil’nykh materialov [Questions fireproof-ing textile materials] //F+S: tekhnologiya bezopasnosti i protivopozharnoy zashchity. 2011. №4. S. 28–31.
  19. Reznichenko S.V. Bol’shoy spravochnik rezinshika. Ch. 2 Reziny i rezino-tekhnicheskie izdeliya [Great Compendium rezinschikov. Part 2. Rubber and rubber products]. M.: MAI. 2012. S. 388–403.
  20. Mikhalchan A.A., Lysenko V.A. Myradova N.Sh., Zhiteneva D.A., Saklakova E.V., Lysenko A.A. Yglerodnye nanotrubki morfologiya i svoystva [Carbon nanotubes: morphology and properties] //Khimicheskie volokna 2010. №5. S. 18–21.
  21. Badamshina E.R., Gafurova M.P., Estrin Ya.I. Modifitsirovanie uglerodnykh nanotrubok i sintez polimernykh kompozitsionnykh materialov s ix uchastiem [Modifica-tion of carbon nanotubes and synthesis of polymeric composites with their participation] //Uspekhi ximii 2010. Т. 79. №11. S. 1027–1064.
  22. Ekstrin Ya.I., Badamshina E.R., Grishchuk A.A., Kylagina G.S., Lesnichaya V.A., Ol’khov Yu.A., Ryabenko A.G., Sul’yanov S.N. Svoystva nanokompozitov na osnove shitogo elasnomernogo poliuretana i ul’tramalykh dobavok odnosloynykh uglerodnykh nanotrubok [Properties of nanocomposites based on crosslinked elastomeric polyurethane additives and ultrasmall single-walled carbon nanotubes] //Vysokomolekylyarnye soedeneniya Ser. А. 2012. Т. 54. №4. S. 568–577.
  23. Lysenko V.A., Sal’nikova A.A., Mikhalchan A.A. Uglerod-ftorpolimernye kompozity: povyshenie elektroprovodimosti [Carbon-fluoropolymer composites: increase the electrical conductivity] //Khimicheskie volokna. 2012. №1. S. 41–44.
  24. Dick Dzh.S. Tekhnologiya reziny: retsepturostroenie i ispytaniya [Rubber Technology: retsepturostroenie and testing]. SPb.: NOT 2010. S. 601–610.
  25. Reznichenko S.V. Bol’shoi spravochnik rezinshchika. Ch. 1 Kauchuki i ingredient [Great Compendium rezinschikov. Part 1. Rubbers and ingredients]. M.: MAI. 2012. S. 294–323.
  26. Nesterova T.A., Barbot’ko S.L., Nikolaeva M.F., Gerter Yu. A. Mnogosloynyy zashchitno- dekorativnyy material dlya dekorirovaniya detaliy v salonakh samoletov i vertoletov [Multilayer protective and decorative material for decorating details in the cabin of aircraft and helicopters] //Trudy VIAM. 2013. №8. St. 04 (viam-works.ru).