Soldering technology of porous fibrous material of the «fehral»-type alloy for seal-ing of the flow part of GTE

Afanasiev-Khodykin A.N., Rylnikov V.S., Farafonov D.P.
Afanasiev-Khodykin A.N., Rylnikov V.S., Farafonov D.P. Soldering technology of porous fibrous material of the «fehral»-type alloy for seal-ing of the flow part of GTE // Proceedings of VIAM. 2014. No. 1. DOI: 10.18577/2307-6046-2014-0-1-2-2. URL: https://viam-works.ru/en/journal/2014/1/2
Abstract

This article contains information about a new porous fibrous sealing material for sealing the flow of the gas turbine engine. Highlight features of its brazing. The results of testing various solders for the brazing of porous fibrous sealant. Provides basic in-formation about the new composite solder iron base specifically designed for brazing porous fibrous sealant type alloy «fehral».

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic approaches to the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i staley spetsial'nogo naznacheniya, zaschitnyh i teplozaschitnyh pokrytiy [Development strategy of heat-resistant alloys and special-purpose steels, protective and thermal-protective coatings] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 19–35.
  3. Kablov E.N., Muboyadzhyan S.A. Zharostoykie i teplozaschitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat-resistant and thermal-protective coatings for the high-pressure turbine blades of promising GTEs] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 60–70.
  4. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie protsessa napravlennoy kristallizatsii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoy i kompozitsionnoy strukturoy [Development of directional solidification process in the GTE blades made of heat-resistant alloys with single crystal and composite structure] //Aviatsionnye materialy i tehnologii. 2012. №1. S. 3–8.
  5. Kablov E.N. Litye lopatki gazoturbinnyh dvigateley [Cast blades of gas-turbine engines]. M.: MISIS. 2001. 632 s.
  6. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detaley gazoturbinnyh dvigateley [Materials for highly thermal-loaded parts of gas-turbine engines] //Vestnik MGTU im. N.E. Baumana. 2011. Spets. vyp. «Perspektivnye konstruktsionnye materialy i tehnologii». S. 13–19.
  7. Ryl'nikov V.S., Afanas'ev-Hodykin A.N., Krasikov M.I. Issledovanie remontnoy tehnologii ispravleniya defektov payanyh soedineniy toplivnyh kollektorov [Study of repair technology to correct the defects of soldered joints in fuel manifolds] //Trudy VIAM. 2013. №12. St. 02 (viam-works.ru).
  8. Lashko N.F., Lashko S.V. Voprosy teorii i tehnologii payki [Theoretical and practical issues of soldering]. M.: Izd-vo Saratovskogo un-ta. 1974. 248 s.
  9. Lashko N.F., Lashko S.V. Payka metallov [Soldering metals]. M.: Mashinostroenie. 1967. 368 s.
  10. Horunov V.F., Maksimova S.V. Payka zharoprochnyh splavov na sovremennom etape [Soldering of heat-resistant alloys at the current stage] //Svarochnoe proizvodstvo. 2010. №10. S. 24–27.
  11. Lukin V.I., Ryl'nikov V.S., Afanas'ev-Hodykin A.N. Osobennosti polucheniya payanyh soedineniy iz splava ZhS36 [Peculiarities of soldered joints of ZhS36 alloy] //Tehnologiya mashinostroeniya. 2010. №5. S. 21–25.
  12. Lukin V.I., Ryl'nikov V.S., Afanas'ev-Hodykin A.N., Orehov N.G. Osobennosti payki monokristallicheskih otlivok iz splava ZhS32 [Peculiarities of ZhS 32 alloy single crystal castings soldering] //Svarochnoe proizvodstvo. 2012. №5. S. 24–30.
  13. Kablov E.N., Evgenov A.G., Ryl'nikov V.S., Afanas'ev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev dlya diffuzionnoy vakuumnoy payki, poluchennyh metodom atomizatsii rasplava [Research of solder fine powders for diffusion vacuum soldering, obtained by melt atomization] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. Spets. vyp. «Perspektivnye konstruktsionnye materialy i tehnologii». S. 79–87.
  14. Shmotin Yu.N., Starkov R.Yu., Danilov R.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for advanced engine of JSC NPO SATURN] //Aviatsionnye materialy i tehnologii. 2012. №2. S. 6–8.