Formation of new surfaces in a firm body at stages of elastic and plastic deformations, the beginning and destruction development

Erasov V.S., Oreshko E.I., Lutsenko A.N.
Erasov V.S., Oreshko E.I., Lutsenko A.N. Formation of new surfaces in a firm body at stages of elastic and plastic deformations, the beginning and destruction development // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-12-12. URL: https://viam-works.ru/en/journal/2018/2/12
Keywords
potential energy, surface of a firm body, elastic deformation, plastic deformation, deformation model, destruction model, cylindrical isotropic sample.
Abstract

Models of formation of new surfaces in a firm body at stages of elastic and plastic deformations, the beginning and development of fragile destruction, destruction with existence of plastic deformation are presented. The assessment of the power expenses necessary for formation of unit of a new surface, and as influences on these expenses of plastic deformation is carried out. The method of determination of superficial energy of a material for fragile bodies is presented.

Reference list
  1. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. № 2 (14). S. 16–21.
  2. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Erasov V.S., Oreshko E.I. Deformaciya i razrushenie kak processy izmeneniya obema, ploshhadi poverhnosti i linejnyh razmerov v nagruzhaemyh telah [Deformation and destruction as processes of change of volume, the areas of a surface and the linear sizes in loaded bodies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8. St. 11. Available at: http://www.viam-works.ru (accessed: January 25, 2018). DOI: 10.18577/2307-6046-2016-0-8-11-11.
  5. Erasov V.S., Oreshko E.I., Lucenko A.N. Ploshhad svobodnoj poverhnosti kak kriterij hrupkogo razrusheniya [Area of a free surface as criterion of brittle fracture] // Aviacionnye materialy i tehnologii. 2017. № 2 (47). S. 69–79. DOI: 10.18577/2071-9140-2017-0-2-69-79.
  6. Shibkov A.A., Zolotov A.E., Zheltov M.A., Shuklinov A.V., Denisov A.A. Dinamika deformacionnyh polos i razrushenie alyuminij-magnievogo splava AMg6 // Fizika tverdogo tela. 2011. T. 53. №10. S. 1873–1878.
  7. Shibkov A.A., Zolotov A.E., Zheltov M.A., Denisov A.A. Deformacionnyj haos i samoorganizaciya na stadii predrazrusheniya splava AMg6 [Deformation chaos and self-organization at stage of predestruction of alloy AMg 6] // Fizika tverdogo tela. 2011. T. 53. №10. S. 1879–1884.
  8. Erasov V.S., Oreshko E.I. Silovoj, deformacionnyj i energeticheskij kriterii razrusheniya [Force, deformation and energy criteria of destruction] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10 (58). St. 11. Available at: http://viam-works.ru (accessed: January 25, 2018). DOI: 10.18577/2307-6046-2017-0-10-11-11.
  9. GOST 25.506–85. Raschety i ispytaniya na prochnost. Metody mehanicheskih ispytanij metallov. Opredelenie harakteristik treshhinostojkosti (vyazkosti razrusheniya) pri staticheskom nagruzhenii [State Standart 25.506-85. Calculations and strength tests. Methods of mechanical tests of metals. Definition of characteristics crack resistance (fracture toughness) at static loading]. M.: Izd-vo standartov, 1985. 61 s.
  10. Zhu X.-K., Joyce, J.A. Review of fracture toughness (G, K, J, CTOD, CTOA) testing and stan-dardization // U.S. Navy Research. 2012. Paper 49.
  11. Shtremel M.A. Razrushenie [Destruction]. M.: MISiS, 2014. Kn.1: Razrushenie materiala. S. 66–113.
  12. OST1 90356–84. Metally. Metod opredelenie staticheskoj treshhinostojkosti (vyazkosti razrusheniya) obshivochnyh materialov pri ploskom napryazhennom sostoyanii [Industry Standard 90356–84. Metals. Method of definition of static treshchinostoykost (fracture toughness) of sheathing materials at flat tension]. M., 1984. 31 s.
  13. OST1 92122–88. Metally. Metod opredelenie krivoj soprotivleniya rasprostraneniyu treshhiny pri staticheskom nagruzhenii (R-krivoj) obshivochnyh materialov pri ploskom napryazhennom sostoyanii [Industry Standard 1 92122-88. Metals. Method of definition of curve of resistance to crack distribution at static loading (R-curve) of sheathing materials at flat tension]. M., 1988. 32 s.
  14. ASTM E 561-10. Standard Test Method for K-R Curve Determination. American Society for Testing and Materials, 2010.
  15. Terentev V.F. Ustalost metallicheskih materialov [Fatigue of metal materials]. M.: Nauka, 2003. S. 37–44.
  16. Vildeman V.E., Tretyakov V.P. Ispytaniya materialov s postroeniem polnyh diagramm deformirovaniya [Tests of materials with creation of full charts of deformation] // Problemy mashinostroeniya i nadezhnosti mashin. 2013. №2. S. 93–98.
  17. Mahutov N.A., Moskvitin G.V. Vliyanie uslovij nagruzheniya na nakoplenie povrezhdenij i razrushenie [Influence of conditions of loading on accumulation of damages and destruction] // Mashinostroenie: enciklopediya. M.: Mashinostroenie, 2010. T. II-I: Fiziko-mehanicheskie svojstva. Ispytaniya metallicheskih materialov. S. 220–221.
  18. Shanyavskij A.A. Sinergetika evolyucii metallov ot chastichno zamknutoj k otkrytoj dinamicheskoj sisteme pri ciklicheskom nagruzhenii [Synergetrics of evolution of metals from partially closed to open dynamic system at cyclic loading] // Dinamika slozhnyh sistem. 2007. T. 1. №1. S. 90–104.
  19. Terentev V.F., Korableva S.A. Ustalost metallov [Fatigue of metals]. M.: Nauka, 2015. S. 73–77.