Abstract
The article provides an overview of scientific and technical information in the field of high-temperature carbon plastics based on currently manufactured thermosetting binders with imide cycles and continuous carbon reinforcing fillers: comparative information on the assortment and properties of materials from various manufacturers, advantages and disadvantages, directions of application, an overview of developments and prospects for the development of work in the field of high-temperature carbon plastics at FSUE «VIAM».
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh sistem [The role of chemistry in the creation of new generation materials for complex technical systems] // Tez. dokl. XX Mendeleyevskogo syezda po obshchey i prikladnoy khimii. UrO RAN, 2016. S. 25–26.
- Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
- Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviaсionnye materialy i tehnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Valuyeva M.I., Gulyayev I.N. Uglerodnyye volokna i ugleplastiki: istoriya, sovremennost i perspektivy razvitiya. Obzor [Carbon fibers and carbon plastics: history, modernity and development prospects. Overview] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №11. S. 2–8.
- Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polimernyye kompozitsionnyye materialy novogo pokoleniya na osnove svyazuyushchego VSE-1212 i napolniteley, alternativnykh napolnitelyam firm Porcher Ind. i Toho Tenax [Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. AND Toho Tenax] // Aviacionnye materialy i tehnologii. 2018. №3 (52). S. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
- Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Kleyevyye prepregi – perspektivnyye materialy dlya detaley i agregatov iz PKM [Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
- Mikhaylin Yu.A. Teplo-, termo- i ognestoykost polimernykh materialov [Heat, heat and fire resistance of polymeric materials]. SPb.: Nauchnyye osnovy i tekhnologii, 2011. 416 s.
- Valuyeva M.I., Zelenina I.V., Akhmadieva K.R., Zharinov M.A., Khaskov M.A. Razrabotki FGUP «VIAM» v oblasti vysokotemperaturnykh ugleplastikov: napravleniya i perspektivy [Developments of FSUE VIAM in the field of high-temperature carbon plastics: directions and prospects] // Materialy IV Vseros. konf. «Rol fundamentalnykh issledovaniy pri realizatsii «Strategicheskikh napravleniy razvitiya materialov i tekhnologiy ikh pererabotki na period do 2030 goda» (g. Moskva, 28 iyunya 2018 g.). M.: VIAM, 2018. S. 71–76. 1 elektron. opt. disk (CD-ROM).
- Mikhaylin Yu.A. Termoustoychivyye polimery i polimernyye materialy [Heat-resistant polymers and polymeric materials]. SPb.: Professiya, 2006. 624 s.
- High temperature plastics market by type (polysulfones, polyimides, polyphenylene sulfide, fluoropolymers, and others), by end-use industries (electrical & electronic, transportation, industrial, medical, and others) – Global trends & forecast to 2019 // MarketsandMarketsTM. Available at: https://www.marketsandmarkets.com/Market-Reports/high-temperature-plastics-market-1192.html (accessed: November 17, 2019).
- Shama Rao N., Simha T.G.A., Rao K.P., Ravi Kumar G.V.V. Sarbon composites are becoming competetive and cost effective // Infosys Limited. Available at: https://www.infosys.com/ engineering-services/white-papers/documents/carbon-composites-cost-effective.pdf (accessed: November 17, 2019).
- High temperature resins market by resin type (BMI, cyanate ester, polyimide, thermoplastics, and others), by end-use industry type (aerospace & defense, transportation, and others), by manufacturing process type (prepreg layup, RTM, and orhers), and by region (North America, Europe, Asia-Pacific, and Rest the World), trend, forecast, competitive analysis, and growth opportunity: 2018–2023 // MarketResearch. Available at: https://www.marketresearch.com/Stratview-Research-v4143/High-Temperature-Composite-Resins-Resin-11797958/ (accessed: November 17, 2019).
- Kurnosov A.O., Raskutin A.E., Mukhametov R.R., Melnikov D.A. Polimernyye kompozitsionnyye materialy na osnove termoreaktivnykh poliimidnykh svyazuyushchikh [Polymer composite materials based on thermosetting polyimide binders] // Voprosy materialovedeniya. 2016. №4. S. 50–62.
- Kuznetsov A.A., Semenova G.K. Perspektivnyye vysokotemperaturnyye termoreaktivnye cvyazuyushchiye dlya polimernykh kompozitsionnykh materialov [Promising high-temperature thermosetting binders for polymer composite materials] // Rossiyskiy khimicheskiy zhurnal. 2010. T. 53. №4. S. 86–96.
- Other resins // NetComposites. Available at: https://netcomposites.com/guide/resin-systems/other-resins/ (accessed: November 17, 2019).
