The study of influence organic and inorganic corrosion inhibitors on the stress-corrosion cracking high-strength steels
UDC
667.6:620.193
DOI
10.18577/2307-6046-2017-0-6-12-12
Article PDF (Russian)
(504.98 KB)
How to cite
Rakova T.M., Kozlova A.A., Nefyodov N.I., Laptev A.B. The study of influence organic and inorganic corrosion inhibitors on the stress-corrosion cracking high-strength steels // Proceedings of VIAM. 2017. No. 6. DOI: 10.18577/2307-6046-2017-0-6-12-12. URL: https://viam-works.ru/en/journal/2017/6/12
Keywords
paint coatings, corrosion inhibitors, stress-corrosion cracking, brittle fracture.
Abstract
It was conducted studies of organic and inorganic corrosion inhibitors, their combined effect on the development of cracks on high-strength steels and in aqueous media when introduced into the paint coating. It was found that among the inorganic salts and oxides of the most effective in protecting from high-strength steels are brittle chromates provide the longest time to failure of samples and the best protection against general corrosion of steel. Studies have shown that the greatest protective effect is a mixture of inorganic and organic corrosion inhibitors provide a synergistic effect.
Reference list
- Laptev A.B., Nikolaev E.V., Pavlov M.R. Issledovanie prichin razrusheniya stali 06H16N15M2G2TFR zmeevika pechi i razrabotka metoda zashhity [Research of causes of destruction of steel 06H16N15M2G2TFR of coil of the furnace and development of method of protection] // Praktika protivokorrozionnoj zashhity. 2017. №1 (83). S. 39–44.
- Rozenfeld I.L., Rubinshtejn F.I. Antikorrozionnye gruntovki i ingibirovannye lakokrasochnye pokrytiya [Corrosion inhibiting primers and inhibited paint coatings]. M.: Himiya, 1980. S. 95–112.
- Ingibitor «Reakor-2» korrozionno-mehanicheskogo razrusheniya nizkolegirovannyh stalej: pat. 2068628 Ros. Federaciya. №94010478/02 [Reakor-2 inhibitor of corrosion and mechanical destruction of low-alloy steels: pat. 2068628 Rus. Federation. No. 94010478/02]; zayavl. 25.03.94; opubl. 27.10.96, Byul. №30. 5 s.
- Rahmankulov D.L., Bugaj D.E., Gabitov A.I., Golubev M.V., Laptev A.B., Kalimullin A.A. Ingibitory korrozii [Corrosion inhibitors]. Ufa: Reaktiv, 1997. T. 1: Osnovy teorii i praktiki primeneniya. S. 117–128.
- Bugaj D.E., Golubev M.V., Laptev A.B. i dr. O zashhitnyh svojstvah nekotoryh aminov, ketosulfidov, acetalej i ih analogov pri ingibirovanii korrozii pod napryazheniem stroitelnoj stali [About protective properties of some ammines, cetosulfides, atsetaly and their analogs at corrosion inhibition energized building steel]// Bashkirskij himicheskij zhurnal. 1996. T. 3. №4. S. 59–63.
- Astafev V.I., Radaev Yu.N, Stepanova L.V., Shiryaeva L.K. Nakoplenie povrezhdennosti i razrushenie metallov v usloviyah korrozionnogo rastreskivaniya pod napryazheniem [Accumulation of povrezhdennost and destruction of metals in the conditions of stress corrosion cracking]. Samara: Izd-vo Samar. un-ta, 1998. 123 s.
- Gareev A.G., Nasibullina O.A., Rizvanov R.G. Issledovanie osobennostej korrozionnogo rastreskivaniya pod napryazheniem obrazca stali H70, otobrannogo iz ochagovoj zony razrusheniya [Research of features of stress corrosion cracking of sample of the X70 steel which has been selected from zone of destruction] // Neftegazovoe delo. 2015. T. 13. №4. S. 244–248.
- n-izobutil-n-2-trimetilsililoksi(etil)-n-ciklogeksan-2-onilmetilamin v kachestve ingibitora kor-rozionno-mehanicheskogo razrusheniya nizkolegirovannyh stalej: pat. 2119492 Ros. Federaciya. №93047885 [n-isobutyl-n-2-threemethylsililoxi(etil)-n-ciclogexan-2-onilmethylamine as inhibitor of corrosion and mechanical destruction of low-alloy steels: pat. 2119492 Rus. Federation. No. 93047885]; zayavl. 15.10.93; opubl. 27.09.98, Byul. №30. 5 s.
