Microstructure changes during MCrAlY bond coats oxidation (review)
UDC
629.7.023.224
DOI
10.18577/2307-6046-2019-0-10-50-60
Article PDF (Russian)
(896.56 KB)
How to cite
Movenko D.A., Medvedev P.N. Microstructure changes during MCrAlY bond coats oxidation (review) // Proceedings of VIAM. 2019. No. 10. DOI: 10.18577/2307-6046-2019-0-10-50-60. URL: https://viam-works.ru/en/journal/2019/10/5
Keywords
TBC, bond coat, TGO, isothermal oxidation, microstructure evolution, interdiffusion.
Abstract
The state of the question of structure changing of MCrAlY bond coats during isothermal oxidation is studied. The influence of coating methods on their structure during long-term oxidation is shown. Criteria for assessing the lifetime of thermal barrier coatings with MCrAlY bond coats are shown. The influence of the composition and morphology of thermally grown oxide on the oxidation intensity of the bond coat and its adhesion to the ceramic layer of the thermal barrier coating are presented.
Reference list
- Kablov E.N., Muboyadzhyan S.A. Teplozashchitnyye pokrytiya s keramicheskim sloyem ponizhennoy teploprovodnosti na osnove oksida tsirkoniya dlya lopatok turbiny vysokogo davleniya perspektivnykh GTD [Heat-insulating coatings with a ceramic layer of reduced thermal conductivity based on zirconium oxide for high-pressure turbine blades of promising gas turbine engines] // Sb. dokl. konf. «Sovremennyye dostizheniya v oblasti sozdaniya perspektivnykh nemetallicheskikh kompozitsionnykh materialov i pokrytiy dlya aviatsionnoy i kosmicheskoy tekhniki» M.: VIAM, 2015. St. 3.
- Budinovskij S.A., Chubarov D.A., Matveev P.V. Sovremennye sposoby naneseniya teplozashhitnyh pokrytij na lopatki gazoturbinnyh dvigatelej (obzor) [Modern methods for deposition of thermal barrier coatings on GTE turbine blades] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 38–44. DOI: 10.18577/2071-9140-2014-0-s5-38-44.
- Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlya rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Receiving ceramic heat-protective coatings for working blades of turbines of aviation GTD magnetronny method] // Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.
- Kablov e.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye polifunktsionalnye vysokotemperaturnye pokrytiya dlya nikelevykh splavov, uplotnitelnykh metallicheskikh voloknistykh materialov i berilliyevykh splavov [Modern multifunctional high-temperature coatings for nickel alloys, sealing metal fibrous materials and beryllium alloys] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2013. №1. St. 05. Available at: http://www. materialsnews.ru (accessed: July 10, 2019).
- Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
- Matveev P.V., Budinovskij S.A., Chubarov D.A. Tehnologiya polucheniya ionno-plazmennyh zharostojkih podsloev s povyshennym soderzhaniem alyuminiya dlya perspektivnyh TZP [Technology for production of ion-plasma heat-resistant bonding sub-layers with increased aluminum content for advanced TBCs] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 56–60. DOI: 10.18577/2071-9140-2014-0-s5-56-60.
- Naumenko D., Shemet V., Singheiser L., Quadakkers W.J. Failure mechanisms of thermal barrier coatings on MCrAlY-type bondcoats associated with the formation of the thermally grown oxide // Journal of Materials Science. 2009. Vol. 44. P. 1687–1703.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Mauer G., Sebold D., Vaßen R. et al. Impact of processing conditions and feedstock characteristics on thermally sprayed MCrAlY bondcoat properties // Surface and Coatings and Technology. 2017. Vol. 318. P. 114–121.
- Ichikawa Y., Ogawa K. Critical deposition condition of CoNiCrAlY cold spray based on particle deformation behavior // Journal of Thermal Spray Technology. 2017. Vol. 26. P. 340–349.