- Mikhaylin Yu.A. Termoustoychivyye polimery i polimernyye materialy na ikh osnove [Heat-resistant polymers and polymer materials based on them] // Polimernyye materialy. 2005. №8. S. 23–26.
- Fisher G. High temperature and toughened bismaleimide composite materials for aeronautics. Materials. Université de Lyon, 2015 // HAL archives-ouvertes. Available at: https://hal.archives-ouvertes.fr/tel-01299359 (accessed: November 17, 2019).
- Prepregi i smoly [Prepregs and resins] // Hexcel Corporation. Available at: http://www.hexcel.com/ (accessed: November 17, 2019).
- Prepregi Tenax® [Prepregs Tenax®] // Teijin Carbon Europe GmbH. Available at: https://www.teijincarbon.com/ru/produkcija/kompozity-tenaxr/tenaxr-prepreg (accessed: November 17, 2019).
- Teijin developes hightly heat- and impact-resistant prepreg as carbon fiber intermediate material for aerospace applications // Teijin Limited. Available at: https://www.teijin.com/news/2019/20190304_3521.html (accessed: November 17, 2019).
- Evonik for composites // Evonik Industries AG. Available at: https://www.rohacell.com/
- sites/lists/RE/DocumentsHP/Evonik-for-composites-EN.pdf (accessed: November 17, 2019).
- Global polyimides market // Market Litmus. Available at : https://marketlitmus.com/report-store/chemicals-and-materials/resins-and-polymers/global-polyimides-market/ (accessed: November 17, 2019).
- Yang S.-Y. Advance polyimide materials: synthesis, characterization, and applications. 1st ed. Elsevier, 2018. 498 p.
- Products // Solvay. Available at: https://www.solvay.com/en (accessed: November 17, 2019).
- Products // Maverick Corp. Available at: http://www.maverickcorp.com/ (accessed: November 17, 2019).
- Products // Ube Industries, Ltd. Available at: http://www.upilex.jp/ (accessed: November 17, 2019).
- Products // Nexam Chemical AB. Available at: http://www.nexamchemical.com/products/ (accessed: November 17, 2019).
- Tsampas S., Fernberg P., Joffe R. Development of novel high Tg polyimide-based composites. Part II: Mechanical characterization // Journal of Composite Materials. 2018. Vol. 52. No. 2. Р. 261–274.
- Fernberg P., Gong G., Mannberg P. Processing and properties of new polyimide composites with high temperature ability // ECCM16 – 16th European Conference on Composite Materials (Seville, Spain. June 22–26, 2014). Available at: http://www.escm.eu.org/eccm16/assets/0600.pdf (accessed: November 17, 2019).
- Publications // Swerea AB. URL: https://www.swerea.se/ (accessed: November 17, 2019).
- TenCate Corporate // Koninklijke Ten Cate bv. Available at: https://www.tencate.com/en/ (accessed: November 17, 2019).
- Product TC890 // Toray Advanced Composites. Available at: https://www.toraytac.com/product-explorer/products/mhdR/TC890 (accessed: November 17, 2019).
- Whitley K.S., Collins T.J. Mechanical Properties of T650-35/AFR-PE-4 at Elevated Temperatures for Lightweight Aeroshell Designs // NASA Langley Research Center. Available at: https://ntrs.nasa.gov/
- search.jsp?R=20060013437 2018-02-25T20:16:46+00:00Z (accessed: November 17, 2019).
- Ruslantsev A.N., Dumanskiy A.M., Portnova Ya.M. Modul polzuchesti ugleplastika BMI-3/3692 na osnove ravnoprochnoy tkani [Creep modulus of carbon fiber reinforced plastic BMI-3/3692 based on equally strong fabric] // Tez. dokl. XXI Mezhdunar. nauch.-tekhn. konf. «Konstruktsii i tekhnologii polucheniya izdeliy iz nemetallicheskikh materialov» (Obninsk, 5–7 okt. 2016 g.). Obninsk: ONPP «Tekhnologiya», 2017. S. 128–130.
- Volkov D.A., Popov A.G., Osaulenko A.V., Petrova O.L., Lititskaya V.A., Khandorina E.A. Issledovaniye vliyaniya tekhnologicheskikh faktorov i konfiguratsii obraztsov na znacheniye predela prochnosti pri szhatii ugleplastika na osnove preprega BMI-3/3692 [Investigation of the influence of technological factors and sample configuration on the value of compressive strength of carbon fiber based on the prepreg BMI-3/3692] // Tez. dokl. XXI Mezhdunar. nauch.-tekhn. konf. «Konstruktsii i tekhnologii polucheniya izdeliy iz nemetallicheskikh materialov» (Obninsk, 5–7 okt. 2016 g.). Obninsk: ONPP «Tekhnologiya», 2017. S. 168–170.
