The influence of the mechanical alloying parameters on the particles morphology of the metalceramiс powder composition made from VZH175 alloy with TiCN nanopowder

Buyakina A.A., Letnikov M.N., Efimochkin I.Yu.
Buyakina A.A., Letnikov M.N., Efimochkin I.Yu. The influence of the mechanical alloying parameters on the particles morphology of the metalceramiс powder composition made from VZH175 alloy with TiCN nanopowder // Proceedings of VIAM. 2017. No. 9. DOI: 10.18577/2307-6046-2017-0-9-4-4. URL: https://viam-works.ru/en/journal/2017/9/4
Keywords
powder metallurgy, mechanical alloying, titanium carbonitride, nanoparticles, Ni-base superalloy.
Abstract

The influence of the main parameters of the mechanical alloying in the planetary ball mill on flowability and morphology of the metalceramiс made from Ni-based superalloy VGH175 and nanoparticles of titanium carbonitride are investigated. As the basis of metalceramiс composition have been used powder of VGH175 superalloy with particle size less than 63 μm produced by gas atomization; аs the reinforcing filler have been used nanoparticles of titanium carbonitride produced by the plasma-chemical synthesis method. The effect of the rotation speed of grinding jars and time process on flowability of compositions and morphology of the particles (average diameter and powder-size distribution) are presented. The optimal parameters for producing metalceramiс powders with the uniform distribution of the nanoparticles on the matrix granules surface with keepping their original spherical form are determined.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the develop-ment of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and VIAM technologies for «Aircraft engine»] // Permskie aviatsionnye dvigateli: inform. byull. 2014. №31. S. 43–47.
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennykh zharoprochnykh materialov i tekhnologii ikh proizvodstva dlia aviatsionnogo dvigatelestroeniia [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  4. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  5. Cao G., Van I. Nanostruktury i nanomaterialy: sintez, svojstva i primenenie [Nanostructures and nanomaterials: synthesis, properties and application]. M.: Nauchnyj mir, 2012. 515 s.
  6. Bykov Ju., Karpuhin S. Konstrukcionnye nanomaterialy, struktura, svojstva, sposoby poluchenija [Constructional nanomaterials, structure, properties, ways of receiving]. Saarbrjukken: LAP LAMBERT Academic Publishing, 2012. 84 s.
  7. Azarenkov N.A., Beresnev V.M., Pogrebnjak A.D., Kolesnikov D.A. Nanostrukturnye pokrytija i nanomaterialy: Osnovy poluchenija. Svojstva. Oblasti primenenija. Osobennosti sovremennogo nanostrukturnogo napravlenija v nanotehnologii [Nanostructural coverings and nanomaterials: Receiving bases. Properties. Scopes. Features of the modern nanostructural direction in nanotechnology]. M.: Librokom, 2012. 368 s.
  8. Eliseev A.A., Lukashin A.V. Funkcionalnye nanomaterialy [Functional nanomaterials]. M.: Fizmatlit, 2010. 456 s.
  9. Rodionov A.I., Efimochkin I.Ju., Bujakina A.A., Letnikov M.N. Sferoidizacija metallicheskih poroshkov (obzor) [The spheroidization of metallic powders (review)] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 60–64. DOI: 10.18577/2071-9140-2016-0-S1-60-64.
  10. Grashhenkov D.V., Shhetanov B.V., Efimochkin I.Ju. Razvitie poroshkovoj metallurgii zharoprochnyh splavov [Development of powder metallurgy of hot strength alloys] // Vse materialy. Jenciklopedicheskij spravochnik. 2011. №5. S. 13–26.
  11. Kablov E.N. Konstruktsionnye i funktsionalnye materialy – osnova ekonomicheskogo i nauchno-tekhnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  12. Bolshakova A.N., Efimochkin I.Ju., Murasheva V.V. Mehanicheski legirovannye dispersno-uprochnennye kompozicionnye materialy [Mechanically alloyed disperse strengthened composite materials] // Konstrukcii iz kompozicionnyh materialov. 2015. №1 (137). S. 36–40.
  13. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  14. Bakradze M.M., Ovsepjan S.V., Bujakina A.A., Lomberg B.S. Razrabotka kompozicii zharoprochnogo nikelevogo splava s rabochej temperaturoj do 800°S dlja diskov gazoturbinnyh dvigatelej [Development of composition of heat resisting nickel alloy with working temperature to 800°С for disks of gas turbine engines] // Voprosy materialovedenija. 2017. №1 (86). S. 64–74.
  15. Garibov G.S., Gric N.M., Volkov A.M., Vostrikov A.V., Fedorenko E.A. Metallovedcheskie aspekty proizvodstva zagotovok diskov iz granuliruemyh zharoprochnyh nikelevyh splavov metodom GIP [Metallovedchesky aspects of production of preparations of disks from granulated heat resisting nickel alloys HIP method] // Tehnologija legkih splavov. 2014. №3. S. 54–59.
  16. Samohin A.V., Alekseev N.V., Sinajskij M.A., Cvetkov Ju.V. Ravnovesnye jenergotehnologicheskie harakteristiki plazmennyh processov poluchenija nitrida, karbida i karbonitrida titana iz hlorida titana [Equilibrium power technical characteristics on plasma processes of receiving nitride, carbide and carbotitanium nitride from titanium chloride] // Fizika i himija obrabotki materialov. 2015. №4. S. 18–24.