Thermodynamics analysis of magnetoplastic effects in «non-magnetic» metals

Morgunov R.B., Piskorsky V.P., Valeev R.A., Korolev D.V.
Morgunov R.B., Piskorsky V.P., Valeev R.A., Korolev D.V. Thermodynamics analysis of magnetoplastic effects in «non-magnetic» metals // Proceedings of VIAM. 2018. No. 12. DOI: 10.18577/2307-6046-2018-0-12-79-87. URL: https://viam-works.ru/en/journal/2018/12/9
Keywords
magnetoplasticity, thermodynamic analysis, yield strength, hardness, magnetic field, mechanical properties.
Abstract

Many works were devoted to the influence of the magnetic field of 0.05 - 30 T induction and the duration of exposure in the magnetic field from 1 µs to several days on the mechanical properties of polymers, ion crystals, semiconductors, transition metals, fullerites, technological alloys. A brief analysis of the results in the study of magnetoplastic effects (the phenomena of changes in the plasticity and strength of metals under the action of a magnetic field) was done. 

The classification of known and physically justified effects on the basis of thermodynamic analysis of the energy is reported for the systems and the relaxation time of changes induced by the field. Controversial experimental results and their interpretations are discussed. Unified physical mechanisms controlling magnetoplasticity stimulated discussion of magnetoplastic effects simultaneously in nonmetallic solids, where the magnetic field also change structurally sensitive properties.

Most of the magnetoplastic effects, regardless of the type of material, obey a simple rule: transition time decreases with the growth of the magnetic field and the energy transmitted to the crystal lattice. Magnetoplastic effects which, obey this law can be called as "power" effects, i.e. those, which has a value of the magnetic force on the structural elements of the crystal or defects. Another part is characterized by more exotic mechanisms of influence of the field, not limited by the transfer of energy necessary for overcoming potential barriers. It is shown, that the effect of the magnetic field on the subsystem of structural defects is irreversible in many cases, while there are completely irreversible magneto plastic effects. In this case, the system does not return to its original free energy state even if its plastic properties seem to be restored.

<p st

Reference list
  1. Glavatskyy I., Glavatska N., Dobrinsky A. et al. Crystal structure and high-temperature magnetoplasticity in the new Ni–Mn–Ga–Cu magnetic shape memory alloys // Scripta Materialia. 2007. Vol. 56. Is. 7. P. 565–568.
  2. Kostorz G., Müllner P. Basic – magnetoplasticity // Zeitschrift für Metallkunde. 2005.
  3. Vol. 96. Is. 7. Р. 703–709.
  4. Alshits V.I., Darinskaya E.V., Koldaeva M.V., Petrzhik E.A. Resonance magnetoplasticity in ultralow magnetic fields // Dislocations in solids. Amsterdam: Elsevier, 2008. Vol. 14. Ch. 86. P. 333.
  5. Alshits V.I., Darinskaya E.V., Koldayeva M.V., Petrzhik E.A. Magnitoplasticheskiy effekt: osnovnye svoystva i fizicheskie mekhanizmy [Magnetoplastic effect: basic properties and physical mechanisms] // Kristallografiya. 2003. T. 48. №5. S. 826–854.
  6. Golovin Yu.I. Magnitoplastichnost tverdykh tel (obzor) [Magnetoplasticity of solids (review)] // Fizika tverdogo tela. 2004. T. 46. Vyp. 5. S. 769–863.
  7. Morgunov R.B. Spinovaya mikromekhanika v fizike plastichnosti [Spin micromechanics in plasticity physics] // Uspekhi fizicheskikh nauk. 2004. № 2. S. 131–153.
  8. Buchachenko A.L. MASS-Independent Isotope Effects // Journal of Physical Chemistry. B. 2013. Vol. 117. No. 8. P. 2231–2238.
  9. Beaugnon E. Physical modeling of anisotropic grain growth at high temperature in local strong magnetic force field // Science Technology of Advanced Materials. 2008. Vol. 9. P. 356–401.
  10. Molodov D.A., Bollmann C., Gottstein G. Impact of a magnetic field on the annealing be-havior of cold rolled titanium // Materials Science and Engineering A. 2007. Vol. 467. P. 71–80.
  11. Yonenaga I., Takahashi K. Effect of magnetic field on dislocation-oxygen impurity in-teraction in silicon // Journal of Applied Physics. 2007. Vol. 101. P. 568–576.
  12. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the pe-riod until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Kablov E.N., Morozov G.A., Krutikov V.N., Muravskaya N.P. Attestaciya standartnyh obrazcov sostava slozhnolegirovannyh splavov s primeneniem etalona [Certification of standard samples of structure of complex-alloyed alloys using standard] // Aviacionnye materialy i tehnologii. 2012. №2. S. 9–11.
  14. Kablov E.N., Ospennikova O.G., Piskorskij V.P., Rezchikova I.I., Valeev R.A., Davydova E.A. Fazovyj sostav spechennyh materialov sistemy Pr–Dy–Fe–Co–B [Phase composition of the Pr–Dy–Fe–Co–B sintered materials] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 5–10. DOI: 10.18577/2071-9140-2015-0-S2-5-10.
  15. Kablov E.N., Ospennikova O.G., Cherednichenko I.V., Rezchikova I.I., Valeev R.A., Piskorskij V.P. Vliyanie soderzhaniya medi na fazovyj sostav i magnitnye svojstva termosta-bil'nyh spechennyh magnitov sistem Nd–Dy–Fe–Co–B i Pr–Dy–Fe–Co–B [Influence of Cu content to phase structure and magnetic properties of thermostable sintered magnets of Nd–Dy–Fe–Co–B and Pr–Dy–Fe–Co–B systems] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 11–19. DOI: 10.18577/2071-9140-2015-0-S2-11-19.
  16. Kablov E.N., Ospennikova O.G., Rezchikova I.I., Piskorskij V.P., Valeev R.A., Korolev D.V. Zavisimost svojstv spechennyh materialov sistemy Nd–Dy–Fe–Co–B ot tehnologicheskih parametrov [Properties dependence of the Nd–Dy–Fe–Co–B sintered materials on technological parameters] // Aviacionnye materialy i tehnologii. 2015. №S2 (39). S. 24–29. DOI: 10.18577/2071-9140-2015-0-S2-24-29.