Strain and stress evolution in organic glasses with different structures at non-uniform heating

Yakovlev N.O., Mekalina I.V., Kharitonov G.M., Khitrova O.I.
Yakovlev N.O., Mekalina I.V., Kharitonov G.M., Khitrova O.I. Strain and stress evolution in organic glasses with different structures at non-uniform heating // Proceedings of VIAM. 2017. No. 3. DOI: 10.18577/2307-6046-2017-0-3-10-10. URL: https://viam-works.ru/en/journal/2017/3/10
Keywords
organic glass, polymethylmethacrylate, relaxation behavior, rubber-like elastic strain.
Abstract

The strain and stress evolution characteristics of the organic glass with linear (SO-120, Tg=120°C) and copolymer rarely cross-linked structures (VОS-2, Tg=148°C) and oriented versions thereof – АО-120 (orientation degree 60 and 79%) and VОS-2АО (orientation degree 50%), accordingly, at a non-uniform heating across the thickness, were investigated. It was shown that the rubber-like elastic strain by heating, thermoelastic and residual temperature stress in organic glazing in a large extent depend on the modulus of elasticity and coefficient of linear expansion of the glass. The oriented glass tightness similar to the tightness of the elementary layers of glazing at non-uniform heating has a significant impact on the development of shrinkage strain in the layers. These deformations cause an increase in tensile stresses during cooling and residual temperature stress.

This work was performed as part of the comprehensive scientific areas 2.2. «Qualification and materials research» («The strategic directions of development of materials and technologies of their processing for the period till 2030») 

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Yakovlev N.O. Issledovanie i opisanie relaksacionnogo povedeniya polimernyh materialov (obzor) [Study and description of relaxation behavior of polymers (review)] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 50–54. DOI: 10.18577/2071-9140-2014-0-s4-50-54.
  3. Yakovlev N.O. Ocenka granic oblasti relaksacionnogo povedeniya organicheskogo stekla na osnove polimetilmetakrilata [Assessment of borders of area of relaxation behavior of organic glass on basis polymethylmetacrylate] // Plasticheskie massy. 2015. №1–2. S. 36–39.
  4. Yakovlev N.O., Erasov V.S., Sentyurin E.G., Haritonov G.M. Relaksaciya ostatochnyh napryazhenij v aviacionnyh organicheskih steklah pri poslepoletnoj stoyanke samoleta [Relaxation of residual stresses in aviation organic glasses at postflight parking of airplane] // Aviacionnye materialy i tehnologii. 2012. №2. S. 66–69.
  5. Yakovlev N.O., Sentyurin E.G., Kharitonov G.M. [Features of rubber-like elastic strain in organic glasses during their unloading at temperatures near to the softening temperature] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 12. Available at: http://www.viam-works.ru (accessed: March 28, 2016). DOI: 10.18577/2307-6046-2015-0-9-12-12
  6. Kharitonov G.M., Yakovlev N.O., Mekalina I.V. Vliyanie fiziko-mekhanicheskikh kharakteristik orgstekol na napryazheniya v samoletnom osteklenii pri aerodinamicheskom nagreve [Influence of physicomechanical characteristics of organic glasses on tension in aircraft glazing at aerodynamic heating] // Aviatsionnye materialy i tekhnologii. 2015. №S1. S. 56–60. DOI: 10.18577/2071-9140-2015-0-S1-56-60.
  7. Kablov E.N. Himiya v aviacionnom materialovedenii [Materials and chemical technologies for aviation engineering] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  8. Mekalina I.V., Bogatov V.A., Trigub T.S., Sentyurin E.G. Aviacionnye organicheskie stekla [Aviation organic glasses] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 04. Available at: http://www.viam-works.ru (accessed: March 28, 2016).
  9. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  10. Bogatov V.A., Trigub T.S., Mekalina I.V., Ayzatulina M.K. Otsenka ekspluatatsionnykh kharakteristik novykh teplostoykikh organicheskikh stekol VOS-1 i VOS-2 [Assessment of utilization properties of new heatresistant organic glasses VOS-1 and VOS-2] // Aviatsionnye materialy i tekhnologii. 2010. №1. S. 21–26.
  11. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  12. Yakovlev N.O. Opisanie deformacionnyh krivyh polimernyh stekol [Description of deformation curve polymeric glasses] // Vysokomolekulyarnye soedineniya. Ser. A. 2017. T. 59. №3. S. 1–6.
  13. Haritonov G.M., Hitrova O.I., Yakovlev N.O., Erasov V.S. Zakonomernosti povedeniya VE deformacij v aviacionnyh steklah iz linejnyh i poperechnosshityh polimerov pri znakoperemennyh nagruzheniyah [Patterns of behavior of VE of deformations in aviation glasses from the linear and cross sewed polymers at sign-variable loadings] // Aviacionnaya promyshlennost. 2011. №3. S. 7.
  14. Yakovlev N.O., Mekalina I.V., Sentyurin E.G. Peculiarities of resilient highly elastic deformation of organic glasses with linear and rarely cross-linked structure // Inorganic Materials: Applied Research. 2015. Vol. 6. No. 4. P. 336–342. DOI: 10.1134/S2075113315040267.
  15. Kablov E.N., Yakovlev N.O., Haritonov G.M., Mekalina I.V. Osobennosti relaksacionnogo povedeniya polimernyh stekol na osnove polimetilmetakrilata i ih uchet pri prochnostnom raschete aviacionnogo ostekleniya [Features of relaxation behavior of polymeric glasses on basis polymethylmetacrylate and their accounting at strength calculation of aviation glazing] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №9. S. 2–9.