P.G. Min, V.E. Vadeev, D.A. Chemov, R.V. Sankin Development and implementation of a rhenium‑nickel alloy for alloying monocrystalline high‑temperature nickel alloys // Proceedings of VIAM. 2026. No. 7. DOI: 10.18577/2307-6046-2026-0-7-76-90. URL: https://viam-works.ru/index%2ephp/en/journal/2026/7/6

Development and implementation of a rhenium‑nickel alloy for alloying monocrystalline high‑temperature nickel alloys

P.G. Min, V.E. Vadeev, D.A. Chemov, R.V. Sankin
Abstract

The article presents the technology of production of rhenium-nickel alloying, intended for alloying of casting high-temperature nickel alloys. A detailed technological scheme of production of alloying from preparation of initial materials to the release of finished products is described. It is shown that preliminary vacuum annealing of rhenium powder provides sintering of particles and effective degassing. The developed modes of powder annealing and alloying in a vacuum arc furnace with a non-consumable electrode allow to minimize the gas content, ensure uniform distribution of components inside the ingot, and increase the yield of the metal. The developed alloying is successfully used in the manufacture of single-crystal heat-resistant nickel alloys.

Keywords
rhenium, alloying, mechanical properties, long-term strength, cast heat-resistant alloys, single crystal, VZhM4, ZhS32, aircraft blades, gas turbine engines
Reference list
  1. Kishkin S.T., Kablov E.N. Casting heat-resistant alloys for turbine blades. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISiS; VIAM, 2002, pp. 48–58.
  2. Sidorov V.V., Podkopaeva L.A., Min P.G. Use of rhenium-containing master alloy in smelting single-crystal high-heat-resistant nickel alloys. Metallurg, 2013, no. 6, pp. 77–81.
  3. Nickel-based alloy: pat. 1157865 USSR; appl. 01.06.84; publ. 10.06.97.
  4. Logunov A.V., Bykov Yu.G. Problems of design and production of high-temperature cast blades for aircraft gas turbine engines: in 2 books. Moscow: Nauka i tekhnologii, 2023, book 2: Technology and Production, 640 p.
  5. Min P.G., Vadeev V.E., Min M.G. Development and implementation in production of the new single-crystal high-temperature nickel alloy for casting of gas turbine blades for the prospective engine PD-8. Aviation materials and technologies, 2025, no. 1 (78), pp. 3–17. Available at: http://www.journal.viam.ru (accessed: November 11, 2025). DOI: 10.18577/2713-0193-2025-0-1-3-17.
  6. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaev M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: November 11, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  7. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaev M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: November 11, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  8. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30–41. Available at: http://www.journal.viam.ru (accessed: November 11, 2025). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  9. Kablov E.N., Bondarenko Yu.A., Surova V.A. Features of high-gradient directional solidification and equipment for casting single-crystal samples and turbine blades from heat-resistant alloys containing rhenium. Casting heat-resistant alloys. Effect of S.T. Kishkin. Moscow: Nauka, 2006, pp. 194–205.
  10. Min P.G., Goryunov A.V., Vadeev V.E. Modern heat-resistant nickel alloys and efficient resource-saving technologies for their manufacture. Tekhnologiya metallov, 2014, no. 8, pp. 12–23.
  11. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. Development of technologies and equipment for producing blades of the hot path of gas turbine engines from superalloys with directional and single-crystal structure. Trudy VIAM, 2023, no. 7 (125), pp. 3–14. Available at: http://www.viam-works.ru (accessed: November 11, 2025). DOI: 10.18577/2307-6046-2023-0-7-3-14.
  12. Giamei A.F., Anton D.L. Rhenium additions to a Ni-base superalloy: Effects on microstructure. Metallurgical transactions, 1985, vol. 16, pp. 1997–2005.
  13. Blavette D., Caron P., Khan T. An atom probe investigation of the role rhenium additions in improving creep resistance of Ni-base superalloys. Scripta metallurgica, 1986, vol. 20, no. 10, pp. 1395–1400.
