Evaluation of properties of fire safety fabric-film material for emergency slide

Nesterova T.A., Platonov M.M., Sharakina L.A.
Nesterova T.A., Platonov M.M., Sharakina L.A. Evaluation of properties of fire safety fabric-film material for emergency slide // Proceedings of VIAM. 2014. No. 10. DOI: 10.18577/2307-6046-2014-0-10-9-9. URL: https://viam-works.ru/en/journal/2014/10/9
Abstract

Results of research of properties of VRT-10 fabric-film material for emergency slide, manufactured on a base of commercial polyether fabric with double-sided fireproof coating and electro-conducting coating from a face are presented . Influence of higher and lower temperature, climatic impacts on strength characteristics and conductivity of the material was studied. The carried out study showed that the material keeps more than 90% of its strength properties after all influences, except for weft breaking strength after 100°С temperature effect for 200 hours (81,4% preservation of strength).However, in many cases a strength of material remained actually without change. A tearing resistance characteristic decreases after a cyclic drop of temperatures for 10–15%, and increases after above-zero temperatures influence. At direct increase of temperature influence, more considerable decrease of strength and elongation at rupture of VRT-10 grade material takes place. However, a residual valu

Reference list
  1. Kirin K.M. Perspektivnye pozharobezopasnye tekstil'nye materialy dlja primenenija v grazhdanskoj aviacii [Prospective fireproof textile materials for use in civil aircraft]: Avtoref. dis. k.t.n. M. 2004. 16 s.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Flammability of Aircraft Materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  4. Technical Standard Orbler TSO-C69с; pabl. 18.8.1999. P. 1–20.
  5. Escape device for aircraft: pat. 5542629 JP; pabl. 06.08.1996.
  6. Escape slides: pat. 1442711 GB; pabl. 14.07.1974.
  7. Tokoprovodjashhaja tkan' [Conductive fabric]: pat. 2354766 Ros. Federacija; opubl. 10.05.2009.
  8. Nesterova T.A., Platonov M.M., Nazarov I.A., Gerter Ju.A. Pozharobezopasnyj tkaneplenochnyj material dlja dorozhki skol'zhenija spasatel'nogo trapa [Tkaneplenochny fireproof material for sliding track rescue ladder] //Trudy VIAM. 2014. №6. St. 11 (viam-works.ru).
  9. Mnogoslojnyj material dlja spasatel'nyh sredstv [Multi-layer material for life-saving appliances]: pat. 2502605 Ros. Federacija; opubl. 27.12.2013.
  10. Lysenko V.A., Sal'nikova A.A., Mihalchan A.A. Uglerod-ftorpolimernye kompozity: povyshenie jelektroprovodnosti [Carbon-fluoropolymer composites: increase the electrical conductivity] //Himicheskie volokna. 2012. №1. S. 41–44.
  11. Larionov S.A., Deev I.S., Petrova G.N., Bejder Je.Ja. Vlijanie uglerodnyh napolnitelej na jelektrofizicheskie, mehanicheskie i reologicheskie svojstva polijetilena [Influence of carbon fillers on the electrical, mechanical and rheological properties of polyethylene] //Trudy VIAM. 2013. №9. St. 04 (viam-works.ru).
  12. Kablov E.N. Himija v aviacionnom materialovedenii [Chemicals in aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  13. Jekstrin Ja.I., Badamshina Je.R., Grishhuk A.A., Kulagina G.S., Lesnichaja V.A., Ol'hov Ju.A., Rjabenko A.G., Sul'janov S.N. Svojstva nanokompozitov na osnove sshitogo jelastomernogo poliuretana i ul'tramalyh dobavok odnoslojnyh uglerodnyh nanotrubok [Properties of nanocomposites based on crosslinked elastomeric polyurethane and ultra supplements of single-walled carbon nanotubes] //Vysokomolekuljarnye soedinenija. 2012. Ser. A. T. 54. №4. S. 568–577.
  14. Platonov M.M., Nazarov I.A., Nesterova T.A., Bejder Je.Ja. Tkaneplenochnyj material VRT-9 dlja naduvnoj obolochki aviacionnyh spasatel'nyh trapov [Tkaneplenochny material VRT-9 inflatable shell aviation rescue ladders] //Trudy VIAM. 2013. №5. St. 05 (viam-works.ru).
  15. Tjumeneva T.Ju., Kogtjonkov A.S., Lukina N.F., Chursova L.V. Uspehi v oblasti razrabotki kleev i tehnologij dlja izgotovlenija rezinotehnicheskih izdelij aviacionnogo naznachenija [Progress in the development of adhesives and technologies for the manufacture of rubber products for aircraft industry] //Klei. Germetiki. Tehnologii. 2013. №10. S. 7–10.
  16. Tjumeneva T.Ju., Kogtjonkov A.S., Lukina N.F., Chursova L.V. Vlijanie napolnitelej na svojstva kleev rezinotehnicheskogo naznachenija [Effect of fillers on the properties of rubber-purpose adhesives] //Trudy VIAM. 2014. №4. St. 05 (viam-works.ru).
  17. Polimernaja teplootrazhajushhaja kompozicija dlja pokrytija [Polymer heat-reflecting coating composition]: pat. 2467042 Ros. Federacija; opubl. 07.06.2011.