The influence of metallurgical factors on the phase composition and technological characteristics of the nickel base solders with a high content of silicon and boron
Evgenov A.G., Galushka I.A., Shurtakov S.V., Ignatov V.A. The influence of metallurgical factors on the phase composition and technological characteristics of the nickel base solders with a high content of silicon and boron // Proceedings of VIAM. 2019. No. 2. DOI: 10.18577/2307-6046-2019-0-2-3-16. URL: https://viam-works.ru/en/journal/2019/2/1
Keywords
soldering, VPr27, VPr50, TEM, X-ray microanalisys, EDS, mapping.
Abstract
In this article the inspection of technological characteristics in Si content brazing alloys: VPr27 and VPr50 – in a cast form and a powder made by gas dispersion was carried out. Structure and a phase composition of brazing alloy characteristics such as spreading area and melting uniformity were researched. Comparative researches of brazing alloys consist of high purity materials and with technical Chrome purity were made. The reasons of unsatisfactory results of VPr27 spreading area tests were established. The Destabilising Cr influence, polluted by impurity intercalation, on doping system VPr50 brazing alloy, that leads to emergence of non-distinctive for cast materials compounds based on Cr–Mo, were shown.
Reference list
- Kablov E.N. Materialy novogo pokoleniya [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
- Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
- Afanasev-Khodykin A.N., Rylnikov V.S., Farafonov D.P. Tekhnologiya pajki poristo-voloknistogo materiala iz splava tipa «fekhral» dlya uplotneniya protochnoj chasti GTD [Technology soldering porous fibrous material of the alloy of the «fehral» to seal the flow part of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №1. St. 02. Available at: http://www.viam-works.ru (accessed: November 26, 2018). DOI: 10.18577/2307-6046-2014-0-1-2-2.
- Rylnikov V.S., Afanasev-Hodykin A.N., Galushka I.A. Tehnologiya pajki konstrukcii tipa «blisk» iz raznoimennyh splavov [Technology of the soldering of design of the blisk type from heteronymic alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №10. St. 02. URL: http://www.viam-works.ru (accessed: November 26, 2018).
- Stolyankov Yu.V., Aleksashin V.M., Antyufeeva N.V., Shheglova T.M. Ocenka stekloobrazuyushhej sposobnosti metallicheskoj sistemy na osnove nikelya tipa «metall–metalloid» [Glass-forming ability evaluation of the nickel-based «metall–metalloid» system] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 66–71. DOI: 10.185.77/2071-9140-2016-0-1-66-71.
- Plotnikova M.R., Glezer A.M. Megaplasticheskaya deformaciya amorfnogo splava na osnove nikelya [Severe plastic deformation of amorphous nickel-based alloy] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 10–13.
- Maksimova S.V. Amorfnyye pripoi dlya payki nerzhaveyushchey stali i titana i struktura payanykh soyedineniy [Amorphous solders for brazing stainless steel and titanium and the structure of brazed joints] // Adgeziya rasplavov i payka materialov, 2007. Vyp. 40. S. 70–81.
- Kablov E.N., Evgenov A.G., Rylnikov V.S., Afanasyev-Khodykin A.N. Issledovaniye melkodispersnykh metallicheskikh poroshkov pripoyev dlya diffuzionnoy vakuumnoy payki, poluchennykh metodom atomizatsii rasplava [Study of fine metal solder powders for diffusion vacuum soldering, obtained by the method of melt atomization] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2011. №SP2. S. 79–87.
- Ospennikova O.G., Lukin V.I., Afanasyev-Khodykin A.N., Galushka I.A., Shevchenko O.V. Perspektivnyye razrabotki v oblasti vysokotemperaturnoy payki zharoprochnykh splavov [Advanced developments in the field of the high-temperature soldering of heat resisting alloys] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 144–158. DOI: 10.18577/2071-9140-2017-0-S-144-158.
- Rylnikov V.S. Voprosy po pajke, reshennye v processe izgotovleniya izdeliya «Buran» [Some problems of brazing solved in the course of manufacture of «Buran» reusable spaceship] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 33–34.
- Chulkov E.I., Ivanov M.A., Belova E.A., Afanasyev-Khodykin A.N., Rylnikov V.S. Payka vysokotemperaturnym pripoyem truboprovodov iz stali 12Kh18N10T v zashchitnoy atmosfere s primeneniyem lokalnogo induktsionnogo nagreva [The soldering high-temperature solder of pipelines from steel 12Х18Н10Т in the protective atmosphere using local induction heating] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich zhurn. 2014. №5. St. 10. Available at: http://www.materialsnews.ru (accessed: November 26, 2018).
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Gnesin I.B. Eksperimentalnoye issledovaniye struktury i svoystv tverdykh rastvorov silitsidov molibdena i volframa i ikh primeneniye: avtoref. dis. … kand. tekhn. nauk [Experimental study of the structure and properties of solid solutions of molybdenum and tungsten silicides and their application: thesis abstract … Cand. Sc. (Tech.)]. Chernogolovka, 2008. 24 s.
- Tarasenko L.V., Titov V.I. Protsessy fazovoy nestabilnosti v zharoprochnykh stalyakh pri dlitelnykh nagrevakh [Phase instability processes in heat-resistant steels with prolonged heating] // Metallovedeniye i termicheskaya obrabotka metallov. 2005. №12. S. 10–15.
- Tarasenko L.V., Titov V.I. Intermetallicheskaya R-faza v martensitnostareyushchikh stalyakh sistemy Fe–Cr–Ni–Co–Mo [Intermetallic R-phase in maraging steel of the Fe–Cr–Ni–Co–Mo system] // Metallovedeniye i termicheskaya obrabotka metallov. 2006. №8. S. 44–48.
- Diagrammy sostoyaniya dvoynykh metallicheskikh sistem / pod red. N.P. Lyakisheva [Phase diagrams of double metallic systems / ed. by N.P. Lyakishev]. M.: Mashinostroyeniye, 1997. T. 2. 1023 s.
- Pouranvari M. Diffuzion brazing of a nickel based superalloy. Part 1: Solidification behavior // Mediterranean Journal of Mathematics. 2010. Vol. 16 (4). P. 241–247.