  14. Petrushin N.V., Ospennikova O.G., Elyutin E.S. Rhenium in single crystal nickel-based superalloys for gas turbine engine blades. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 5–16. DOI: 10.18577/2071-9140-2014-0-s5-5-16.
  15. Ospennikova O.G. Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review). Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 3–19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
  16. Khryashchev I.I., Danilov D.V., Logunov A.V. Development of an economically alloyed nickel heat-resistant alloy for gas turbine blades. Vestnik Moskovskogo aviatsionnogo instituta, 2019, vol. 26, no. 2, pp. 205–218.
  17. Anderson C., Taylor P., Anderson C. Extractive Metallurgy of Rhenium A Review. Minerals & Metallurgical Processing, 2013, vol. 30, pp. 59–73. DOI: 10.1007/BF03402342.
  18. Mineral commodity summaries. Reston: U.S. Geological Survey, 2020, 200 p. DOI: 10.3133/mcs2020.
  19. Kasikov A.G., Petrova A.M. Rhenium Recycling. Moscow: RIOR; INFRA-M, 2014, 95 p. DOI: 10.12737/3285.
  20. Ignatovich A.S. Extraction of Copper and Rhenium from Ammonia Leaching Solutions of Substandard Copper Concentrates: thesis, Cand. Sc. (Tech.). St. Petersburg, 2021, 118 p.
  21. Sidorov V.V., Kablov D.E., Rigin V.E. Metallurgy of Casting Heat-Resistant Alloys: Technology and Equipment. Ed. E.N. Kablov. Moscow: VIAM, 2016, 368 p.
  22. Kablov D.E. Patterns of nitrogen behavior during the production of single crystals of heat-resistant nickel alloys and improving their performance properties: thesis abstract, Cand. Sc. (Tech.). Moscow, 2012, 17 p.
  23. Kablov D.E., Sidorov V.V., Min P.G. Patterns of nitrogen behavior during the production of single crystals of heat-resistant nickel alloys and its influence on their performance properties. Metallovedenie i termicheskaya obrabotka metallov, 2014, no. 1, pp. 8–12.
  24. Mitchel A. Nitrogen in Superalloys. High Temperature Materials and Processes, 2005, vol. 24, no. 2, pp. 101–109.
  25. Logunov A.V., Mikhailov A.M., Rumyantseva S.B. Determination of temperature-time parameters of dissolution of refractory elements in a liquid melt for the purpose of further improvement of technology of vacuum-induction smelting of nickel heat-resistant alloys using a complex ligature. Special electrometallurgy, 2024, no. 3, pp. 2–13.
  26. Zelikman A.N., Korshunov B.G. Metallurgy of Rare Metals: A Textbook for Universities. 2nd ed., rev. and add. Moscow: Metallurgy, 1991, 432 p.
  27. Petukhov O.F., Sanakulov K.S., Kurbanov M.A., Sharafutdinov U.Z. Reniy. Navoi, 2020, 397 p.
  28. Venatovskij I.V. Study of the geotechnical conditions of uranium deposits of Uzbekistan during exploration work. Uranium in situ leaching: proceedings of a Technical Committee Meeting (Vienna, 5–8 October, 1992). Vienna: International Atomic Energy Agency, 1993, pp. 95–103.
  29. Palant A.A., Troshkina I.D., Chekmarev A.M., Kostylev A.I. Rhenium Technology. Moscow: Galley-Print, 2015, 324 p.
  30. Korovin S.S., Bukin V.I., Fedorov P.I., Reznik A.M. Rare and Trace Elements. Chemistry and Technology: in 3 vols. Ed. S.S. Korovin. Moscow: MISiS, 2003, vol. 3, p. 375.
  31. Rakov E.G., Troshkina I.D. Rhenium. Chemical Encyclopedia: in 5 vols. Ed. N.S. Zefirov. Moscow: Great Russian Encyclopedia, 1995. Vol. 4. Polymer – Trypsin, p. 639.
  32. Min P.G., Pitelin N.S., Vadeev V.E. Development of a Technology for Obtaining a Hafnium-Nickel Master Alloy in a Vacuum Arc Furnace for Alloying Heat-Resistant Nickel Casting Alloys. Tekhnologiya metallov, 2022, no. 7, pp. 30–39.
  33. Min P.G., Vadeev V.E., Pitelin N.S. Technology for the Production of Refractory Metal Master Alloys and Their Testing in the Melting of Heat-Resistant Nickel Casting Alloys. Metallurg, 2022, no. 11, pp. 88–94.
  34. Lyakishev N.P., Bannykh O.A., Rokhlin L.L. et al. Phase diagrams of binary metallic systems: a handbook in 3 vols. Moscow: Mashinostroenie, 1997, vol. 2, pp. 885–889.
  35. TU 48-19-92–88. Rhenium metal hydrogen reduction. Moscow, 1988, 21 p.
  36. Rhenium (Superalloy grade). No 8112 9131. MMTA Consolidated Regulations. Available at: http://www.mmta.co.uk (accessed: November 11, 2025).
  37. Bradbury S. Powder Metallurgy Equipment Manual. Preston: Metal Powder Industries Federation, 1986, p. 113.
  38. Method for producing ligatures in a vacuum arc furnace with a non-consumable electrode: pat. 2734220 Rus. Federation; appl. 27.02.20; publ. 13.10.20.