Carbon fibers composite material on the basis of volume reinforcing triax braiding preformes
Donetskiy K.I., Karavaev R.Y., Raskutin A.E., Dun V.A. Carbon fibers composite material on the basis of volume reinforcing triax braiding preformes // Proceedings of VIAM. 2019. No. 1. DOI: 10.18577/2307-6046-2019-0-1-55-63. URL: https://viam-works.ru/en/journal/2019/1/7
Keywords
reinforcing braided preforms, carbon fibers composite material, epoxy binding, vacuum infusion, reinforcing corner, physicomechanical properties, outside hydrostatic pressure.
Abstract
In work it is considered carbon fibers composite on the basis of volume reinforcing triax braiding preformes, made in the way of vacuum infusion with use of the molten epoxy binding. Possible scopes of such material and its physicomechanical properties are given. It is shown that when manufacturing the designs working at influence of outside hydrostatic pressure, important task is decrease in their weight and dimensional characteristics. Application carbon fibers composite on the basis of volume reinforcing braiding preformes will allow to improve weight characteristics that will lead in turn to increase of technical characteristics of made designs.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
- Borshchev A.V., Gusev Yu.A. Polimernye kompozicionnye materialy v avtomobilnoj promyshlennosti [Polymer composite materials in automotive industry] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 34–38.
- Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Kablov E.N., Startsev V.O., Inozemtsev A.A. Vlagonasyshhenie konstruktivno-podobnyh elementov iz polimernyh kompozicionnyh materialov v otkrytyh klimaticheskih usloviyah s nalozheniem termociklov [The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
- Braided reinforcement for aircraft fuselage frames and method of producing the same: pat. 8210086B2 US; publ. 03.07.12.
- Dushin M.I., Doneckij K.I., Karavaev R.Yu. Ustanovlenie prichin obrazovaniya poristosti pri izgotovlenii PKM [Identification of the reasons of porosity formation when manufacturing composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6 (42). St. 08. Available at: http://www.viam-works.ru (accessed: December 14, 2018). DOI: 10.18577/2307-6046-2016-0-6-8-8.
- Donetskij K.I., Hrulkov A.V., Kogan D.I., Belinis P.G., Lukyanenko Yu.V. Primenenie obemno-armiruyushhih preform pri izgotovlenii izdelij iz PKM [Use of three-dimensional reinforcing preforms during the production of polymer composite products] // Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
- Vlasenko F.S., Raskutin A.E., Doneckij K.I. Primenenie pletenyh preform dlya polimernyh kompozicionnyh materialov v grazhdanskih otraslyah promyshlennosti (obzor) [Application of braided preforms for polymer composite materials in civil industries (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 05. Available at: http://www.viam-works.ru (accessed: December 14, 2018). DOI: 10.18577/2307-6046-2015-0-1-5-5.
- Erber A., Birkefeld K., Drechsler K. The influence of braiding configuration on damage tolerance of drive shafts // SAMPE EUROPE: 30th International Jubilee Conference and Forum. 2010. P. 364–371.
- Branscomb D., Beale D., Broughton R. New directions in braiding // Journal of Engineered Fibers and Fabrics. 2013. No. 8 (2). R. 11–24.
- Donetskij K.I., Kogan D.I., Hrulkov A.V. Svojstva polimernyh kompozicionnyh materialov, izgotovlennyh na osnove pletenyh preform [Properties of the polymeric composite materials made on the basis of braided preforms] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 05. Available at: http://www.viam-works.ru (accessed: December 14, 2018). DOI: 10.18577/2307-6046-2014-0-3-5-5.
- Lebel L.L., Nakai A. Design and manufacturing of an L-shaped thermoplastic composite beam by braid-trusion // Composites. Part A: Applied Science and Manufacturing. 2012. No. 43 (10). P. 1717–1729.
- Kohlman L.W., Bail J.L., Roberts G.D. et al. A notched coupon approach for tensile testing of braided composites // NASA Publications. 2012. No. 65. P. 1–9.
- Dun V.A., Petrovskiy O.L., Rumyantsev A.F., Ushakov P.G. Rezultaty primeneniya ugleplastika dlya izgotovleniya malogabaritnykh korpusov [The results of carbon fiber for the manufacture of small buildings] // Sudostroitelnaya promyshlennost, seriya PVMO. 1986. Vyp. 2. S. 70–75.
- Kompozitnyy korpus glubokovodnogo tekhnicheskogo sredstva: pat. 2453464 Ros. Federatsiya [Composite hull deep-sea technical means: pat. 2453464 Rus. Federation]; zayavl. 17.08.10; opubl. 20.06.12.
- Carey J.P. Handbook of Advances in Braided Composite Materials. Woodhead Publishing is an Imprint of Elsevier, 2017. No. 72. R. 3–6.
- Chursova L.V., Babin A.N., Panina N.N., Tkachuk A.I., Terekhov I.V. Ispolzovaniye aromaticheskikh aminnykh otverditeley dlya sozdaniya epoksidnykh svyazuyushchikh dlya PKM konstruktsionnogo naznacheniya [Usage of aromatic amine curing agents for epoxy resins binders for production of structural PCM] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2016. №6 (42). St. 04. Available at: http://www.viam-works.ru (accessed: December 14, 2018). DOI: 10.18577/2307-6046-2016-0-6-4-4.