Monitoring of the deformability of the composite structure of the arch bridge based on fiber-optic sensors

Raskutin A.E., Makhsidov V.V., Smirnov O.I., Kasharina L.A.
Raskutin A.E., Makhsidov V.V., Smirnov O.I., Kasharina L.A. Monitoring of the deformability of the composite structure of the arch bridge based on fiber-optic sensors // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-49-59. URL: https://viam-works.ru/en/journal/2018/3/6
Keywords
monitoring of structures, polymeric composite materials, fiber-optic Bragg grating, loading of arched elements, deformation
Abstract

A description is given of the developed fiber-optic system for monitoring structural loading (arch-bridge elements) operating in real time and warning of approaching the critical level of loading. The criteria for working capacity of the design of the a two-lane automobile arched bridge. The choice of the main criterion was made on the basis of the principle of assessing the structural stability of the structure taking into account the capabilities of the equipment used. It is shown that the relative axial deformation of the arched elements practically did not change over the period of observation.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  3. Doriomedov M.S., Daskovskij M.I., Skripachev S.Yu., Shein E.A. Polimernye kompozicionnye materialy v zheleznodorozhnom transporte Rossii (obzor) [Polymer com-posite materials in the Russian railways (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 12. Available at: http://www.viam-works.ru (accessed: February 27, 2018). DOI: 10.18577/2307-6046-2016-0-7-12-12.
  4. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  5. Dyshenko V.S., Raskutin A.E., Zuev M.A. Dorozhnyj detektor v sistemah bezostanovochnogo avtomaticheskogo vzveshivaniya [The road detector in systems of Weigh-In-Motion] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 12. Available at: http://www.viam-works.ru (accessed: February 27, 2018). DOI: 10.18577/2307-6046-2016-0-5-12-12.
  6. Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitelnyh konstrukcijah [Applying FRP in building structures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 03. Available at: http://viam-works.ru (accessed: February 27, 2018).
  7. Vasilev S.A., Medvedkov I.O., Korolev I.G. i dr. Volokonnye reshetki pokazatelya prelomleniya i ih primenenie [Fiber grids of refraction index and their application] // Kvantovaya elektronika. 2005. T. 35. №12. S. 1085–1103.
  8. Sposob izmereniya deformacii konstrukcii iz kompozicionnogo materiala: pat. 2427795 Ros. Federaciya [Way of measurement of deformation of design from composite material: pat. 2427795 Ros. Federation]; opubl. 03.12.09.
  9. Kablov E.N., Sivakov D.V., Gulyaev I.N. i dr. Primenenie opticheskogo volokna v kachestve datchikov defopmacii v polimepnyh kompozicionnyh materialah [Application of optical fiber as deformation sensors in polymeric composite materials] // Vse materialy. Enciklopedicheskij spravochnik. 2010. №3. S. 10–15.
  10. Kablov E.N., Sivakov D.V., Gulyaev I.N., Sorokin K.V., Fedotov M.Yu., Goncharov V.A. Metody issledovaniya konstrukcionnyh kompozicionnyh materialov s integrirovannoj el-ektromehanicheskoj sistemoj [Methods of research of constructional composite materials with the integrated electromechanical system] //Aviacionnye materialy i tehnologii. 2010. №4. S. 17–20.
  11. Shhetanov B.V., Kuptsov R.S., Svistunov V.I. Metody polucheniya monokristallicheskih volokon oksida alyuminiya dlya sozdaniya kompozicionnyh materialov i vysokotemperaturnoj volokonnoj optiki [Methods of receiving single-crystal fibers of aluminum oxide for creation of composite materials and high-temperature fiber optics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 01. Available at: http://www.viam-works.ru (accessed: February 27, 2018).
  12. Nikitina V.J., Kolyshev S.G., Kuptsov R.S. Sposoby opredeleniya ploshhadi secheniya monokristallicheskih volokon Al2O3 dlya rascheta prochnosti pri rastyazhenii [The methods of determination of Al2O3 single-crystal fibers cross-section area for tensile strength calculation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 03. Available at: http://www.viam-works.ru (accessed: February 27, 2018). DOI: 10.18577/2307-6046-2014-0-2-3-3.
  13. Huang Y., Palek L., Strommen R. et al. Real-Time Weigh-In-Motion Measurement Using Fiber Bragg Grating Sensors // Sensors and Smart Structures Technologies for Civil, Mechanical and Aerospace Systems. 2014. Vol. 9061. P. 96–102.
  14. Zhou Z., Liua W., Huang Y. et al. Optical Fiber Bragg Grating Sensor Assembly for 3D Strain Monitoring and Its Case Study in Highway Pavement // Mechanical Systems and Signal Pro-cessing. 2012. Vol. 28. P. 36–49.
  15. Wang K., Wei Z., Zhang H. et al. Fiber-Bragg-grating-based weigh-in-motion system using fiber-reinforced composites as the load-supporting material // Optical Engineering. 2006. Vol. 45. No. 6. P. 33–39.
  16. Zhan H., Wei Z., Fan L. et al. Sensing System and a High Performance Optical Fiber Bragg Grating (FBG) Demodulator // Sensors and Smart Structures Technologies for Civil, Mechanical and Aerospace Systems. 2010. Vol. 7647. P. 102–109.