Production of standard polymer composite samples with the set porosity by vacuum infusion

Gusev Y.A., Grigoriev M.M., Timoshina L.N.
Gusev Y.A., Grigoriev M.M., Timoshina L.N. Production of standard polymer composite samples with the set porosity by vacuum infusion // Proceedings of VIAM. 2014. No. 11. DOI: 10.18577/2307-6046-2014-0-11-6-6. URL: https://viam-works.ru/en/journal/2014/11/6
Abstract

In this study the manufacturing technologies of standard CFRP samples with the set porosity by vacuum infusion using a semipermeable membrane, on a basis of epoxy resin depending on impregnation parameters have been considered. Measurement of porosity was carried out visually on sections. Samples of plates were investigated by echo-pulse ultrasonic control method , using phased arrays for detection of dependence between a ground signal and porosity in standard samples.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemicals in aviation materials] //Rossijskij himicheskij zhur-nal. 2010. T. LIV. №1. S. 3–4.
  3. Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozicionnye materialy, po-luchennye putem propitki plenochnym svjazujushhim [Polymer composite material obtained by impregnating a film binder] //Kompozicionnye materialy. 2011. №11. S. 2–6.
  4. Veshkin E.A., Postnov V.I., Abramov P.A. Puti povyshenija kachestva detalej iz PKM pri vakuumnom formovanii [Ways to improve the quality of parts of the PCM with vacuum forming] //Izvestija Samarskogo nauchnogo centra Rossijskoj akademii nauk. 2012. T. 14. №4 (3). S. 831–838.
  5. Minakov V.T., Postnov V.I., Hpul'kov A.V., Postnov A.V., Pletin' I.I. Osobennosti skleivanija detalej iz PKM s ispol'zovaniem polimepnoj osnastki [Features gluing parts of PCM using polymeric snap] //Klei. Germetiki. Tehnologii. 2008. №5. S. 24–29.
  6. Muhametov P.P., Ahmadieva K.R., Chursova L.B., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for the promising methods for the manufacture of structural fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  7. Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy [Structural polymer composite materials]. SPb.: NOT. 2008. 820 s.
  8. Kerber M.L., Vinogradov V.M. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologija [Polymer composite materials: structure, properties, technology]. SPb.: Professija. 2009. 560 s.
  9. Alent'ev A.Ju., Jablokova M.Ju. Svjazujushhie dlja polimernyh kompozicionnyh materialov [Binders for polymeric composite materials]: Ucheb. posobie. M.: MGU im. M.V. Lomono-sova. 2010. 69 s.
  10. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders for advanced methods of manufacturing a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  11. Babin A.N. Svjazujushhie dlja polimernyh kompozicionnyh materialov novogo pokolenija [Binders for polymer composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  12. Borshhev A.V., Hrul'kov A.V., Halturina D.S. Izgotovlenie nizkoporistogo polimernogo kompozicionnogo materiala dlja primenenii v slabo- i srednenagruzhennyh konstrukcijah [Production of low porosity of the polymer composite material for use in low and medium duty designs] //Trudy VIAM. 2014. №7. St. 03 (viam-works.ru).
  13. Himicheskaja promyshlennost'. Obzornaja informacija. Ser. «Jepoksidnye smoly i ma-terialy na ih osnove». «Otverditeli dlja jepoksidnyh smol» [Chemical Industry. Overview. Ser. «Epoxy resins and materials based thereon». «Hardeners for epoxy resins»]. M.: NIITJeHIM. 1983. 39 s.
  14. Jepoksidnaja kompozicija [Epoxy system]: pat. 2447104 Ros. Federacija; opubl. 05.10.2010.
  15. Starcev O.V., Kablov E.N., Mahon'kov A.Ju. Zakonomernosti perehoda jepoksidnyh svjazujushhih kompozicionnyh materialov po dannym dinamicheskogo mehanicheskogo analiza [Laws of the transition epoxy binder composite materials according to the dynamic mechanical analysis] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 104–113.
  16. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development of autoclave and non-autoclave molding technology PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  17. Dushin M.I., Hrul'kov A.V., Muhametov P.P. Vybor tehnologicheskih parametrov avtoklavnogo formovanija detalej iz polimernyh kompozicionnyh materialov [Selection of process parameters autoclave molding parts made of polymeric composite materials] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  18. Postnov V.I., Burhan O.L., Rahmatullin A.Je., Kachura S.M. Nerazrushajushhie metody kontrolja soderzhanija svjazujushhih v prepregah i PKM (obzor) [Non-destructive testing binder content of the prepregs and PCM (review)] //Trudy VIAM. 2013. №12. St. 06 (viam-works.ru).
  19. Dalin M.A., Generalov A.S., Bojchuk A.S., Lozhkova D.S. Osnovnye tendencii razvitija akusticheskih metodov nerazrushajushhego kontrolja [The main trends in the development of acoustic methods of non-destructive testing] //Aviacionnye materialy i teh-nologii. 2013. №1. S. 64–69.
  20. Bojchuk A.S., Stepanov A.V., Kosarina E.I., Generalov A.S. Primenenie tehnologii ul'trazvukovyh fazirovannyh reshetok v nerazrushajushhem kontrole detalej i konstrukcij aviacionnoj tehniki, izgotovljaemyh iz PKM [Application of ultrasonic phased array technology in nondestructive testing of parts and structures of aircraft, manufactured from PCM] //Aviacionnye materialy i tehnologii. 2013. №2. S. 41–46.
  21. GOST 15139–69. Plastmassy. Metody opredelenija plotnosti (ob`emnoj massy) [Plastics. Methods for determining the density (bulk density)].