Niobium silicide synthesis by spark plasma sintering of composite powders

Efimochkin I.Yu., Kuzmina N.A., Grachshencov D.V., Svetlov I.L., Bobrovkiy A.P.
Efimochkin I.Yu., Kuzmina N.A., Grachshencov D.V., Svetlov I.L., Bobrovkiy A.P. Niobium silicide synthesis by spark plasma sintering of composite powders // Proceedings of VIAM. 2018. No. 11. DOI: 10.18577/2307-6046-2018-0-11-54-63. URL: https://viam-works.ru/en/journal/2018/11/7
Keywords
high-temperature materials, composite materials, Nb–Si system, niobium silicide, mechanical alloying, synthesis, spark plasma sintering, structure.
Abstract

The possibility of niobium silicide synthesis by the spark plasma technique from a binary mixture of mechanical alloyed elemental powders is considered. The X-ray phase analysis of the synthesized samples of niobium silicide was carried out, their microstructure were investigated by the methods of scanning electron microscopy, and X-ray microscopic analysis were used to evaluate the elemental composition. The performed X-ray phase analysis of the synthesized samples demonstrated the preparation of stable tetragonal α-Nb5Si3 and hexagonal γ-Nb5Si3, stabilized by intercalation of carbon atoms. The stability of obtained samples of niobium silicide under 1500°Cfor 10 h was investigated.

