Development of the compounding of rubber extremely high heat resistance with temperature range of exploitation from the -60 to +500°С

Chaykun A.М., Venediktova M.A., Bryk Ya. А.
Chaykun A.М., Venediktova M.A., Bryk Ya. А. Development of the compounding of rubber extremely high heat resistance with temperature range of exploitation from the -60 to +500°С // Proceedings of VIAM. 2019. No. 1. DOI: 10.18577/2307-6046-2019-0-1-21-30. URL: https://viam-works.ru/en/journal/2019/1/3
Keywords
rubber, organic silicon rubber, flame retardants, combustibility, sealing details.
Abstract

In some cases, products of special purpose require application of sealing details on the basis of the elastomer, capable to provide working capacity at high temperatures at least short time. The choice for the specified purposes of rubbers is caused by unique highly elastic properties of the elastomer, allowing providing the hard contact of surfaces at small pressing effort. Besides, in this case process of assembly and forming of seal assembly in products of difficult configuration considerably becomes simpler. Application for these purposes of more heat-resistant metals or fluoroplastic is connected with considerable technological difficulties. The solution of the specified problem is impossible without development of compounding of rubber, ability to provide necessary technical characteristics in the expanded temperature range. Besides, features of creation of compounding and property of the specified rubber in many respects define both approaches to development and choice of optimum options of manufacturing techniques of products from it. The declared approaches will allow not only developing rubber with considerably improved complex of properties, but also in the maximum degree to keep them upon transition to manufacturing of specific products.

Reference list
  1. Kablov E.N. Khimiya v aviatsionnom materialovedenii [Chemistry in Aviation Materials Science] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 3–4.
  2. Kablov E.N. Shestoy tekhnologicheskiy uklad [The sixth technological structure] // Nauka i zhizn. 2010. №4. S. 2–7.
  3. Kablov E.N. Materialy dlya aviakosmicheskoy tekhniki [Materials for aerospace] // Vse materialy. Entsiklopedicheskiy spravochnik. 2007. №5. S.7–27.
  4. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  5. Fedyukin D.L., Makhlis F.A. Tekhnicheskiye i tekhnologicheskiye svoystva rezin [Technical and technological properties of rubber]. M.: Khimiya, 1985. 240 s.
  6. Uplotneniya i uplotnitelnaya tekhnika: spravochnik / pod obsh. red. A.I. Golubeva, L.A. Kondakova [Seals and sealing equipment: a handbook / gen. ed. by A.I. Golubev, L.A. Kondakov]. M.: Mashinostroyeniye, 1986. 464 s.
  7. Naumov I.S., Petrova A.P., Chaykun A.M. Reziny uplotnitelnogo naznacheniya i snizheniye ikh goryuchesti [Rubber sealing destination and reduce their flammability] // Vse materialy. Entsiklopedicheskiy spravochnik. 2013. №5. S. 28–35.
  8. Naumov I.S. Uplotnitelnyye reziny ponizhennoy goryuchesti: dis. … kand. tekhn. nauk [Sealing rubber low flammability: thesis, Cand. Sc. (Tech.)]. M., 2016. 118 s.
  9. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Osobennosti receptur rezin na osnove etilenpropilenovyh kauchukov i ih primenenie v izdeliyah specialnogo naznacheniya (obzor) [Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review)] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  10. Kodolov V.I. Zamedliteli goreniya polimernykh materialov. M.: Khimiya, 1980. 269 s.
  11. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Mikhaylin Yu.A. Konstruktsionnyye polimernyye kompozitsionnyye materialy. 2-e izd. [Structural polymer composites. 2nd ed.]. SPb.: Nauchnyye osnovy i tekhnologii, 2016. 820 s.
  13. Chaikun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti morozostojkih rezin na osnove razlichnyh kauchukov [Features of old-resistant rubbers on the basis on different unvulcanized rubbers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №12. St. 04. Available at: http://www.viam-works.ru (accessed: December 13, 2018).
  14. Goreniye, destruktsiya i stabilizatsiya polimerov / pod red. G.E. Zaikova [Combustion, destruction and stabilization of polymers / ed. by G.E. Zaikov]. SPb.: Nauchnyye osnovy i tekhnologii, 2008. 422 s.
  15. Clough R.L. Aging Effects on Fire-Retardant Additives in Polymers // Journal of Polymer Science: Polymer Chemistry Edition. 1983. Vol. 21. P. 767–780.
  16. Goryuchest i dymoobrazuyushchaya sposobnost polimernykh materialov aviatsionnogo naznacheniya / pod red. R.E. Shalin, B.I. Panshin [lammability and smoke-forming ability of polymeric materials for aviation purposes / ed. By R.E. Shalin, B.I. Panshin]. M.: VIAM, 1986. 104 s.
  17. Barbotko S.L., Shurkova E.N., Volny O.S., Skrylyov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlya vneshnego kontura aviacionnoj tehniki [Evolution of polymer composite fire-safety for the outer contour of aeronautical engineering] // Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
  18. Normy letnoy godnosti samoletov transportnoy kategorii [Airworthiness standards for airplanes of the transport category]: AP-25: utv. Postanovleniyem 28-y sessii Soveta po aviatsii i ispol'zovaniyu vozdushnogo prostranstva 11.12.2008. 3-e izd. M.: Aviaizdat, 2009. 274 s.
  19. GOST R 57924–2017. Kompozity polimernyye. Metod opredeleniya goryuchesti polimernykh materialov dlya aviatsionnoy tekhniki [State Standard R 57924–2017. Polymer composites. Method for determining the flammability of polymeric materials for aircraft]. M.: Standartinform, 2017. 19 s.
  20. Naumov I.S., Chaykun A.M., Eliseyev O.A. Rossiyskiye i mezhdunarodnyye standarty na metody ispytaniy rezin, syrykh rezinovykh smesey i vysokomolekulyarnykh kauchukov [Russian and International Standards for Test Methods for Rubber, Raw Rubber Mixtures and High-Molecular Rubbers] // Vse materialy. Entsiklopedicheskiy spravochnik. 2014. №11. S. 4–13.
  21. Tekhnologiya reziny: retsepturostroyeniye i ispytaniya. Per. s angl. [Rubber technology: formulation and testing. Trans. from Engl.]. SPb.: Nauchnyye osnovy i tekhnologii, 2010. 632 s.
  22. Nurmukhametova A.N., Zenitova L.A. Sposoby polucheniya nanodispersnykh napolniteley [Methods of obtaining nano-dispersed fillers] // Tez. dokl. XII Mezhdunar. konf. molodykh uchenykh, studentov i aspirantov «Sintez, issledovaniye svoystv, modifikatsiya i pererabotka vysokomolekulyarnykh soyedineniy – IV Kirpichnikovskiye chteniya». Kazan, 2008. S. 120.
  23. Bolshoy spravochnik rezinshchika v 2 ch. [Great reference book of rubberman in 2 parts]. M.: Tekhinform, 2012. 1385 s.