The current state of the question in the field of cleaning of the compressor GTE from operational pollution (review)

Nochovnaya N.A., Nikitin Ya.Yu.
Nochovnaya N.A., Nikitin Ya.Yu. The current state of the question in the field of cleaning of the compressor GTE from operational pollution (review) // Proceedings of VIAM. 2017. No. 3. DOI: 10.18577/2307-6046-2017-0-3-5-5. URL: https://viam-works.ru/en/journal/2017/3/5
Keywords
cleaning, removing, carbon deposits, operational pollution, titanium alloys, GTE, GTU.
Abstract

Are considered foreign and domestic cleaning technology flow of the gas turbine compressor from pollution (carbon deposits) in the operation and repair of the factory. The advantages and disadvantages of existing clean technologies. It was found that most of the available publications hardly carry experimental data on effect of treatment technologies on the physico-chemical and mechanical properties of the parts to be cleaned. It is shown that further work should focus on applied research in technology to remove carbon deposits from a titanium alloy parts in the factory. Particular attention should be given to finding a resource-saving way to clean parts made of titanium alloys, providing fast and safe removal of carbon deposits without affecting the performance of the cleaned parts.

Reference list
  1. Ujam A.J., Ekere P.O., Chime T.O. Performance Evaluation of a Gas Turbine Power Plant by the application of Compressor Off-Line and On-Line Water Washing Techniques (A Case Study of 450MW Sapele Power Station in Delta State, Nigeria) // IOSR Journal of Engineering. 2013. Vol. 3. Issue 11. P. 29–41.
  2. Hovland G.E., M. Antoine M. Scheduling of Gas Turbine Compressor Washing // Intelligent Automation & Soft Computing. 2006. Vol. 12. Issue 1. Р. 63–73.
  3. Maiwada B., Muaz N.I., Ibrahim S., Musa S.M. Impacts of Compressor Fouling On the Performance of Gas Turbine // International Journal of Engineering Science and Computing. 2016. Vol. 6. Issue 3. P. 2118–2125.
  4. Meher-Homji C.B., Bromley A.F. Gas Turbine Axial Compressor Fouling and Washing // Proceedings of the thirty-third turbomachinery symposium. USA, Texas, A&M University, 2004. P. 163–191.
  5. Modern Gas Turbine Systems: High Efficiency, Low Emission, Fuel Flexible Power Generation / ed. by P. Jansohn. Woodhead Publishing, 2013. 838 p.
  6. Razak A.M.Y. Industrial Gas Turbines: Performance and Operability. CRC Press, 2007. 624 p.
  7. Hovland G.E., M. Antoine M. Economic optimization of gas turbine compressor washing // Proceedings of the Australasian Universities Power Engineering Conference. Brisbane, 2004. P. 78–83.
  8. Boyce M.P., Gonzalez F. A study of on-line and off-line turbine washing to optimize the study of a gas turbine // Journal of Engineering for Gas Turbines and Power. 2007. Vol. 129. No. 1. P. 114–122.
  9. Enyia J.D., Li J., Thаnk-God I., Igbong D.I. Industrial Gas Turbine On-line Compressor Washing for Power Generation // Isaiah International Journal of Engineering Research and Technology. 2015. Vol. 4. Issue 08. P. 500–506.
  10. Semenyuk A.V., Andreev A.K., Semenyuk L.A. Ekspluatacionnye zagryazneniya gazoturbonagnetatelej DVS i sposoby ih ochistki: metod. ukaz. [Operational pollution of turbo gas supercharger ICE and ways of their cleaning: methodical instructions]. Vladivostok: MGU im. adm. G.I. Nevel'skogo, 2008. 30 s.
  11. Zysin L.V. Parogazovye i gazoturbinnye teplovye elektrostancii: ucheb. posobie [Steam-gas and gas-turbine thermal power stations: manual]. SPb.: Sankt-Peterburgskij gos. politeh. un-t, 2010. 368 s.
  12. Sulejmanov A.M. Energosberezhenie v tehnologicheskih processah truboprovodnogo transporta gaza: avtoref. dis. … kand. tehn. nauk [Energy saving in technological processes of pipeline transport of gas: thesis of cand. tech. sci.]. Ufa, 2005. 22 s.
