The estimation of ballistic properties of ceramic materials

Grinevich A.V., Lavrov A.V.
Grinevich A.V., Lavrov A.V. The estimation of ballistic properties of ceramic materials // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-95-102. URL: https://viam-works.ru/en/journal/2018/3/11
Keywords
ballistic characteristics, ceramics, shock tests.
Abstract

The article analyzes the criteria for estimating the ballistic durability of ceramic materials. It is shown that the physicomechanical characteristics of ceramics obtained during static tests make it possible to assess the ballistic characteristics of ceramics only at a qualitative level, and therefore it is necessary to develop special test methods that ensure the ceramics work efficiency at high rates of its interaction with the impactor. A technique for direct estimation of the ballistic characteristics of ceramics using a trap with discrete screens is described. The results of a comparative evaluation of the ballistic characteristics of experimental batches of armored ceramics based on aluminum oxide and silicon carbide are presented. A close correspondence of the results of direct ballistic tests and calculations on the basis of the attached mass model is shown.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Sorokin O.Yu., Grashhenkov D.V., Solntsev S.St., Evdokimov S.A. Keramicheskie kompozicionnye materialy s vysokoj okislitelnoj stojkostyu dlya perspektivnyh letatelnyh apparatov (obzor) [Ceramic composite materials with high oxidation resistance for the novel aircrafts (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 08. Available at: http://www.viam-works.ru (accessed: October 16, 2017). DOI: 10.18577/2307-6046-2014-0-6-8-8.
  3. Evteev A.A. Nekotorye aspekty razrabotki optimalnyh rezhimov obzhiga keramicheskih kompozicij, soderzhashhih evtekticheskie dobavki [Some aspects of development of optimal firing conditions for ceramic compositions containing eutectic additives] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №2. St. 12. Available at: http://www.viam-works.ru (accessed: October 16, 2017). DOI: 10.18577/2307-6046-2016-0-2-12-12.
  4. Ivahnenko Yu.A., Varrik N.M., Maksimov V.G. Vysokotemperaturnye radioprozrachnye keramicheskie kompozicionnye materialy dlya obtekatelej antenn i drugih izdelij aviacionnoj tehniki (obzor) [The high-temperature radiolucent ceramic composite materials for the radomes and other products of aviation engineering (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 05. Available at: http://www.viam-works.ru (accessed: October 16, 2017). DOI: 10.18577/2307-6046-2016-0-5-5-5.
  5. Babashov V.G., Ivahnenko Yu.A., Yudin A.V., Zimichev A.M. Keramicheskij material dlya detalej ustanovok nepreryvnoj razlivki cvetnyh splavov [Ceramic material for parts of continuous casting units intended for production of non-ferrous alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 05. Available at: http://www.viam-works.ru (accessed: October 16, 2017). DOI: 10.18577/2307-6046-2014-0-12-5-5.
  6. Markov V.N. Novosibirskaya bronekeramika: prochnost, priznannaya za rubezhom [Novosibirsk ceramic armor: durability recognized abroad] // Oruzhie Rossii: informacionnoe agentstvo [Elektronnyj resurs]. Available at: http://wwww.arms-expo.ru. (accessed: October 16, 2017).
  7. Zajcev G.P. Korundovaya bronekeramika: opyt proizvodstva i primeneniya [Corundum ceramic armor: experience of production and application] // Ekspertnyj soyuz. 2012. №3. Available at: http://unionexpert.ru/index.php/2011-07-25-5-56-33/item/287 (accessed: October 16, 2017).
  8. Rosenberg Z., Dekel E. Terminal Ballistics. Springer-Verlag Berlin Heidelberg, 2012. 306 p.
  9. Zashhita tankov / pod red. V.A. Grigoryana. M.: Izd-vo MGTU im. N.E. Baumana, 2007. 327 s.
  10. Grigoryan V.A. i dr. Chastnye voprosy konechnoj ballistiki [Private questions of final ballistics]. M.: Izd-vo MGTU im. N.E. Baumana, 2006. 586 s.
  11. Grigoryan V.A., Kobylkin I.F., Marinin V.M., Chistyakov E.N. Materialy i zashhitnye struktury dlya lokalnogo i individualnogo bronirovniya [Materials and protective structures for local and individual armoring]. M.: RadioSoft, 2008. 406 s.
  12. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  13. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S., Sevastyanov V.G. Glass and ceramics based high-temperature composite materials for use in aviation technology // Glass and Ceramics. 2012. Vol. 69. No. 3–4. P. 109–112.
  14. Garshin A.P., Gropyanov V.M., Zajcev G.P., Semenov S.S. Keramika dlya mashinostroeniya [Ceramics for mechanical engineering]. M.: Nauchtehlitizdat, 2003. 384 s.
  15. Kremenchugskij M.V., Savkin G.G., Malinov V.I. i dr. Razrabotka protivopulnoj broni s primeneniem keramicheskih materialov [Development of the anti-bullet armor using ceramic materials] // Trudy RFYaC-VNIIEF, №9. 2005. S. 302–309.
  16. Grinevich A.V., Yarosh V.V. Osobennosti razrusheniya keramiki pri udarnom vozdejstvii [Features of destruction of ceramics at shock influence] // Voprosy oboronnoj tehniki. Ser.: 15. 1999. Vyp. 1–2. S. 23–30.
  17. Erasov V.S., Lavrov A.V., Lucenko A.N., Grinevich A.V. K voprosu vzaimodejstviya termouprochnennogo udarnika s keramicheskoj pregradoj [About the question of the interaction of hardened core with ceramic barrier] // Aviacionnye materialy i tehnologii. 2016. №2. S. 69–75. DOI: 10.18577/2071-9140-2016-0-2-69-75.