On technological approaches to the creation of composite materials based on nickel monoaluminide NiAl (review)

Karashaev M.M., Lomberg B.S., Bakradze M.M., Letnikov M.N.
Karashaev M.M., Lomberg B.S., Bakradze M.M., Letnikov M.N. On technological approaches to the creation of composite materials based on nickel monoaluminide NiAl (review) // Proceedings of VIAM. 2019. No. 12. DOI: 10.18577/2307-6046-2019-0-12-55-66. URL: https://viam-works.ru/en/journal/2019/12/7
Keywords
nickel monoaluminide NiAl, directional crystallization, thermomechanical treatment, infiltration, mechanical activation, deformation-diffusion solid-phase association, intermetallic.
Abstract

 

The article discusses the main technological features of the formation of natural and artificial composite structures based on NiAl compound. It is shown that this kind of materials can be obtained by directional crystallization methods and by technology, including thermomechanical processing, as well as using mechanical activation methods followed by controlled reaction synthesis, forced and reaction infiltration with a matrix-forming melt, and deformation-diffusion solid-phase combination. Some experimental and theoretical calculations based on multicomponent phase diagrams that allow the creation of such materials using the above methods are presented and generalized. Based on the data obtained conclusions are drawn about further paths in the development and creation of materials based on nickel monoaluminide NiAl.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Petrushin N.V., Ospennikova O.G., Elyutin E.S. Renij v monokristallicheskih zharoprochnyh nikelevyh splavah dlya lopatok gazoturbinnyh dvigatelej [Rhenium in single crystal nickel-based superalloys for gas turbine engine blades] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 5–16. DOI: 10.18577/2071-9140-2014-0-s5-5-16.
  3. Ospennikova O.G. Tendencii sozdaniya zharoprochnyh nikelevyh splavov nizkoj plotnosti s polikristallicheskoj i monokristallicheskoj strukturoj (obzor) [Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review)] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 3–19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
  4. Bondarenko Yu.A., Bazyleva O.A., Rayevskikh A.N., Narskiy A.R. Issledovaniya po sozdaniyu novoy vysokotemperaturnoy zharostoykoy matritsy na osnove intermetallidov NiAl–Ni3Al [Research on the creation of a new high-temperature heat-resistant matrix based on intermetallic compounds NiAl–Ni3Al] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №11 (71). St. 01. Available at: http://www.viam-works.ru (accessed: November 06, 2019). DOI: 10.18577/2307-6046-2018-0-11-3-11.
  5. Povarova K.B., Lomberg B.S., Filin S.A. i dr. Struktura i svoystva (b+γ)-splavov sistemy Ni–Al–Co [Structure and properties of (β+γ) alloys of the Ni–Al–Co system] // Metally. 1994. №3. S. 1–14.
  6. Noebe R.D., Misra A., Gibala R. Plastic flow and fracture of NiAl-based alloys containing a ductile second phase // Iron and Steel Institute of Japan. 1991. Vol. 31. No. 10. P. 1172–1185.
  7. Petrushin N.V., Bronfin M.B., Chabina E.B., Dyachkova L.A. Fazovyye prevrashcheniya i struktura napravlenno zakristallizovannykh intermetallidnykh splavov Ni–Al–Re [Phase transformations and the structure of directionally crystallized Ni–Al–Re intermetallic alloys] // Metally. 1994. №3. S. 30–47.
  8. Bazyleva O.A., Turenko Ye.YU., Shestakov A.V. Vliyaniye termicheskoy obrabotki na mikrostrukturu i mekhanicheskiye svoystva splava na osnove intermetallida NiAl // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2014. №9. St. 02. URL: http://www.viam-works.ru (data obrashcheniya: 06.11.2019). DOI: 10.18577/2307-6046-2014-0-9-2-2.
  9. Hubert-Protopopescu M., Hubert H. Aluminium-cobalt-nickel // Ternary alloys: a comprehensive compendium of evaluated constitutional data and phase diagrams. Weinheim–N.Y.: VCH Cop., 1991. P. 234–244.
  10. Kornilov I.I. Fiziko-khimicheskiye osnovy zharoprochnosti splavov [Physicochemical fundamentals of heat resistance of alloys]. M.: Izd-vo AN SSSR, 1961. 516 s.
  11. Kornilov I.I., Mints R.S. Issledovaniye sistemy Ni–Cr–NiAl [Investigation of the Ni–Cr–NiAl system] // Neorganicheskaya khimiya. 1958. T. III. Vyp. 5. S. 699–707.
  12. Kablov E.N., Bondarenko Yu.A., Echin A.B. Razvitiye tekhnologii napravlennoy kristallizatsii liteynykh vysokozharoprochnykh splavov s peremennym upravlyayemym temperaturnym gradiyentom [Development of technology of cast superalloys directional solidification with variable controlled temperature gradient] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  13. Povarova K.B., Kazanskaya N.K., Lomberg B.S. i dr. Fazovyy sostav i struktura splavov na osnove NiAl sistem Ni–Al–Co–M, gde M–Ti, Zr, Hf, V, Nb, Ta, Cr, Mo [Phase composition and structure of alloys based on NiAl Ni–Al–Co–M systems, where M is Ti, Zr, Hf, V, Nb, Ta, Cr, Mo] // Metally. 1996. №3. S. 1–19.
