Research of influence of homogenizing modes on mechanical properties of large bars from aluminum-lithium alloys V-1481

Oglodkov M.S., Grigoriev M.V., Pahomkin S.I., Ryabova E.N.
Oglodkov M.S., Grigoriev M.V., Pahomkin S.I., Ryabova E.N. Research of influence of homogenizing modes on mechanical properties of large bars from aluminum-lithium alloys V-1481 // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-1-1. URL: https://viam-works.ru/en/journal/2017/8/1
Keywords
Al–Cu–Li, structure, properties, ingots, aluminum-lithium alloy, homogenization, technological plasticity, Al–Cu–Li.
Abstract

A study was made of the features of phase dissolution in the two-step homogenization of pi-lot-industrial ingots of B-1481 alloy based on the Al–Cu–Li system. It is shown that an increase in exposure at the second stage contributes to the almost complete dissolution of the nonequilibrium eutectic. Homogenization of ingots of alloy B-1481 according to the regime: the first stage – at a temperature of 70–100°C below the temperature of the nonequilibrium solidus, and the high-temperature second stage is slightly higher than the temperature of the nonequilibrium solidus, it allows achieving the most complete dissolution of phases precipitated during crystallization, Technological plasticity of the material at the temperature of hot deformation.

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  3. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Alyuminij-litievye splavy novogo pokoleniya i sloistye alyumostekloplastiki na ih osnove [Aluminum-lithium alloys of new generation and layered aluminum glass plastics on their basis] // Tsvetnye metally. 2016. №8 (884). S. 86–91.
  4. Fridlyander I.N., Chuistov K.V., Berezina A.L., Kolobnev N.I. Alyuminij-litievye splavy. Struktura i svojstva [Aluminum-lithium alloys. Structure and properties]. Kiev: Naukova dumka, 1992. 192 s.
  5. Fridlyander I.N., Kolobnev N.I., Sandler V.S. Alyuminij-litievye splavy [Aluminum-lithium alloys] // Mashinostroenie: enciklopediya. M.: Mashinostroenie, 2001. T. II-3. Tsvetnye metally i splavy. Kompozicionnye metallicheskie materialy. S. 156–184.
  6. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  7. Priemoperedayushhee ustrojstvo: pat. 2463364 Ros. Federaciya [Transceiving device: pat. 2463364 Rus. Federation]; zayavl. 03.05.11; opubl. 10.10.12, Byul. №28.
  8. Ovsyannikov B.V., Komarov S.B. Razvitie proizvodstva deformirovannyh polufabrikatov iz alyuminievo-litievyh splavov v OAO «KUMZ» [Development of production of the deformed semi-finished products from aluminum-lithium alloys in JSC «KUMZ»] // Tehnologiya legkih splavov. 2014. №1. S. 97–103.
  9. Ovsyannikov B.V., Zamyatin V.M., Mushnikov V.S., Oglodkov M.S. Termicheskij i mikrorentgenospektralnyj analiz slitkov splava V-1461 na osnove sistemy Al–Cu–Li [Thermal and microx ray spectral analysis of ingots of alloy V-1461 on the basis of Al–Cu–Li system] // Metallovedenie i termicheskaya obrabotka metallov. 2014. №6 (708). S. 12–17.
  10. Kolobnev N.I., Hohlatova L.B., Antipov V.V. Perspektivnye alyuminij-litievye splavy dlya samoletnyh konstrukcij [Perspective aluminum-lithium alloys for aircraft designs] // Tehnologiya legkih splavov. 2007. №2. S. 35–38.
  11. Ryabova E.N., Kolobnev N.I., Hohlatova L.B., Oglodkov M.S. Osobennosti struktury i svojstv listov iz splavov sistemy Al–Cu–Li–Mg [Features of structure and properties of sheets from Al–Cu–Li–Mg system alloys] // Metallurgiya mashinostroeniya. 2015. №1. S. 17–19.
  12. Oglodkov M.S., Hohlatova L.B., Kolobnev N.I., Alekseev A.A., Lukina E.A. Vlijanie termomehanicheskoj obrabotki na svojstva i strukturu splava sistemy Al–Cu–Mg–Li–Zn [Influence of thermomechanical processing on properties and Al–Cu–Mg–Li–Zn system alloy structure] // Aviacionnye materialy i tehnologii. 2010. №4. S. 7–11.
  13. Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie alyuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development aluminum lithium alloys and multistage modes of thermal processing] // Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
  14. Hohlatova L.B., Kolobnev N.I., Oglodkov M.S., Mihajlov E.D. Alyuminij-litievye splavy dlya samoletostroeniya [Aluminum-lithium alloys for aircraft construction] // Metallurg. 2012. №5. S. 31–35.
  15. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  16. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.