- Gavendová P., Čížek J., Čupera J. et al. Microstructure modification of CGDS and HVOF sprayed CoNiCrAlY bond coat Remelted by electron beam // Procedia Material Science. 2016. Vol. 12. P. 89–94.
- Doleker K.M., Karaoglanli A.C. Comparison of oxidation behavior of shot-peened plasma spray coatings with cold gas dynamic spray coatings // Oxidation of Metals. 2017. Vol. 88. P. 121–132.
- Tolpygo V.K., Clarke D.R. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation // Acta Materialia. 2000. Vol. 48. Issue 13. P. 3283–3293.
- Belzunce F.J., Higuera V., Poveda S. High temperature oxidation of HFPD thermal-sprayed MCrAlY coatings // Materials Science and Engineering: A. 2001. Vol. 297, Issues 1–2. P. 162–167.
- Prieto-García E., Baldenebro-Lopez F.J., Estrada-Guel I. et al. Microstructural evolution of mechanically alloyed Ni-based alloys under high temperature oxidation // Powder Technology. 2015. Vol. 281. P. 57–64.
- Richer P., Yandouzi M., Beauvais L., Jodoin B. Oxidation behaviour of CoNiCrAlY bond coats produced by plasma, HVOF and cold gas dynamic spraying // Surface and Coatings Technology. 2010. Vol. 204. P. 3962–3974.
- Wei P., Wei Z., Zhao G. et al. The analysis of melting and refining process for in-flight particles in supersonic plasma spraying // Computer Material Science. 2015. Vol. 103. P. 8–19.
- Poza P., Grant P.S. Microstructure evolution of vacuum plasma sprayed CoNiCrAlY coatings after heat treatment and isothermal oxidation // Surface and Coatings Technology. 2006. Vol. 201. P. 2887–2896.
- Li Y., Li C.-J., Yang G.-J., Xing L.-K. Thermal fatigue behavior of thermal barrier coatings with the MCrAlY bond coats by cold spraying and low-pressure plasma spraying // Surface Coatings and Technology. 2010. Vol. 205. P. 2225–2233.
- Chen H. Microstructure characterization of un-melted particles in a plasma sprayed CoNiCrAlY coating // Materials Characterization. 2017. P. 1–8.
- Shibata M., Kuroda S., Murakami H. et al. Comparison of Microstructure and Oxidation Behavior of CoNiCrAlY Bond Coatings Prepared by Different Thermal Spray Processes // Material Translations. 2006. Vol. 47 (7). P. 1638–1642.
- Yilbas B.S., Al-Zaharnah I., Sahin A. HVOF Coating and Characterization // Flexural Testing of Weld Site and HVOF Coating Characteristics. Materials Forming, Machining and Tribology. Springer, Berlin, Heidelberg, 2014. 176 p.
- Mercier D., Gauntt B.D., Brochu M. Thermal stability and oxidation behavior of nanostructured NiCoCrAlY coatings // Surface & Coatings Technology. 2011. Vol. 205. P. 4162–4168.
- Tang F., Ajdelsztajn L., Schoenung J.M. Influence of Cryomilling on the Morphology and Composition of the Oxide Scales Formed on HVOF CoNiCrAlY Coatings // Oxidation of Metals. 2004. Vol. 61. Issue 3–4. P. 219–238.
- Алхимов А.П., Клинков С.В., Косарев В.Ф., Фомин В.М. Холодное газодинамическое напыление. Теория и практика. М.: Физ.-мат. лит., 2010. 536 с.
- Zhang Q., Li C.-J., Li C.X. et al. Study of Oxidation Behavior of Nanostructured NiCrAlY Bond Coatings Deposited by Cold Spraying // Surface and Coatings Technology. 2008. Vol. 202. Issue 14. P. 3378–3384.
- Ajdelsztajn L., Zuniga A., Jodoin B., Lavernia E. Cold gas dynamic spraying of a high temperature Al alloy // Surface and Coatings Technology. 2006. Vol. 201. Issue 6. P. 2109–2116.