  14. Povarova K.B., Kazanskaya N.K., Lomberg B.S., Bondarenko Yu.A., Shkolnikov D.Yu. Konstruktsionnyye zharoprochnyye (b+γ)-splavy na osnove NiAl s povyshennoy nizkotemperaturnoy plastichnostyu [Heat-resistant structural (β+γ)-alloys based on NiAl with increased low-temperature ductility] // Metallurg. 1996. №5. S. 1–9.
  15. Povarova K.B., Filin S.A., Maslenkov S.B. Fazovyye ravnovesiya s uchastiyem b-fazy v sistemakh Ni–Al–Me (Me–Co, Fe, Mn, Cu) pri 900 i 1100°C [Phase equilibria involving the β phase in Ni–Al–Me systems (Me–Co, Fe, Mn, Cu) at 900 and 1100°С] // Metally. 1993. №1. S. 191–205.
  16. Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Issledovanie kompozicij sistemy Ni–Al–Co pri razrabotke novogo zharoprochnogo deformiruemogo intermetallidnogo splava [Investigation experimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. № 10. St. 01. Available at: http://www.viam-works.ru (accessed: November 06, 2019).
  17. Kablov E.N., Ospennikova O.G., Kucheryaev V.V., Rozenenkova V.A. i dr. Termomekhanicheskoye povedeniye intermetallidnykh splavov sistemy Ni–Al–Co i Ti–Al–Nb pri izotermicheskoy deformatsii [Thermomechanical behavior of intermetallic alloys of the Ni–Al–Co and Ti–Al–Nb systems under isothermal deformation] // Pisma o materialakh. 2016. T. 6. №3 (23). S. 189–194.
  18. Kablov E.N., Abuzin Yu.A., Shavnev A.A., Efimochkin I.Yu. Tekhnologicheskaya baza dlya issledovaniya, razrabotki i proizvodstva metallicheskikh kompozitsionnykh materialov [Technological base for research, development and production of metal composite materials] // 75 let. Aviacionnye materialy. Izbrannyye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 249–255.
  19. Shahzad A., Abuzin Yu., Karashaev M. In situ fabrication of NixAlx intermetallic reinforcement particles and of Al-matrix composite reinforced with those particles // Nanoscience and Technology: An International Journal. 2017. Vol. 8 (3). P. 211–222.
  20. Abuzin Yu.A., Karashayev M.M., Sokolov R.A. Samorazogrev mekhanicheski aktivirovannykh elementarnykh metallicheskikh poroshkov [Self-heating of mechanically activated elementary metal powders] // Uspekhi sovremennoy nauki. 2016. T. 3. S. 123–128.
  21. Abuzin Yu.A., Karashayev M.M. Issledovaniye alyumotermicheskikh reaktsiy v poroshkovykh sistemakh Nb2O5 (WO3; MoO3; Fe2O3; NiO)-Al posle mekhanicheskoy aktivatsii [Investigation of aluminothermic reactions in powder systems Nb2O5 (WO3; MoO3; Fe2O3; NiO)-Al after mechanical activation] // Mezhdunarodnyy nauchno-issledovatelskiy zhurnal. 2016. №7 (49). S. 6–9. DOI: 10.18454/IRJ.2016.49.036.
  22. Abuzin Yu., Karashaev M.M., Sokolov R.A. Evaluation of Energy Efficiency of the Alumothermic Process of Producing Metal Composite Materials by the Criteria of the Maximum Self-Heating Temperature and the Aggregate State of Oxygen Exchange Reaction Products // Nanomechanics Science and Technology: An International Journal. 2015. Vol. 6 (4). P. 299–304.
  23. Lurie S., Abuzin Yu., Sokolov R., Karashaev M., Belov P. Experimental and Theoretical Study of Mass Transport during Annealing of Mechanically Activated Composite Granules of Ni–Al System // International Journal of Engineering and Innovative Technology. 2014. Vol. 4. Iss. 5. P. 194–200.
  24. Sposob polucheniya izdeliya iz metallicheskogo kompozitsionnogo materiala: pat. 2283726 S1 Ros. Federatsiya [A method of obtaining a product from a metal composite material: pat. 2283726 C1 Rus. Federation]; zayavl: 17.02.05; opubl. 20.09.06.
  25. Sposob polucheniya izdeliya iz metallicheskogo kompozitsionnogo materiala: pat. 2283727 S1 Ros. Federatsiya [A method of obtaining a product from a metal composite material: pat. 2283727 C1 Rus. Federation]; zayavl: 17.02.05; opubl. 20.09.06.
  26. Krasnov E.I., Shtejnberg A.S., Shavnev A.A., Berezovskij V.V. Issledovanie sloistogo metallicheskogo kompozicionnogo materiala sistemy Ti–TiAl3 [Study of Ti–TiAl3 laminate metal composite material ] // Aviacionnye materialy i tehnologii. 2013. №3. S. 16–19.
  27. Sposob polucheniya kompozitsionnogo materiala: pat. 2394665 S1 Ros. Federatsiya [A method of obtaining a composite material: pat. 2394665 C1 Rus. Federation]; zayavl. 31.03.09; publ. 20.07.10.
  28. Zhabin A.N., Serpova V.M., Grishina O.I., Shavnev A.A. Issledovaniye formirovaniya fazovogo sostava matritseobrazuyushchego alyuminidnogo splava dlya vysokotemperaturnykh metallicheskikh kompozitsionnykh materialov [Research of phase composition formation of the matrix forming aluminide alloy for high temperature metallic composite materials] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 18–21. DOI: 10.18577/2071-9140-2016-0-2-18-21.
  29. Sposob polucheniya izdeliya iz zharoprochnogo kompozitsionnogo materiala: pat. 2346997 S2 Ros. Federatsiya [A method of obtaining a product from a heat-resistant composite material: pat. 2346997 C2 Rus. Federation]; zayavl. 15.11.06; opubl. 20.02.09.