- Vorvul S.V., Mosiyuk V.N., Tomchani O.V. Podbor rezhimov dopolnitelnoy termoobrabotki svyazuyushchego BMI-3 metodom DMA [Selection of modes for additional heat treatment of a binder BMI-3 by the DMA method] // Tez. dokl. XXI Mezhdunar. nauch.-tekhn. konf. «Konstruktsii i tekhnologii polucheniya izdeliy iz nemetallicheskikh materialov» (Obninsk, 5–7 okt. 2016 g.). Obninsk: ONPP «Tekhnologiya», 2017. S. 178–181.
- Produktsiya [Products] // Institut plastmass. Available at: https://www.instplast.ru/ (accessed: November 17, 2019).
- Poliimidnoye svyazuyushcheye PRIS [Polyimide binder PRIS] // Superplast. Available at: http://superplast.ru/pris (accessed: November 17, 2019).
- Polimernyye svyazuyushchiye dlya kompozitsionnykh materialov kompanii proizvodstva OOO «Superplast» [Polymer binders for composite materials manufactured by Superplast LLC] // Superplast. Available at: http://dubna-oez.ru/images/data/gallery/299_3057_06_Sal_nikov_A.A._Polimernie_svyazuyuschie_
- dlya_kompozitsionnih_materialov_proizvodstva_OOO_%ABSuperplast%BB.pdf (accessed: November 17, 2019).
- Svyazuyushchiye dlya PKM [Binders for PCM] // ONPP «Tekhnologiya». Available at: https://technologiya.ru/files/1154/%D0%A1%D0%B2%D1%8F%D0%B7%D1%83%D1%8E%D1%89%D0%B8%D0%B5%20%D0%B4%D0%BB%D1%8F%20%D0%9F%D0%9A%D0%9C.pdf (accessed: November 17, 2019).
- Bismaleimidnyye svyazuyushchiye [Bismaleimide binders] // AO «INUMiT». Available at: https://inumit.ru/rus/produkciya-i-uslugi/ugleplastiki/Resins/bismaleimides/ (accessed: November 17, 2019).
- Produktsiya [Products] // Itecma. Available at: https://itecma.ru/products/ (accessed: November 17, 2019).
- Vaganov G.V., Yudin V.E., Elokhovskiy V.Yu. Ugleplastiki na osnove poroshkovykh poliimidnykh svyazuyushchikh, modifitsirovannykh uglerodnymi nanokonusami [CFRPs based on powder polyimide binders modified with carbon nanocones] // Polimernyye materialy i tekhnologii. 2015. T. 1. №1. S. 38–44.
- Mukhametov R.R., Akhmadiyeva K.R., Soloveva N.A., Gulyayev A.I. Povysheniye vodostoykosti bismaleimidnogo svyazuyushchego [Increase in water resistance of bismaleimide binder] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №5 (53). St. 08. Available at: http://www.viam-works.ru (accessed: November 17, 2019). DOI: 10.18577/2307-6046-2017-0-5-8-8.
- Muhametov R.R., Dolgova E.V., Merkulova Yu.I., Dushin M.I. Razrabotka bismaleimidnogo termostoikogo svyazuiushchego dlya kompozitsionnyh materialov aviacionnogo naznacheniya [Development of heat-resistant bismaleimide binder for composites for aeronautical application] // Aviacionnye materialy i tehnologii. 2014. №4 (33). S. 53–57. DOI: 10.18577/2071-9140-2014-0-4-53-57.
- Sposob polucheniya rasplavnykh poliimidnykh svyazuyushchikh polimerizatsionnogo tipa: pat. 2666734 Ros Federatsiya. №2017135540 [A method of producing melt polyimide binders of the polymerization type: US Pat. 2666734 Rus. Federation. No. 2017135540]; zayavl. 05.10.17; opubl. 12.09.18.
- Zharinov M.A., Shimkin A.A., Akhmadiyeva K.R., Zelenina I.V. Osobennosti i svoystva rasplavnogo poliimidnogo svyazuyushchego polimerizatsionnogo tipa [Features and properties of solvent-free PMR-type polyimide resin] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №12 (72). St. 05. Available at: http://www.viam-works.ru (accessed: November 17, 2019). DOI: 10.18577/2307-6046-2018-0-12-46-53.