Abstract

Bismaleimide binder was developed with high resistance to water. Using a part of the binder allyl and propenyl hardener yielded net structurally elasticized co-polyimide. The choice of a ratio of components, the use of active diluents, the variation in time of synthesis allowed to obtain without solvent of bismaleimide binder composition for the manufacture of composite materials with operating temperature up to 200°C in a humid environment.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossiiskii khimicheskii zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N., Chursova L.V., Babin A.N., Muhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuiushchih dlya polimernyh kompozitsionnyh materialov [Development of FSUE «VIAM» in the field of molten binding for polymeric composite materials] // Polimernye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
  4. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: September 05, 2016). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  5. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  6. Beider E.Ya., Petrova G.N., Dykun M.I. Appretirovanie uglerodnyh volokon-napolnitelej termoplastichnyh karboplastikov [Dressing of carbon fibers – fillers of thermoplastic carbon reinforced plastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 03. Available at: http://www.viam-works.ru (accessed: March 06, 2017). DOI: 10.18577/2307-6046-2014-0-10-3-3.
  7. Tyumeneva T.Yu., Kogtyonkov A.S., Lukina N.F., Chursova L.V. Vliyanie napolnitelej na svojstva kleev rezinotekhnicheskogo naznacheniya [Influence of fillers on properties of adhesives of industrial rubber assignment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 05. Available at: http://www.viam-works.ru (accessed: February 09, 2016). DOI: 10.18577/2307-6046-2014-0-4-5-5.
  8. Gulyaev I.N., Gunyaev G.M., Raskutin A.E. Polimernye kompozitsionnye materialy s funktsiyami adaptacii i diagnostiki sostoianiya [Polymeric composite materials with functions of adaptation and condition diagnostics] // Aviacionnye materialy i tehnologii. 2012. №S. S. 242–253.
  9. Muhametov R.R., Dolgova E.V., Merkulova Yu.I., Dushin M.I. Razrabotka bismaleimidnogo termostoikogo svyazuiushchego dlya kompozitsionnyh materialov aviacionnogo naznacheniya [Development of heat-resistant bismaleimide binder for composites for aeronautical application] // Aviacionnye materialy i tehnologii. 2014. №4 (33). S. 53–57. DOI: 10.18577/2071-9140-2014-0-4-53-57.
  10. Stenzenberger H.D. Recent advances in thermosetting polyimides // British Polymer Journal. 1988. Vol. 20. No. 5. P. 383–396.
  11. McConnell V.P. Resins for the hot zone. Part II: BMIs, CEs, benzoxazines and phthalonitriles // High Performance Composites. 2009. Vol. 17. Issue 5. P. 43. Available at: http://www.compositesworld.com (accessed: April 12, 2017).
  12. Mangalgiri P.D. Polymer-matrix composites for high-temperature applications // Def. Sci. J. 2005. Vol. 55. No. 2. P. 175–193.
  13. Black S. Are high-temp thermosets ready to go commercial? // High-Perform Composites. Available at: http://www.compositesworld.com/articles/are-high-temp-thermosets-ready-to-go-commercial (accessed: April 12, 2017).
  14. Iijima T. The Polymeric Materials Encyclopedia, Boca Raton: CRC, 1996. Vol. 1. P. 683–687.
  15. Mikhailin Yu.A. Termoustoichivye polimery i polimernye materialy [Thermosteady polymers and polymeric materials]. SPb.: Professiia, 2006. S. 528–623.
  16. Mikhailin Yu.A., Miichenko I.P. Maleinimidnye sviazuiushchie (obzor) [Maleinimide binding (overview)] // Plasticheskie massy. 1992. №5. S. 56–59.