Comparative researches of phase composition influence on mechanical and technological properties of MA20-SP and MA2-1 magnesium alloys

Volkova E.F., Mostyaev I.V., Akinina M.V.
Volkova E.F., Mostyaev I.V., Akinina M.V. Comparative researches of phase composition influence on mechanical and technological properties of MA20-SP and MA2-1 magnesium alloys // Proceedings of VIAM. 2018. No. 1. DOI: 10.18577/2307-6046-2018-0-1-5-5. URL: https://viam-works.ru/en/journal/2018/1/5
Keywords
magnesium alloys, phase composition, high dispersed hardening phases, microstructure, rare earth metals (REM), bending, deep drawing, mechanical and technological properties.
Abstract

The paper presents the comparative investigation results of phase composition influence of new economically alloying MA20-SP alloy and commercial MA2-1 alloy on their based properties under room and elevated temperatures. It was found out the parameters of bending and deep drawing of sheets. It was showed, that alloying MA20-SP alloy by zirconium and cerium (0,25–0,30 mass %) promotes the forming of high dispersed hardening precipitates of phases, the emergence of uniaxial and refine structure and helps to achieve the higher level of mechanical and technological properties in comparison with MA2-1 alloy.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  3. Volkova E.F., Akinina M.V., Mostyaev I.V. Puti povysheniya osnovnyh mehanicheskih harakteristik magnievyh deformiruemyh splavov [The ways of rising of wrought magnesium alloys main mechanical characteristics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №10 (58). St. 02. Available at: http://www.viam-works.ru (accessed: November 20, 2017). DOI: 10.18577/2307-6046-2017-0-10-2-2.
  4. Volkova E.F., Duyunova V.A. O sovremennyh tendenciyah razvitiya magnievyh splavov [About current trends of development of magnesium alloys] // Tehnologiya legkih splavov. 2016. №3. S. 94–105.
  5. Kablov E.N., Volkova E.F., Filonova E.V. Issledovanie vliyaniya RZE na fazovyj sostav i svojstva novogo zharoprochnogo magnievogo splava sistemy Mg–Zn–Zr–RZE [Research of influence of REE on phase structure and properties of new heat resisting magnesium alloy of Mg-Zn-Zr-REE system] // MiTOM. 2017. №7. S. 19–26.
  6. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  7. Dobatkin S.V., Rohlin L.L., Dobatkina T.I. Issledovanie magnievyh splavov sistemy
  8. Mg–Sm–Y, podvergnutyh intensivnoj plasticheskoj deformacii i posleduyushhej termicheskoj obrabotke [Research of magnesium alloys of system Mg–Sm–Y subjected to intensive plastic strain and the subsequent thermal processing] // Metally. 2011. №4. S. 32–37.
  9. Furro R., Saccone A., Delfino S. Magnesium alloys of the rare earth metals systematics and properties // Metallurgical Science and Technology. 1998. Vol. 16 (1–2). P. 25–44.
  10. Kainer K.U. Magnesium alloys for structural application // Miner. Metals and Mater. Soc., 2000. Vol. 52. No. 11. P. 198–199.
  11. Sankaranarayanan Seetharaman, Zi Hao Lennon Loy, Sravya Tekumalla et al. Development and characterization of new Magnesium–Yttrium–Calcium alloys // Proceedings of the 10th International Conference on Magnesium Alloys and Their Applications (Mg–2015). 2015. P. 31–37.
  12. Luyao Jiang, Dingfei Zhang, Xiaowei Fan. et al. Influence of 0-2 wt.% Sn addition on the microstructure and mechanical properties of extruded AZ80 alloy // Proceedings of the 10th International Conference on Magnesium Alloys and Their Applications (Mg–2015). P. 128–136.
  13. Shao X.H., Yang Z.Q., Ma X.L. Strengthening and toughening mechanisim in Mg–Zn–Y alloy with a long period stacking ordered structure // Acta Mater. 2010. Vol. 58. No. 14. P. 4760–4771.
  14. Watanabe H., Mukai T., Higashi K. Grain refinement in superplasticity in magnesium alloys // Ultrafine Grained Materials II.TMS, Warrendale, PA, 2002. P. 469–476.
  15. Sharon J.A., Zhang Y., Mompiou F., Legros M., Hemker K.J. Discerning size effect strengthening in ultrafine grained Mg thin films // Scripta Mater. 2014. Vol. 75. P. 10–13.
  16. Lashko N.F., Zaslavskaya L.V., Kozlova M.N. i dr. Fiziko-himicheskij fazovyj analiz stalej i splavov [Physical and chemical phase analysis staly and alloys]. M.: Metallurgiya, 1978. 336 s.
  17. Emli E.F. Osnovy tehnologii proizvodstva i obrabotki magnievyh splavov [Bases of the production technology and processing of magnesium alloys]. M.: Metallurgiya, 1972. S. 203–204.
  18. Magnievye splavy: spravochnik / pod red. M.B. Altmana, M.E. Drica, M.A. Timonova i dr. [Magnesium alloys: the directory / ed. by M.B. Altman, M.E.Drits, Timonov and dr.]. M.: Metallurgiya, 1978. T. I. S. 116–118.