Abstract
The use of composite materials is increasingly on a large scale. In the automotive industry composite materials has been used for many years, and every year the level of usage is increasing. If previously, PCM was mainly used as interior trim in the parts not bearing a significant load, but now the polymers were used in large-size details, and foreign companies such as BMW, Ford, Mercedes, Audi and it made the car body which consists entirely of composites.
Reference list
- Kablov E.N. V istorii VIAM Petr Dementev zanimaet osoboe mesto [In the history of VIAM Peter Dementyev takes special place] // Krylya Rodiny. 2017. №1. S. 1–2.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation are the base of innovations, technological leadership and national security of Russia] // Intellekt & Tehnologii. 2016. №4. S. 41–46.
- Kablov E.N. Materialy i tehnologii VIAM dlya «Aviadvigatel» [Materials and VIAM technologies for «Aircraft engine»] // Permskie aviacionnye dvigateli: inform. byul. 2014. №31. S. 43–47.
- Kablov E.N. O nastoyashhem i budushhem VIAM i otechestvennogo materialovedeniya: intervyu [About the real and future VIAM and domestic materials science: interview] // Rossijskaya akademiya nauk. 2015. 19 yanvarya.
- Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
- Kablov E.N., Chursova L.V., Babin A.N., Muhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnyh svyazuyushhih dlya polimernyh kompozicionnyh materialov [Development of FSUE «VIAM» in the field of molten binding for polymeric composite materials] // Polimernye materialy i tehnologii. 2016. T. 2. №2. S. 37–42.
- Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
- Chursova L.V., Dushin M.I., Hrulkov A.V., Muhametov R.R. Osobennosti tehnologii izgotovleniya detalej iz kompozicionnyh materialov metodom propitki pod davleniem [Researches and development of autoclave and autoclave-free technologies of formation of PCM] // Kompozicionnye materialy v aviakosmicheskom materialovedenii: sb. tez. dokl. mezhotras. nauch.-tehnich. konf. M.: VIAM, 2009. S. 17.
- Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] // Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
- Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokoleniya [Modern production technologies of polymeric composite materials of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 07. Available at: http://www.viam-works.ru (accessed: April 03, 2017).
- Vicari A. Will Carbon Fiber Find Widespread Use in the Automotive Industry? // Composites today. 2015. №3. Р. 3–10.
- Mirnyj M.M. Avtomobili budushhego budut na 75% iz plastika [Cars of the future will be for 75 % from plastic] // Kompozitnyj mir. 2015. №3. S. 5–10.
- Mirnyj M.M. Avtomobilestroenie kak drajver sprosa na polimernuyu produkciyu [Automotive industry as driver of demand for polymeric products] // Informacionno-analiticheskij spravochnik. 2014. S. 15–18.
- Available at: http://www.1gai.ru/techno-cars/514689-bmw-originalnym-obrazom-okazalis-vperedi-po-konstrukcii-novoy-7-serii.html (accessed: April 17, 2017).
- Available at: http://remontpeugeot.ru/avtozhizn/ novye-kompozitnye-materialy-v-avtomobile-primenenie-konstrukcii.html (accessed: April 18, 2017).
- Kichigin A.S. Plastmassovaya evolyuciya [Plastic evolution] // Neftehimiya RF. 2016. №2. S. 1–4.
- Sabitov A.A. Primenenie v avtomobilestroenii kompozicionnyh materialov [Application in automotive industry of composite materials]. Irkutsk: Irkutskij tehnikum mashinostroeniya, 2016. S. 5–6.
- Available at: https://rg.ru/2016/05/26/avtoprom-budushchee-rynka-za-avtomobiliami-iz-polimerov.html (accessed: April 18, 2017).