Reference list
  1. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsional'noy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  4. Kuzmina N.A., Bondarenko Yu.A. Issledovanie fazovogo sostava i struktury niobij-kremnievogo kompozita, poluchennogo metodom napravlennoj kristallizacii v zhidkome-tallicheskom ohladitele [The phase composition and structure of the niobium-silicon composite manufactured by directional solidification in the liquid metal cooler] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 03. Available at: http://www.viam-works.ru (accessed: November 20, 2018). DOI: 10.18577/2307-6046-2016-0-5-3-3.
  5. Svetlov I.L. Vysokotemperaturnyye Nb–Si kompozity [High-Temperature Nb–Si Composites] // Materialovedeniye. 2010. №9–10. S. 18–38.
  6. Kablov E.N., Svetlov I.L., Yefimochkin I.Yu. Vysokotemperaturnyye Nb–Si-kompozity [High-Temperature Nb–Si Composites] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashi-nostroyeniye. 2011. №SP2. S. 164–173.
  7. Shchetanov B.V., Efimochkin I.Yu., Paegle S.V., Karachevtsev F.N. Issledovanie vysokotemperaturnoj prochnosti in-situ-kompozitov na osnove Nb, armirovannyh monokristallicheskimi voloknami α-Al2O3 [Study of high-temperature strength of Nb–Si–Ti in-situ-composites reinforced by single-crystal α-Al2O3] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 53–59. DOI: 10.18577/2071-9140-2016-0-3-53-59.
  8. Chang K.M., Bewley B.P., Sattley J.A., Jackson M.R. Cold-Crusible Directional Solidification of Refractory Metal-Silicide Eutectics // Journal of Metals. 1992. Vol. 44. No. 6. P. 59.
  9. Subramanian P.R., Mendiratta M.G., Dimiduk D.M. Development of Nb-based Advanced Intermetallic Alloys for Structural Application (Overview) // Journal of Metals. 1996. Vol. 48. No. 1. P. 33–38.
  10. Jackson M.R., Bewley B.P., Rowe R.G., Skelly D.W. Lipsitt High Temperature Refractory Metall-Intermetallic Composites // Journal of Metals. 1996. Vol. 48. No. 1. P. 39–44.
  11. Bewley B.P., Levandovsky J.J., Jackson M.R. Refractory Metall-Intermetallic in Situ Composites for Aircraft Engine (Overview) // Journal of Metals. 1997. Vol. 49. No. 8. P. 44–67.
  12. Bewley V.P., Jackson M.R., Subramanian P.R. Processing High Temperature Refractory Metall-Silicide in Situ Composites (Overview) // Journal of Metals. 1999. Vol. 51. No. 4. P. 32–36.
  13. Bewley B.P., Jackson M.R., Zhao J.C., Subramanian P.R. A Review of Very-High-Temperature Nb-Silicide-based Composites // Metallurgical and Materials Transactions. 2003. Vol. 34A. No. 10. P. 2043–2052.
  14. Grashchenkov D.V., Shchetanov B.V., Efimochkin I.Yu. Razvitiye poroshkovoy metallurgii zharoprochnykh splavov [Development of powder metallurgy of superalloys] // Vse materialy. Entsiklopedicheskiy spravochnik. 2011. №5. S. 13–26.
  15. Svetlov I.L., Kuzmina N.A., Zavodov A.V., Zaytsev D.V. Termicheskaya stabil'nost' poverkhnostey razdela mezhdu niobiyevoy matritsey i γ -Nb5Si3 silitsidom v kompozite na osnove sistemy Nb–Si [Thermal stability of interfaces between the niobium matrix and γ-Nb5Si3 silicide in eutectic Nb–Si composites] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №8 (68). S. 28–37. URL: http://www.viam-works.ru (accessed: November 20, 2018). DOI: 10.18577/2307-6046-2018-0-8-28-37.
  16. Svetlov I.L., Abuzin Yu.A., Vlasenko S.Ya., Efimochkin I.Yu. i dr. Vysokotemperaturnyye niobiyevyye kompozity, uprochnennyye silitsidami niobiya [High-Temperature Niobium Composites Strengthened with Niobium Silicides] // Zhurnal funktsional'nykh materialov. 2007. T. 1. №2. S. 48–53.
  17. Grashchenkov D.V., Shchetanov B.V., Efimochkin I.Yu., Sevostyanov N.V. Kompozitsionnyye materialy na osnove tugoplavkikh metallov [Composite materials based on refractory metals] // Konstruktsii iz kompozitsionnykh materialov 2016. №4. S. 16–23.
  18. Kuz'mina N.A., Marchenko Ye.I., Yeremin N.N., Yakushev D.A. Issledovaniye defektov vnedreniya v polimorfnykh modifikatsiyakh silitsidov niobiya Nb5Si3 metodami atomi-sticheskogo komp'yuternogo modelirovaniya [The study of defects intro-duction in polymorphic modifications of niobium silicide Nb5Si3 by the methods of atomistic computer simulation] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №1 (61). Ct. 02. URL: http://www.viam-works.ru (accessed: November 20, 2018). DOI: 10.18577/2307-6046-2018-0-1-2-2.
  19. Timofeyeva O.B., Kolodochkina V.G., Shvanova N.F., Neiman A.V. Issledovanie mikrostruktury vysokotemperaturnogo estestvenno kompozicionnogo materiala na osnove niobija, uprochnennogo intermetallidami silicida niobiya [The microstructure analysis of niobium-based high-temperature natural composite material reinforced with niobium silicide intermetallics] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 60–64. DOI: 10.18577/2071-9140-2015-0-1-60-64.
  20. Savitskiy E.M., Efimov Yu.V., Bodak O.I., Kharchenko O.I., Myasnikova E.A. Sistema niobiy–kremniy–uglerod [System niobium–silicon–carbon] // Neorganicheskiye materialy. 1981. T. 17. №12. S. 2207–2210.
  21. Kuzmina N.A., Eremin N.N., Marchenko E.I., Svetlov I.L. i dr. Puti diffuzii primesey vnedreniya v silitside niobiya Nb5Si3 razlichnykh polimorfnykh modifikatsiy [Ways of dif-fusion of impurities of intrusion in Nb5Si3 niobium silicide of various polymorphic modifications] // Kristallografiya. 2017. №4. S. 21–35.
  22. Kablov E.N., Kuzmina N.A., Eremin N.N., Svetlov I.L., Neyman A.V. Atomnyye modeli struktury silitsidov niobiya v in situ kompozitakh Nb–Si [Atomic models of the structure of niobium silicides in in situ Nb–Si composites] // Zhurnal strukturnoy khimii. 2017. №3. S. 27–37.