- Borchers C., Gärtner F., Stoltenhoff T. Microstructural and macroscopic proper-ties of cold sprayed copper coatings // Journal of Applied Physics. 2003. Vol. 93. Issue 12. P. 1063–1069.
- Dykhuizen R.C., Smith M.F. Gas dynamic principles of cold spray // Journal of Thermal Spray Technology. 1998. Vol. 7. Issue 2. P. 205–212.
- Stoltenhoff T., Kreye H., Richter H.J. An analysis of the cold spray process and its coatings // Journal of Thermal Spray Technology. 2002. Vol. 11. Issue 4. P. 542–550.
- Wright P.K., Evans A.G. Mechanisms governing the performance of thermal bar-rier coatings // Current Opinion in Solid State and Materials Science. 1999. Vol. 4. Issue 3. P. 255–265.
- Messaoudi K., Huntz A.M. Diffusion and growth mechanism of Al2O3 scales on ferritic Fe-Cr-Al alloys // Materials Science and Engineering: A. 1998. Vol. 247. Issues 1–2. P. 248–262.
- Hesnawi A., Li H., Zhou Z. et al. Isothermal oxidation behaviour of EB-PVD MCrAlY bond coat // Vacuum. 2007. Vol. 81. Issue 8. P. 947–952.
- Leyens C., Wright I.G., Pint B.A. Effect of Experimental Procedures on the Cy-clic, Hot-Corrosion Behavior of NiCoCrAlY-Type Bondcoat Alloys // Oxidation of Metals. 2000. Vol. 54. Issue 3–4. P. 255–276.
- Wefer K., Misra C. Oxides and Hydroxides of Aluminum. New York: Wiley, 1987. 92 p.
- Pint B., Treska M., Hobbs L. The effect of various oxide dispersions on the phase composition and morphology of Al2O3 scales grown on β-NiAl // Oxidation of Metals. 1997. Vol. 47. Issue 1–2. P. 1–20.
- Pieraggi B., Rapp R.A. Stress generation and vacancy annihilation during scale growth limited by cation-vacancy diffusion // Acta Metallurgica. 1988. Vol. 36. Issue 5. P. 1281–1289.
- Brumm M.W., Grabke H.J., Wagemann B. The oxidation of NiAl-III. Internal and intergranular oxidation // Corrosion Science. 1994. Vol. 36. Issue 1. P. 37–53.
- Hejrani E., Sebold D., Nowak W.J. et al. Isothermal and cyclic oxidation behavior of free standing MCrAlY coatings manufactured by high-velocity atmospheric plasma spraying // Surface and Coatings Technology. 2017. Vol. 313. P. 191–201.
- Yuan K., Peng R.L., Li X.H. et al. Some aspects of elemental behaviour in HVOF MCrAlY coatings in high-temperature oxidation // Surface and Coatings Technology. 2015. Vol. 261. P. 86–101.
- Movenko D.A., Medvedev P.N., Smirnov A.A. Issledovaniye izmeneniya struktury teplozashchitnogo pokrytiya posle ispytaniy na zharostoykost [Study of changes in the heat-resistant alloy coating structure after heat resistance tests] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №11 (71). St. 08. Available at: http://www.viam-works.ru (accessed: July 12, 2019). DOI: 10.18577/2307-6046-2018-0-11-64-73.
- Rinaldi C., Mandelli M. The role of diffusion and oxidation kinetics in a coating life prediction code: application to components // ASME Turbo Expo 2009: Power for Land, Sea, and Air: Proceedings Series. 2009. Vol. 4: Cycle Innovations; Industrial and Cogeneration; Manufacturing Materials and Metallurgy; Marine. P. 893–902.
- Yuan K., Eriksson R., Lin Peng R. et al. Modeling of microstructural evolution and lifetime prediction of MCrAlY coatings on nickel based superalloys during high temperature oxidation // Surface and Coatings Technology. 2013. Vol. 232. P. 204–215.
- Thoma M., Scrivani A. Prolonged MCrAlY coating lifetime by means of the LPPS process // Proceedings of Conference ASME Turbo Expo. 2013. P. 535–543.
