Research of influence of operational and climatic factors on properties of material for ballonet pneumatic ladder for emergency evacuation of cabin of the helicopter

Nesterova T.A., Nazarov I.A., Barbotko S.L., Volnyj O.S., Platonov M.M.
Nesterova T.A., Nazarov I.A., Barbotko S.L., Volnyj O.S., Platonov M.M. Research of influence of operational and climatic factors on properties of material for ballonet pneumatic ladder for emergency evacuation of cabin of the helicopter // Proceedings of VIAM. 2017. No. 6. DOI: 10.18577/2307-6046-2017-0-6-11-11. URL: https://viam-works.ru/en/journal/2017/6/11
Abstract

The complex of properties of the fabric film material consisting of polyester fabric (art. 208) with the double-sided polyurethane covering on the basis of SKU-8TB rubber with functional additives, intended for manufacturing ballonet pneumatic ladder for emergency evacuation of cabin of the helicopter is investigated. Results of research of properties of this material in initial condition and after the operational and climatic factors carried out after influence (elevated temperature, humidity, mold fungi, influence of humid tropical climate, etc.) have shown that properties change slightly from reference values that confirms its working capacity at temperatures from -60 to +80°С.

Reference list
  1. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk, 2012. T. 82. №6. S. 520–530.
  2. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  3. Kablov E.N. Klyuchevaya problema – materialy [Materials are the key problem] // Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. inform. mater. 3-e izd., pererab. i dop. M.: VIAM, 2015. S. 458–464.
  4. Kablov E.N. Sozdanie nacionalnoj seti klimaticheskih stancij – neobhodimoe uslovie nadezhnosti i resursa aviacionnoj tehniki [Creation of national network of climatic stations – necessary condition of reliability and resource of aviation engineering] // Krylya Rodiny. 2010. №8. S. 3–6.
  5. Normy letnoj godnosti samoletov transportnoj kategorii: AP-25. 5-e izd., s popravkami 1–8 [Standards of the flight validity of airplanes of transport category: AP-25. 5th ed., with corrections 1–8]. M.: Aviaizdat, 2015. 278 s.
  6. Normy letnoj godnosti grazhdanskih legkih samoletov: AP-23. 4-e izd., s popravkami 1–5 [Standards of the flight validity of civil light aircrafts: AP-23. 4 ed., with corrections 1–5.]. M.: Aviaizdat, 2014. 207 s.
  7. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  8. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  9. Platonov M.M., Nazarov I.A., Nesterova T.A. Tkaneplenochnye materialy dlya naduvnyh aviacionnyh sredstv spaseniya [Fabrics film materials for inflatable aviation survival equipment] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 06. Available at: http://www.materialsnews.ru (accessed: February 20, 2017).
  10. Platonov M.M., Nazarov I.A., Nesterova T.A. Tkaneplenochnye materialy dlya naduvnyh aviacionnyh sredstv spaseniya [Fabrics film materials for inflatable aviation survival equipment] // Sb. dokl. konf. «Teploizolyacionnye i tekstilnye materialy aviacionnogo naznacheniya». M.: VIAM, 2013. S. 7.
  11. Nesterova T.A., Platonov M.M., Sharakina L.A. Ocenka svojstv pozharobezopasnogo tkaneplenochnogo materiala dlya dorozhki skolzheniya spasatelnogo trapa [Assessment of properties of the fireproof fabric film material for path of sliding of the saving rescue ladder] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 09. Available at: http://www.viam-works.ru (accessed: February 20, 2017). DOI: 10.18577/2307-6046-2014-0-10-9-9.
  12. Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Issledovanie svojstv ugleplastika na polifenilensulfidnom svyazuyushhem posle uskorennyh i naturnyh klimaticheskih ispytanij [Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
  13. Sorokin A.E., Bejder E.Ya., Perfilova D.N. Vliyanie klimaticheskih faktorov na svojstva ugleplastika na polifenilensulfidnom svyazuyushhem [Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 10. Available at: http://www.viam-works.ru (accessed: September 20, 2015). DOI: 10.18577/2307-6046-2015-0-1-10-10.
  14. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] // Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  15. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Investigation of polymer composite materials under effect of climatic factors and loads in laboratory and environmental conditions] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 68–73.
  16. Barbotko S.L., Nesterova T.A., Kirienko O.A., Volnyj O.S. Issledovanie vliyaniya ekspluatacionnyh i klimaticheskih faktorov na goryuchest tekstilnyh materialov aviacionnogo naznacheniya [The research of operational and climatic factors influence on flammability of textile materials used in aviation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №3. St. 12. Available at: http://www.viam-works.ru (accessed: February 20, 2017). DOI: 10.18577/2307-6046-2016-0-3-12-12.
  17. Platonov M.M., Shuldeshov E.M., Nesterova T.A., Sagomonova V.A. Akusticheskie polimernye materialy novogo pokoleniya (obzor) [Acoustic polymeric materials of new generation (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4. St. 09. Available at: http://viam-works.ru (accessed: February 16, 2017). DOI: 10.18577/2307-6046-2016-0-4-9-9.
  18. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Osobennosti receptur rezin na osnove etilenpropilenovyh kauchukov i ih primenenie v izdeliyah specialnogo naznacheniya (obzor) [Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  19. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  20. Nesterova T.A., Platonov M.M., Nazarov I.A., Barbotko S.L. Issledovaniya po razrabotke novogo materiala dlya balloneta pnevmaticheskogo trapa dlya avarijnogo pokidaniya kabiny vertoleta [Researches on development new material for ballonet of pneumatic emergency slide of helicopter] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №12 (48). St. 07. Available at: http://www.viam-works.ru (accessed: February 20, 2017). DOI: 10.18577/2307-6046-2016-0-12-7-7.