UDC
669.15-194.55:621.762
DOI
10.18577/2307-6046-2026-0-7-63-75
Article PDF (Russian)
(1.67 MB)
How to cite
V.D. Gogoleva, P.E. Kuznetsova, I.S. Kuko, T.A. Mazalova, I.A. Bogachev Structure and properties investigation of the synthesized steel material of Fe–Cr–Ni–Co–Mo system, obtained by selective laser melting after different heat treatments // Proceedings of VIAM. 2026. No. 7. DOI: 10.18577/2307-6046-2026-0-7-63-75. URL: https://viam-works.ru/index%2ephp/en/journal/2026/7/5
Structure and properties investigation of the synthesized steel material of Fe–Cr–Ni–Co–Mo system, obtained by selective laser melting after different heat treatments
Abstract
The influence of different aging parameters on the structure and mechanical properties of maraging steel of 02Kh13N5K9M4 grade, obtained by selective laser melting was investigated from the initial state material without the use of quenching. In the course of the work, the chemical composition and content of impurities, technological characteristics of metal powder composition were determined, the percentage of gas pores and microstructure were examined, the mechanical properties of samples after aging were evaluated, as well as the values of indirect indicators, such as the amount of residual austenite and hardness, were determined.
Keywords
additive manufacturing, maraging steel, heat treatment, selective laser melting
Reference list
- State Standard R 57558–2025. Additive Manufacturing. Basic Principles. Terms and Definitions. Moscow: RST, 2025, 36 p.
- Zlenko M.A., Popovich A.A., Mutylina I.N. Additive Manufacturing in Mechanical Engineering: A Textbook. St. Petersburg: Polytech. Univ. Press, 2013, 222 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- National Research Center «Kurchatov Institute» – VIAM. Available at: https://viam.ru/add (accessed: April 24, 2025).
- Bogachev I.A., Sukhov D.I., Khodyrev N.A., Kurkin S.E. Investigation of the supports structures' printing parameters for parts obtained by selective laser melting of metal powder composition of the Co–Cr–Ni–W–Ta alloy. Trudy VIAM, 2022, no. 1 (107), pp. 3–13. Available at: http://www.viam-works.ru (accessed: April 25, 2025). DOI: 10.18577/2307-6046-2022-0-1-3-13.
- Goldstein M.I., Grachev S.V., Veksler Yu.G. Special steels: textbook for universities. Moscow: Metallurgy, 1985, 407 p.
- Arzamasov B.N., Solovieva T.V., Gerasimov S.A. et al. Handbook of structural materials. Moscow: Publ. house of Bauman Moscow State Tech. Univ., 2005, 640 p.
- Perkas M.D. Structure, properties and areas of application of high-strength maraging steels: textbook. Moscow: Mashinostroenie, 1986, 70 p.
- Bodyako M.N., Astapchuk S.A., Yaroshevich G.B. Martensitic aging steels. Minsk: Nauka i tekhnika, 1976, 246 p.
- Perkas M.D., Edneral A.F., Zhukov O.P. et al. On the Role of Cobalt in Strengthening Maraging Steels. Fizika metallov i materialovedenie, 1984, vol. 57, no. 2. Available at: https://eposlink.com/catalog/library/elibrary/book/fizika_metallov_i_metallovedenie-1975/publication/69815/ (accessed: March 14, 2026).
- Tonysheva O.A., Voznesenskaya N.M. Perspective high-strength corrosion-resistant steels alloyed with nitrogen (comparative analysis). Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 27–32. DOI: 10.18577/2071-9140-2014-0-3-27-32.
- Tarasenko L.V., Shalkevich A.B. Phase composition and strengthening of steels of the Fe–Cr–Ni–Co–Mo system with a martensitic-austenitic structure. Materialovedenie i termicheskaya obrabotka metallov, 2007, no. 4, pp. 32–37.
- Sukhov D.I., Nerush S.V., Yurkov M.A., Amirjanyan G.V. Studies of the structure and properties of metal-powder composites from corrosion-resistant steels obtained by gas atomization of the melt and intended for the manufacture of parts by selective laser melting. Voprosy materialovedeniya, 2018, no. 4 (96), pp. 97–106. DOI: 10.22349/1994-6716-2018-96-4-97-106.
- Bogachev I.A., Sulyanova E.A., Sukhov D.I., Mazalov P.B. Microstructure and properties investigations of Fe–Cr–Ni stainless steel obtained by selective laser melting. Trudy VIAM, 2019, no. 3 (75), pp. 3–13. Available at: http://www.viam-works.ru (accessed: March 20, 2025). DOI: 10.18577/2307-6046-2019-0-3-3-13.
- High-strength powder corrosion-resistant steel: pat. RU 2751064 C1; appl. 17.06.20; publ. 07.07.21.
- Sevalnev G.S., Klimov V.S., Vlasov I.I., Mazalova T.A. Study of mechanical properties of Fe–Cr–Ni–Co–Mo steel 3D-printed samples after various types of processing. Trudy VIAM, 2025, no. 6 (148), pp. 3–12. Available at: http://www.viam-works.ru (accessed: October 16, 2025). DOI: 10.18577/2307-6046-2025-0-6-3-12.
- Alekseeva M.S., Slobodskoy P.A., Lukina E.A., Yakusheva N.A. Patterns of structure formation for open-hearth steel of the Fe–Cr–Ni–Mo–Ti system during heat treatment. Trudy VIAM, 2024, no. 2 (132), pp. 3–12. Available at: http://www.viam-works.ru (accessed: May 21, 2025). DOI: 10.18577/2307-6046-2024-0-2-3-12.
- State Standard R 55079–2012. Steel. Method of Atomic Emission Analysis with Inductively Coupled Plasma. Moscow: Standartinform, 2016, 20 p.
- State Standard 17745–90. Steels and Alloys. Methods for Determining Gases. Moscow: Publishing House of Standards, 1990, 12 p.
- State Standard 12344–2003. Alloyed and High-Alloy Steels. Methods for Determining Carbon. Moscow: Standartinform, 2008, 15 p.
- State Standard 12345–2001. Alloyed and High-Alloy Steels. Methods for Determining Sulfur. Moscow: Standartinform, 2006, 23 p.
- State Standard R 8.777–2011. Dispersed Composition of Aerosols and Suspensions. Particle Sizing by Laser Diffraction. Moscow: Standartinform, 2012, 12 p.
- State Standard 1497–2023. Metals. Tensile Test Methods. Moscow: RST, 2024, 54 p.
- State Standard 11150–84. Metals. Tensile Test Methods at Low Temperatures. Moscow: Publ. House of Standards, 1993, 8 p.
- State Standard 9012–59. Metals. Brinell Hardness Measurement Method. Moscow: Standartinform, 2007, 40 p.
- Altiparmak S.C., Lombardi M., Bondioli F. et al. Hot isostatic pressing for powder-based additive manufacturing of metals: State-of-the-art review and future perspectives. Journal of Materials Research and Technology, 2025, vol. 39, pp. 4794–4822. DOI: 10.1016/j.jmrt.2025.10.135.
- Mazalov I.S., Mazalov P.B., Suhov D.I., Sulyanova E.A. Influence of hot isostatic pressing parameters on structure and properties of cobalt-based alloys obtained by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: April 21, 2025). DOI: 10.18577/2713-0193-2021-0-2-3-14.