- Yi H.C., Guan S.W., Smeltzer W.W., Petric A. Internal oxidation of NiAl and NiAlSi alloys at the dissociation pressure of NiO // Acta Metallurgy Materials. 1994. Vol. 42. P. 981–990.
- Reed R.C. The superalloys: fundamentals and applications. Cambridge University Press, 2006. 372 p.
- Sato A., Harada H., Yokokawa T. et al. The effects of ruthenium on the phase stability of fourth generation Ni-base single crystal superalloys // Scripta Materialis. 2006. Vol. 54. P. 1679–1684.
- Zhang P., Yuan K., Peng R.L. et al. Long-term oxidation of MCrAlY coatings at 1000°C and an Al-activity based coating life criterion // Surface & Coatings Technology. 2017. Vol. 36. P. 1–10.
- Liu Y.Z., Zheng S.J., Zhu Y.L. et al. Microstructural evolution at interfaces of thermal barrier coatings during isothermal oxidation // Journal of European Ceramic Society. 2016. Vol. 36. P. 1765–1774.
- Ahmadian S., Jordan E.H. Explanation of the effect of rapid cycling on oxidation, rumpling, microcracking and lifetime of air plasma sprayed thermal barrier coatings // Surface & Coatings Technology. 2014. Vol. 244. P. 109–116.
- Cai J., Guan Q.F., Hou X.L. et al. Isothermal oxidation behaviour of thermal barrier coatings with CoCrAlY bond coat irradiated by highcurrent pulsed electron beam // Applied Surface Science. 2014. Vol. 317. P. 360–369.
- Wang F., Lou H., Zhu S., Wu W. The mechanism of scale adhesion on sputtered microcrystallized CoCrAl films // Oxidation of Metals. 1994. Vol. 45. Issue 1–2. P. 39–50.
- Wang F. The effect of nanocrystallization on the selective oxidation and adhesion of Al2O3 scales // Oxidation of Metals. 1997. Vol. 48. Issue 3–4. P. 215–224.
- Pint B.A., Alexander K.B. Grain boundary segregation of cation dopants in a-Al2O3 scales // Fundamental Aspects of High Temperature Corrosion. Electrochemical Society, Pennington, 1996. Vol. VI. 97 p.
- Pint B.A., More K.L., Wright I.G. Characterization of thermally cycled alumina scales. Materials of High Temperature. 2000. Vol. 17. Issue 1. P. 165–171.
- Subanovic M., Song P., Wessel E. et al. Effect of exposure conditions on the oxi-dation of MCrAlY-bondcoats and lifetime of thermal barrier coatings // Surface & Coatings Technology. 2009. Vol. 204. P. 820–823.
- Yang L.X., Zou Z.H., Kou Z.D. et al. High temperature stress and its influence on surface rumpling in NiCoCrAlY bond coat // Acta Materialia. 2017. Vol. 139. P. 122–137.
- Chen H., Si Y.Q., McCartney D.G. An analytical approach to the β-phase coars-ening behaviour in a thermally sprayed CoNiCrAlY bond coat alloy // Journal of Alloys Compounds. 2017. Vol. 704. P. 359–365.
- Jiang J.S., Zou Z.H., Wang W.Z. et al. Effect of internal oxidation on the inter-facial morphology and residual stress in air plasma sprayed thermal barrier coatings // Surface & Coatings Technology. 2018. Vol. 334. P. 215–226.
- Weng W.-X., Wang Y.-M., Liao Y.-M. et al. Comparison of microstructural evolution and oxidation behaviour of NiCoCrAlY and CoNiCrAlY as bond coats used for thermal barrier coatings // Surface & Coatings Technology. 2018. Vol. 352. P. 285–294.
- Mercier D., Kaplin C., Goodall G. et al. Parameters influencing the oxidation behavior of cryomilled CoNiCrAlY // Surface & Coatings Technology. 2010. Vol. 205. P. 2546–2553.