- Bugaj D.E., Laptev A.B., Gabitov A.I. Uchet haraktera adsorbcii ingibitorov na stali pri opredelenii zashhitnyh svojstv v serovodorodnyh sredah pri korrozii pod napryazheniem [Accounting of nature of adsorption of inhibitors on steel at determination of protective properties in hydrosulphuric environments at corrosion energized] // Bashkirskij himicheskij zhurnal. 1994. T. 1. №2. S. 25–27.
- Bugaj D.E., Gabitov A.I., Laptev A.B. i dr. Mehanizm zashhitnogo dejstviya ingibitorov stress-korrozii klassa acetalej [Mechanism of protective effect of inhibitors stress corrosion of class of the acetale] // Bashkirskij himicheskij zhurnal. 1994. T. 1. №2. S. 28–32.
- Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM is 80: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
- Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
- Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kurs M.G., Laptev A.B., Kutyrev A.E., Morozova L.V. Issledovanie korrozionnogo razrusheniya deformiruemyh alyuminievyh splavov pri naturno-uskorennyh ispytaniyah. Chast 1 [Research of corrosion destruction of deformable aluminum alloys at natural accelerated tests. Part 1] // Voprosy materialovedeniya. 2016. №1. S. 116–126.
- Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science ] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Chebotarevskij V.V., Kondrashov E.K. Tehnologiya lakokrasochnyh pokrytij v mashinostroenii [Technology of paint coatings in mechanical engineering]. M.: Mashinostroenie, 1978. S. 76–105.
- Kondrashov E.K., Kuznecova V.A., Semenova L.V., Lebedeva T.A. Osnovnye napravleniya povysheniya ekspluatacionnyh, tehnologicheskih i ekologicheskih harakteristik lakokrasochnyh pokrytij dlya aviacionnoj tehniki [The main directions of increase of utilization, technical and ecological properties of paint coatings for aviation engineering] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 96–102.
- Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytiya [Paint and varnish materials and coatings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
- Nefyodov N.I., Semyonova L.V. Tendencii razvitiya v oblasti konformnyh pokrytij dlya vlagozashhity i elektroizolyacii plat pechatnogo montazha i jelementov radiojelektronnoj apparatury [Development tendencies in the field on conformal coating for the moisture protection and electrical insulation of printed-circuit boards and electronic elements] // Aviacionnye materialy i tehnologii. 2013. №1. S. 50–52.
- Kozlova A.A., Kondrashov E.K., Deev I.S., Shhegoleva N.E. Issledovanie vliyaniya frakcionnogo sostava i udelnoj poverhnosti antikorrozionnyh pigmentov na zashhitnye svojstva epoksidnyh pokrytij [Research of influence of fractional structure and specific surface of anticorrosive pigments on protective properties of epoxy coverings] // Korroziya: materialy, zashhita. 2013. №3. S. 42–48.
- Kozlova A.A., Kondrashov E.K., Deev I.S. Zashhitnye svojstva lakokrasochnyh pokrytij na osnove ftorsoderzhashhego plenkoobrazuyushhego [Protective properties of paint coatings on the basis of the fluorinated film-forming] // Korroziya: materialy, zashhita. 2014. №4. S. 43–48.
- Yakovlev A.D. Himiya i tehnologiya lakokrasochnyh pokrytij: ucheb. posob. dlya vuzov [Chemistry and technology of paint coatings: manual for higher education institutions]. L.: Himiya, 1981. S. 166–170.
- Kondrashov E.K., Kuznecova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Razvitie aviacionnyh lakokrasochnyh materialov [Development of aviation paint and varnish materials] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №5. S. 49–54.
- Semenova L.V., Nefedov N.I. Primenenie epoksidnyh modificirovannyh gruntovok v sistemah LKP [Application of modified epoxy primers in the painting systems] // Aviacionnye materialy i tehnologii. 2014. №3. S. 38–44. DOI: 10.18577/2071-9140-2014-0-3-38-44.