About features of research of structure and properties foam polymers

Kotova E.A., Avtaev V.V., Erasov V.S., Gulina I.V.
Kotova E.A., Avtaev V.V., Erasov V.S., Gulina I.V. About features of research of structure and properties foam polymers // Proceedings of VIAM. 2017. No. 3. DOI: 10.18577/2307-6046-2017-0-3-11-11. URL: https://viam-works.ru/en/journal/2017/3/11
Keywords
foam, cellular structure, laser scanning microscope, 3D image of the surface, profile of the surface topography, size of the cell.
Abstract

Тhe article describes the various methods of quantitative analysis of microscopic structures using a laser scanning microscope. A method for estimating the relative size of the foam cells, consisting of two phases - the base polymer and the void filled with a gaseous substance, by inscribing circle profile in cellular surface structure with elementary structural element in the form of a three-dimensional polyhedron, is offered. The problems of assessment structures with developed relief, as two-dimensional images from an optical microscope, are shown. Work is executed as part of the comprehensive scientific direction 2. «Fundatally-oriented research, qualification of materials, non-destructive testing» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  3. 3 Kablov E.N., Bejder E.Ya., Petrova G.N., Stolyankov Yu.V., Rumyanceva T.V. Penopoliimidy [Foamed polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 09. Available at: http://viam-works.ru (accessed: November 23, 2016). DOI: 10.18577/2307-6046-2015-0-4-9-9.
  4. Doroshenko N.I., Chursova L.V. Evolyuciya materialov dlya lopastej vertoletov [Evolution of materials for blades of helicopters] // Aviacionnye materialy i tehnologii. 2012. №2. S. 16–18.
  5. Kablov E.N. Khimiya v aviatsionnom materialovedenii [Chemistry in aviation materials science] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 3–4.
  6. Stolyankov Yu.V., Bejder E.Ya., Platonov M.M., Petrova G.N. Ustrojstvo dlya mehanicheskoj obrabotki vspenennyh polimernyh materialov [A device for machining of foamed polymer materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 08. Available at: http://www.viam-works.ru (accessed: November 23, 2016). DOI: 10.18577/2307-6046-2015-0-5-8-8.
  7. Dementev A.G. Struktura i svojstva gazonapolnennyh polimerov: avtoref. dis. na soisk. uchenoj stepeni d-ra tehn. nauk [Structure and properties of gas-filled polymers: thesis of doct. tech. sci.]. M., 1997. 42 s.
  8. Chernous D.A., Shilko S.V. Issledovanie uprugoj anizotropii otkrytoporistyh materialov [Research of elastic anisotropy open porous materials] // Fizicheskaya mezomehanika. 2006. T. 9. №2. S. 79–84.
  9. Yakovlev N.O. Issledovanie i opisanie relaksacionnogo povedeniya polimernyh materialov (obzor) [Study and description of relaxation behavior of polymers (review)] //Aviacionnye materialy i tehnologii. 2014. №S4. S. 50–54. DOI: 10.18577/2071-9140-2014-0-s4-50-54.
  10. GOST 22023–76. Materialy stroitelnye. Metod mikroskopicheskogo kolichestvennogo analiza struktury. M., 1976 (ne dejstvuet, otmenen v RF) [GOST 22023–76. Materials construction. Method of the microscopic quantitative analysis of structure. M., 1976 (does not operate, it is cancelled in the Russian Federation)].
  11. Rush K.С. Load-compression behavior of flexible foams // J. Appl. Pol. Sci., 1969. Vol. 13. No 11. P. 2297–2311.
  12. Rush K.С. Load-compression behavior of brittle foams // J. Appl. Pol. Sci., 1970. Vol. 14. No 5. P. 1263–1276.
  13. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: November 23, 2016). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  14. Lavrov A.V., Erasov V.S., Nochovnaya N.A., Kotova E.A. Issledovanie ansamblya vtorichnyh treshhin vblizi ustalostnogo izloma v obrazce iz titanovogo splava VT23M [Research of ensemble of secondary cracks near fatigue fracture in sample from BT23M titanium alloy] // Deformaciya i razrushenie materialov. 2016. №6. S. 42–45.
  15. GOST 5639–82. Stali i splavy. Metody vyyavleniya i opredeleniya velichiny zerna [GOST 5639-82. There were also alloys. Methods of identification and determination of size of grain]. M.: Izdatelstvo standartov, 2003. 21 s.