Influence of electro-magnetic field treatment at the solidification process on mechanical properties of Ni–Al and Co–Cr–Al–Ni alloys

Nazarkin R.M., Konokotin S.P.
Nazarkin R.M., Konokotin S.P. Influence of electro-magnetic field treatment at the solidification process on mechanical properties of Ni–Al and Co–Cr–Al–Ni alloys // Proceedings of VIAM. 2017. No. 5. DOI: 10.18577/2307-6046-2017-0-5-10-10. URL: https://viam-works.ru/en/journal/2017/5/10
Abstract

The research of Ni–Al alloy and Co–Cr–Al–Ni–Y alloy are provided. Those alloys has tendency to the cold brittleness at the room temperature. The alloy of Ni–Al system and alloy of Co–Cr–Al–Ni–Y system were produced by the technique of electro-magnetic field treatment during equiaxal solidification. It is shown that Ni–Al alloy and Co–Cr–Al–Ni–Y alloy after the electro-magnetic field treatment of liquid metal during crystallization process the size of constituents are decreasing. In addition, the formation of crystallographic texture for researched alloys is detected. For Ni–Al alloy the linear dependence of impact hardness growth on increase of electro-magnetic field induction is identified. It is shown that using of the electro-magnetic field treatment at the crystallization process lead to significantly reduction of the weight loss after heat resistance testing for Ni–Al alloy samples. In addition, the change of phase structure of Ni–Al alloy which produced by electro-magnetic field

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizatsii v resursosberegayushchej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 01. Available at: http://www.viam-works.ru (accessed: February 21, 2017).
  3. Drane Zh.M. Uspehi v razvitii napravlenno zakristallizovannykh i evtekticheskih zharoprochnyh splavov [Successes in development directionally zakristallizovanny and evtektichesky hot strength alloys] // Zharoprochnye splavy dlya gazovykh turbin. M.: Metallurgiya, 1981. S. 365–387.
  4. Proizvodstvo vysokotemperaturnyh litykh lopatok aviacionnyh GTD / pod red. S.I. Iatsika [Production of high-temperature cast blades of aviation GTD / ed. by S.I. Yatsik]. M.: Mashinostroenie, 1995. 33 s.
  5. Kablov E.N., Petrushin N.V., Eliutin E.S. Monokristallicheskie zharoprochnye splavy dlya gazoturbinnyh dvigatelei [Single-crystal hot strength alloys for gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 38–52.
  6. Grinberg B.A., Ivanov M.A. Intermetallidy Ni3Al i TiAl: mikrostruktura, deformatsionnoe povedenie [Ni3Al and TiAl intermetallic compound: microstructure, deformation behavior]. Ekaterinburg: Izd-vo UrO RAN, 2002. 360 s.
  7. Li X., Wang J., Zhang J., Han Y., Li. X. Directional Solidification Microstructure of a Ni-Based Superalloy: Influence of a Weak Transverse Magnetic Field // Materials. 2015. Vol. 8. P. 3428–3441.
  8. Nikrityuk P.A., Eckert K., Grundmann R. Electromagnetically Forced Swirling Flow During Solidification of a Binary Metal alloy // Journal of Computational and Applied Mechanics. 2004. Vol. 5. No. 2. P. 337–352.
  9. Verte L.A. MGD-tehnologiya v proizvodstve chernyh metallov [MGD technology in production of ferrous metals]. M.: Metallurgiya, 1990. 119 s.
  10. Verte L.A. Elektromagnitnaya razlivka i obrabotka zhidkogo metalla [Electromagnetic pouring and processing of liquid metal]. M.: Metallurgiya, 1967. 208 s.
  11. Verte L.A. Magnitnay gidrodinamika v metallurgii [Magnetic hydrodynamics in metallurgy]. M.: Metallurgiya, 1975. 287 s.
  12. Sposob polucheniya otlivok: a. s. 1367286 SSSR [Way of receiving molding: copyright certificate 1367286 USSR]; zaiavl. 25.02.85; opubl. 15.07.94.
  13. Nazarkin R.M., Konokotin S.P., Moiseeva N.S., Azarovskii E.N. Issledovanie Cr-splava, kristallizovannogo v elektromagnitnom pole [Research of Cr-alloy, crystallized in electromagnetic field] // Liteinoe proizvodstvo. 2014. №12. S. 23–27.
  14. Sposob polucheniya otlivok: pat. 2368457 Ros. Federaciya [Way of receiving molding: pat. 2368457 Rus. Federation]; zaiavl. 24.01.08; opubl. 27.09.09.
  15. Mneian M.G. Novye professii magnita [New professions of magnet]. M.: Prosveshchenie, 1985. S. 28–35.
  16. Samoilov A.I., Konokotin S.P., Roshchina I.N. i dr. Povyshenie plastichnosti materialov kristallizatsiei v elektromagnitnom pole [Increase of plasticity of materials by crystallization in electromagnetic field] // Aviacionnye materialy i tehnologii. 2008. Vyp. 1. S. 32–37.
  17. Konokotin S.P., Moiseeva N.S. Vliyanie elektromagnitnogo polya na svoistva intermetallidnogo Ni–Al splava [Influence of electromagnetic field on properties of intermetallic Ni–Al of alloy] // Liteinoe proizvodstvo. 2011. №10. S. 17–19.
  18. Moiseeva N.S., Konokotin S.P. Effektivnost vliyaniya elektromagnitnoi obrabotki na strukturu i svoistva litogo splava sistemy Ni–Al [Efficiency of influence of electromagnetic processing on structure and properties of cast alloy of Ni-Al system] // Metallurgiya mashinostroeniya. 2013. №3. S. 27–31.
  19. Konokotin S.P., Moiseeva N.S. Vliyanie metoda kristallizatsii na strukturu splava sistemy Ni–Al posle vysokotemperaturnogo nagreva [Influence of method of crystallization on Ni-Al system alloy structure after high-temperature heating] // Metallurgiia mashinostroeniia. 2013. №4. S. 27–31.
  20. Konokotin S.P., Moiseeva N.S. Povyshenie fiziko-mehanicheskih svojstv splavov na osnove hroma i sistemy Ni–Al, sklonnyh k hladnolomkosti, metodom ravnoosnoj kristallizacii v elektromagnitnom pole [An increase of physical and mechanical properties of Cr-based and Ni–Al alloys by using the equiaxed crystallization in electromagnetic field] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 15–26. DOI: 10.18577/2071-9140-2015-0-3-15-26.
  21. Yu J., Du D., Ren Z., et al. Influence of an Axial Magnetic Field on Microstructures and Aligment in Directioally Solidified Ni-based Superalloy // ISIJ (Iron and Steel Institute of Japan) International. 2016. Article ID: ISIJINT-2016-352. P. 6.
  22. Nochovnaia N.A., Sivakov D.V. Issledovanie vzaimodeistviya poverkhnostnykh sloev titanovykh splavov razlichnogo fazovogo sostava s elektromagnitnym polem [Research of interaction of surface layers of titanium alloys of different phase structure with electromagnetic field] // Aviacionnye materialy i tehnologii. 2010. №2. S. 14–22.
  23. Ospennikova O.G., Podieiachev V.N., Stoliankov Iu.V. Tugoplavkie splavy dlia novoi tekhniki [Refractory alloys for innovative equipment] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №10. St. 05. Available at: http://www.viam-works.ru (accessed: February 21, 2017). DOI:10.18577/2307-6046-2016-0-10-5-5.