Repair of chemical oxide coating on carbon steel
Dyomin S.A., Vinogradov S.S. Repair of chemical oxide coating on carbon steel // Proceedings of VIAM. 2018. No. 9. DOI: 10.18577/2307-6046-2018-0-9-43-50. URL: https://viam-works.ru/en/journal/2018/9/5
Keywords
repair of chemical oxide coating, molibdenum film, local cathode treatment, rubbing, protective ability, carbon steels.
Abstract
Protective properties of the films formed on carbon steel in solutions of sulfur-containing substances, oxidizers and the tannin, and also the cathode processing in molibdenum solution are investigated. Protective ability of molibdenum film is higher than protective ability of the chemical oxide coating received in caustic solution. Possibility of repair of the damaged chemical oxide coating on carbon steel by way local cathode surface treatment of steel by rubbing by marker with molibdenum solution is shown.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Dobromyslov A.N. Diagnostika povrezhdenij zdanij i inzhenernykh sooruzhenij [Diagnosis of damage to buildings and engineering structures]. M.: ASV, 2006. 256 s.
- Kablov E.N. Shestoj tekhnologicheskij uklad [The Sixth Technological Structure] // Nauka i zhizn. 2010. №4. S. 2–7.
- Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
- Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Perspektivnye pokrytiya dlya zashchity ot korrozii uglerodistykh stalej [Perspective coatings for corrosion protection of carbon steels] // Stal. 2016. №6. S. 70–81.
- Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Zashchita ot korrozii uglerodistykh stalej [Protection against corrosion of carbon steel] // Aviacionnye materialy i tehnologii. 2017. №S. S. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
- Galvanicheskie pokrytiya v mashinostroenii: spravochnik v 2 t. / pod red. M.A. Shlugera, L.D. Toka [Galvanic coatings in mechanical engineering: a reference book in 2 vil. / ed. By M.A. Schluger, L.D. Tok]. M.: Mashinostroenie. 1985. T. 2. 1985. S. 57–60.
- Azhogin F.F., Belenkij M.A., Gal I.E. i dr. Galvanotekhnika [Galvanics]. M.: Metallurgiya, 1987. S. 484–485.
- Spravochnoe rukovodstvo po galvanotekhnike / pod red. V.I. Lajnera; per. s nem. N.B. Stsiborovskoj [Reference guide to electroplating / ed. by V.I. Lajner; trans. From Germ. by N.B. Stsiborovskaya]. M.: Metallurgiya. 1972. Ch. III: Neorganicheskie pokrytiya. Okraska metallov. Korroziya. Ispytanie pokrytij. 423 s.
- Sukhotin A.N. Fizicheskaya khimiya passiviruyushchikh plenok na zheleze [Physical chemistry of passivating films on iron]. L.: Khimiya, 1989. 320 s.
- Nikitin M.K., Melnikova E.P. Khimiya v restavratsii [Chemistry in restoration]. L. Khimiya, 1990. 304 s.
- Shemakhanskaya M.S., Lemenovskij D.A., Lakshin B.V., Brusova G.P. Novye metody v restavratsii arkheologicheskogo metalla [New methods in the restoration of archaeological metal] // Vestnik restavratsii muzejnykh tsennostej. 2008. №1 (11). S. 64.
- Lavorko P.K. Oksidirovanie metallov [Oxidation of metals]. Kiev: Mashgiz, 1951. S. 38–41.
- Grilikhes S.YA., Tikhonov K.I. Elektroliticheskie i khimicheskie pokrytiya. Teoriya i praktika [Electrolytic and chemical coatings. Theory and practice]. L.: Khimiya. 1990. S.160–161.
- Salakhova R.K., Ilin V.A., Semenychev V.V., Tyurikov E.V. Izbiratelnoe nanesenie zashchitnykh elektrokhimicheskikh pokrytij [Elective deposition of protective electrochemical coatings] // Galvanotekhnika i obrabotka poverkhnosti. 2008. T. XVI. №4. S. 36–40.