On the process of electrochemical copper during repair of parts from titanium alloys
Salakhova R.K., Tihobrazov A.B., Smirnova T.B. On the process of electrochemical copper during repair of parts from titanium alloys // Proceedings of VIAM. 2019. No. 12. DOI: 10.18577/2307-6046-2019-0-12-80-87. URL: https://viam-works.ru/en/journal/2019/12/9
Keywords
titanium alloys, copper plating electrolytes, deposition rate, adhesion, microhardness, chrome plating.
Abstract
The process of thick-layer electrochemical copper plating of VT6 titanium alloy has been tested as an alternative to the traditionally used chromium repair technology for restoring the geometric dimensions of worn parts. A method is presented for preparing the surface of titanium alloys for the deposition of a copper coating and the results of a study of the properties of a copper coating with a thickness of more than 100 μm obtained from a copper-plating pyrophosphate electrolyte based on potassium pyrophosphate. The adhesion strength of a copper coating with a titanium substrate is compared with a standard chromium coating.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Russia needs new generation materials] // Redkiye zemli. 2014. №3. S. 8–13.
- Dospekhi dlya «Burana». Materialy i tekhnologii VIAM dlya MKS «Energiya–Buran» / pod obshch. red. E.N. Kablova [Armor for the «Buran». VIAM materials and technologies for the ISS «Energiya–Buran» / gen. ed. E.N. Kablov]. M.: Nauka i zhizn, 2013. 128 s.
- Vinogradov S.S. Sozdaniye ekologicheski bezopasnogo galvanoproizvodstva na osnove ratsionalizatsii vodootvedeniya i reagentnogo metoda ochistki stokov [Creating environmentally friendly galvanic production based on the rationalization of wastewater and a reagent method of wastewater treatment] // Galvanotekhnika i obrabotka poverkhnosti. 2009. T. 17. №3. S. 24–29.
- Vinogradov S.S., Nikiforov A.A., Balahonov S.V. Zamena kadmiya. Etap 1. Povyshenie zashhitnoj sposobnosti cinkovyh pokrytij: termoimmersionnoe i modificirovannoe pokrytiya [Cadmium replacement. Part 1. Improving of protective property of zinc coatings: thermo-immersed and modified coatings] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 53–60. DOI: 10.18577/2071-9140-2015-0-4-53-60.
- Salahova R.K., Tihoobrazov A.B. Fiziko-himicheskie svojstva oksalatno-sulfatnogo elektrolita hromirovaniya, soderzhashhego nanorazmernye chasticy oksidov metallov [Physical and chemical properties of oxalate-sulfate chromium plating electrolyte, containing metal oxide nanoparticles] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 31–39. DOI: 10.18577/2071-9140-2016-0-4-31-39.
- Belov A.F., Benediktova G.P., Viskov A.S. i dr. Stroyeniye i svoystva aviatsionnykh materialov [The structure and properties of aviation material]. M.: Metallurgiya, 1989. 366 s.
- Pavlova T.V., Kashapov O.S., Nochovnaya N.A. Titanovye splavy dlya gazoturbinnykh dvigateley [Titanium alloys for gas turbine engines] // Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №5. S. 8–14.
- Antashov V.G., Nochovnaya N.A., Ivanov V.I. Tendentsii razvitiya zharoprochnykh titanovykh splavov dlya aviadvigatelestroyeniya [Trends in the development of heat-resistant titanium alloys for aircraft engine manufacturing] // Tekhnologiya legkikh splavov. 2002. №4. S. 72–76.
- Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Sostoyanie, problemy i perspektivy sozdaniya zharoprochnyh titanovyh splavov dlya detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 02. Available at: http://www.viam-works.ru (accessed: October 07, 2019).
- Azhogin F.F., Andreyev I.N., Kazakov V.A. i dr. Galvanicheskiye pokrytiya v mashinostroyenii: spravochnik [Galvanic coatings in mechanical engineering: a reference book]. M.: Mashinostroyeniye, 1985. 246 s.
- Yurkevich S.N., Polyakova T.L., Vashchenko I.M. i dr. Tekhnologiya naneseniya khromovogo pokrytiya na detali iz titanovykh splavov [The technology of applying a chrome coating to parts made of titanium alloys] // Galvanotekhnika i obrabotka poverkhnosti. 2017. T. 25. №3. S. 48–53.
- Salakhova R.K., Tikhoobrazov A.B., Smirnova T.B. Ob effektivnosti primeneniya penoobrazovatelya SHROM P-1 pri elektroliticheskom khromirovanii [On the effectiveness of CHROM P-1 foaming agent in electrolytic chromium plating] // Uprochnyayushchiye tekhnologii i pokrytiya. 2018. T. 14. №6 (162). S. 264–268.
- Morgunov Yu.A., Saushkin B.P. Additivnyye tekhnologii dlya aviakosmicheskoy tekhniki [Additive technologies for aerospace engineerin] // Additivnye tekhnologii. 2016. №1. S. 30–38.
- Sokolova I.A. Osobennosti tekhnologiy galvanicheskikh protsessov pri vosstanovlenii detaley mashin [Features of technologies of galvanic processes in the restoration of machine parts] // Izvestiya KGTU. 2010. №17. S. 94–98.
- Yampolskiy A.M. Medneniye i nikelirovanie [Copper plating and nickel plating]. L.: Mashinostroyenie, 1977. 112 s.
- Melnikov P.S. Spravochnik po galvanopokrytiyam v mashinostroyenii [Handbook of Electroplating in Mechanical Engineering]. M.: Mashinostroyeniye, 1991. 384 s.
- Kapustin Yu.I., Averina Yu.M., Nyrkov N.P. i dr. Issledovaniye protsessov skorostnogo medneniya iz sulfatnykh elektrolitov [Research of processes of speed copper plating from sulfate electrolytes] // Uspekhi v khimii i khimicheskoy tekhnologii. 2018. T. XXXII. №14. S. 26–29.
- Shluger M.A., Tok L.D. Galvanicheskiye pokrytiya v mashinostroyenii [Electroplated coatings in mechanical engineering]. M.: Mashinostroyeniye, 1985. T. 2. 248 s.
- Salakhova R.K., Tikhoobrazov A.B. Termostoykost elektroliticheskikh khromovykh pokrytiy [Thermal resistance of electrolytic chromium coatings] // Aviacionnye materialy i tehnologii. 2019. №2 (55). S. 60–67. DOI: 10.18577/2071-9140-2019-0-2-60-67.
- Klots M.U. Opyt khimicheskoy i elektrokhimicheskoy obrabotki detaley iz titanovykh splavov [Experience in chemical and electrochemical processing of parts made of titanium alloys]. L.: LDNTP. 1982. 24 s.
- Mikitchik A.V., Rudoy Yu.E., Grushetskiy I.V. i dr. Vliyaniye mnogosloynykh kondensatsionnykh pokrytiy na kharakteristiki dempfirovaniya titanovogo splava VT-6 [The effect of multilayer condensation coatings on the damping characteristics of VT-6 titanium alloy] // Sovremennaya elektrometallurgiya. 2016. №1 (122). S. 26–31.