Modern methods of mechanical processing of composite materials (review)

Pripisnov Ya.A., Grishina O.I.
Pripisnov Ya.A., Grishina O.I. Modern methods of mechanical processing of composite materials (review) // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-53-61. URL: https://viam-works.ru/en/journal/2018/10/7
Keywords
blade machining, ultrasonic processing, laser processing, waterjet cutting, reinforcing fibers, metallic composite material.
Abstract

A review of the main machining methods currently used for composite materials is given, their machinability is considered, the advantages and disadvantages of various processing methods are indicated. The analysis of blade machining, including features of wear and various options for coating the cutting tool. Two methods of ultrasonic processing are also described, the possibilities of laser processing are displayed, and the essence of water-jet cutting of materials is explained. In conclusion, the conclusion is made about the prospects of mechanical processing of composite materials.

Reference list
  1. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  2. Kablov E.N. Osnovnyye itogi i napravleniya razvitiya materialov dlya perspektivnoy aviatsionnoy tekhniki [The main results and directions of development of materials for advanced aviation equipment] // 75 let. Aviacionnye materialy. M.: VIAM, 2007. S. 20–26.
  3. Kablov E.N. Materialy novogo pokoleniya [New generation materials] // Zashchita i bezopasnost. 2014. №4. S. 28–29.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Ospennikova O.G. Itogi realizacii strategicheskih napravlenij po sozdaniyu novogo pokoleniya zharoprochnyh litejnyh i deformiruemyh splavov i stalej za 2012–2016 gg. [Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016] // Aviacionnye materialy i tehnologii. 2017. №S. S. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  6. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  7. Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  8. Chandramohan D., Murali B. Machining of composites – a review // Academic Journal of Manufacturing Engineering. Available at: http://www.auif.utcluj.ro/images/VOLUME12_3/10_Chandramohan_Murali_67_71 (accessed: September 09, 2018).
  9. Kartashov A.B. Mekhanicheskaya obrabotka kompozitov [Mechanical processing of composites]. Available at: www.bmstu.ru/ps/~kartashov/fileman/download/PKM2017/PKM_VKM_11.pdf (accessed: September 09, 2018).
  10. Raskutin A.E., Khrulkov A.V., Girsh R.I. Tekhnologicheskie osobennosti mekhanoobrabotki kompozitsionnykh materialov pri izgotovlenii detaley konstruktsiy (obzor) [Technological features of machining of composite materials when manufacturing details of designs (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 12. Available at: http://www.viam-works.ru (accessed: September 09, 2018). DOI: 10.18577/2307-6046-2016-0-9-12-12.
  11. Meshkas A.E., Makarov V.F., Shirinkin V.V. Tekhnologii, pozvolyayushchiye povysit effektivnost obrabotki kompozitsionnykh materialov metodom frezerovaniya [Technologies allowing to increase the processing efficiency of composite materials by milling method] // Izvestiya TulGU. Ser.: Tekhnicheskiye nauki. 2016. Vyp. 8. Ch. 2. S. 292.
  12. Yushchenko D.A., Lobanov D.V. Metody lezviynoy obrabotki izdeliy iz kompozitsionnykh materialov ikh spetsifika i perspektivy [Methods of blade processing of products from composite materials, their specificity and prospects] // Tekhnologii i materialy. 2015. №3. S. 30–35.
  13. Ravi Sekhar T.P. Singh Mechanisms in turning of metal matrix composites: a review // Journal of Materials Research and Technology. 2015. No. 4 (2). P. 197–207. Available at: http://www.jmrt.com.br (accessed: September 09, 2018). DOI: 10.1016/j.jmrt.2014.10.013.
  14. El-Gallab M., Sklad M. Machining of Al/SiC particulate metal-matrix composites: Part I: Tool performance // Journal of Materials Processing Technology. 1998. No. 83. P. 151–158. Available at: https://www.sciencedirect.com/science/article/pii/S0924013698000545 (September 09, 2018). DOI: 10.1016/S0924-0136(98)00054-5.
  15. Hooper R.M., Henshall J.L., Klopfer A. The wear of polycrystalline diamond tools used in the cutting of metal matrix composites // International Journal of Refractory Metals and Hard Materials. Available at: https://www.sciencedirect.com/science/article/pii/S0263436898000407 (September 09, 2018). DOI: 10.1016/S0263-4368(98)00040-7.
  16. Weinert K., Biermann D. Turning of fiber and particle reinforced aluminium // Proceedings of the International Conference on Machining Of Advanced Materials. 1993. P. 437–453.
  17. Morgunov Yu.A., Opalnitskiy A.I., Perepechkin A.A. Sovremennoye sostoyaniye i perspektivy primeneniya v mashinostroyenii ultrazvukovoy razmernoy obrabotki izdeliy [The current state and prospects for application in mechanical engineering of ultrasonic dimensional processing of products] // Izvestiya MGTU «MAMI». 2012. №2 (14). T. 2. S. 140–144.
  18. Yan Chen, Yuhong Liang, Jiuhua Xu, Andong Hu. Ultrasonic vibration assisted grinding of CFRP composites: Effect of fiber orientation and vibration velocity on grinding forces and surface quality // International Journal of Lightweight Materials and Manufacture. September. 2018. P. 189–196. Available at: https://www.sciencedirect.com/science/article/pii/S2588840418300386 (September 09, 2018). DOI: 10.1016/j.ijlmm.2018.08.003.
  19. Vashukov Yu.A. Tekhnologiya raketnykh i aerokosmicheskikh konstruktsiy iz kompozitnykh materialov [Technology of rocket and aerospace structures made of composite materials] // Multimediynyy obrazovatelnyy modul. Samara: Izd-vo SGAU, 2012. S. 101. Available at: https://www.twirpx.com/file/1771851/ (September 09, 2018).
  20. Astapchik S.A., Golubev V.S., Maslakov A.G. Lazernyye tekhnologii v mashinostroyenii i metalloobrabotke [Laser technology in mechanical engineering and metalworking]. Minsk: Belorusskaya nauka. 2008. C. 232–242.
  21. Xie J. Dual beam laser welding // Welding Journal. 2002. Vol. 81. No. 10. P. 223–230
  22. Bayeva L.S., Marinin A.A. Sovremennyye tekhnologii additivnogo izgotovleniya obyektov [Modern technologies of additive manufacturing of objects] // Vestnik Murmanskogo gosudarstvennogo tekhnicheskogo universiteta. 2014. T. 17. №1. S. 7–12.
  23. Shanmugam D.K., Chen F.L., Siores E., Brandt M. Comparative study of jetting machining technologies over laser machining technology for cutting composite materials // Composite Structures. 2012. No. 57. P. 289–296. URL: https://www.sciencedirect.com/science/article/pii/S026382230200096X (accessed: September 10, 2018). DOI: 10.1016/S0263-8223(02)00096-X.
  24. Grishchenko T.A., Melyukhov N.I., Lyubushkin V.O. Primeneniye gidroabrazivnoy rezki pri obrabotke detaley iz polimernykh kompozitsionnykh materialov [The use of waterjet cutting in the processing of parts from polymer composite materials] // Vestnik inzhenernoy shkoly DVFU. 2017. №2 (31). S. 49–55. URL: https://www.dvfu.ru/vestnikis/archive-editions/2-31/6/ (accessed: September 10, 2018). DOI: 10.5281/zenodo.808901.