  13. Stalder J.P. Gas Turbine Compressor Washing State of the Art: Field Experiences // Journal of Engineering for Gas Turbines and Power. 2001. Vol. 123. Р. 363–370.
  14. Kitaev S.V. Povyshenie energeticheskoj effektivnosti raboty gazoperekachivayushhih agregatov: avtoref. dis. … kand. tehn. nauk. Ufa, 2003. 22 s.
  15. Available at: http://www.pmz.ru/pr/other/ntex/ib15_3/ib15_20-21/ (accessed: April 11, 2016).
  16. Rudachenko A.V., Chuhareva N.V. Gazoturbinnye ustanovki dlya transporta prirodnogo gaza: ucheb. posobie [Gas turbine units for transport of natural gas: manual]. Tomsk: Tomskij politeh. un-t, 2012. 213 s.
  17. Аiad G. Cascade Testing and CFD Applied to Gas Turbine Performance Improvement with Compressor Cleaning: PhD Thesis. Great Britain, Сranfield University, 2010. 275 p.
  18. Tehnicheskaya ekspluataciya sudovyh gazoturbinnyh ustanovok / pod red. G.Sh. Rozenberga [Technical operation of ship gas turbine units / ed. by G. Sh. Rosenberg]. M.: Transport, 1986. 222 s.
  19. Ogbonnaya E.A. Gas Turbine Performance Optimization Using Compressor Online Water Washing Technique // Engineering. 2011. No. 3. Р. 500–507.
  20. Slobodyanyuk L.I., Polyakov V.I. Sudovye parovye i gazovye turbiny i ih ekspluataciya: uchebnik [Marine steam and gas turbines and their operation: textbook]. L.: Sudostroenie, 1983. 360 s.
  21. Sposob suhoj ochistki poverhnostej lopatok kompressora: pat. 2513525 Ros. Federaciya [Way of dry cleaning of surfaces of compressor blades: pat 2513525 Rus. Federation]; zayavl. 24.08.12; opubl. 20.04.14. Byul. №11. 9 s.
  22. Available at: http://www.rochem.net/pdfs/Fyrewash/Rochem%20Fyrewash.pdf (accessed: February 02, 2016).
  23. Trenin V.M. Sistema promyvki vysokogo davleniya dlya kompressora GTU [System of washing of high pressure for the GTU compressor] // Turbiny i dizeli. 2008. №1. S. 22–25.
  24. Ustanovka dlya promyvki i emulsirovaniya vozdushno-gazovogo trakta gazoturbinnogo dvigatelya: pat. 2323051 Ros. Federaciya [Installation for washing and emulsirovaniye of air-gas path of the gas turbine engine: pat. 2323051 Rus. Federation]; zayavl. 04.08.06; opubl. 27.04.08. Byul. №12. 20 s.
  25. Available at: http://turbotect.ru/systems/index.html (accessed: April 15, 2016).
  26. Stepankov I.A. Kompleksnoe reshenie dlya ochistki kompressorov GTU: ochistitel Turbo-K i antifriz AF10 [The complex decision for cleaning of GTU compressors: cleaner of Turbo-K and AF10 antifreeze] // Turbiny i dizeli. 2015. №1. S. 54–55.
  27. Available at: http://site.ge-energy.com/businesses/ge_oilandgas/en/literature/en/downloads/onoffline_washing.pdf (accessed: April 12, 2015).
  28. Abass K.O. Techno-economic analysis of gas turbine compressor washing to combat fouling: MS. Great Britain, Сranfield University, 2015. 131 p.
  29. Syverud E. Axial Compressor Performance Deterioration and Recovery through Online Washing: PhD Thesis. Norway, Norwegian University of Science and Technology, 2007. 143 p.
  30. Syverud E., Brekke O., Bakken L. Axial compressor deterioration caused by saltwater ingestion // J. of Turbomachinery. 2007. Vol. 129. No. 1. Р. 119–126.
  31. Syverud E., Bakken L.E. Online water wash test of GE J85-13 // J. of Turbomachinery. 2007. Vol. 129. No. 1. Р. 136–142.
  32. Kurz R., Brun K., Mokhatab S. Gas turbine compressor blade fouling mechanisms // Pipeline & Gas Journal. 2011.Vol. 238. No. 9. P. 18–21.
  33. Brun K., Kurz R., Folles W. Experimental evaluation of the effectiveness of online water washing in gas turbine compressors // ASME/IGTI: Proceedings of the forty-second surbomachinery symposium. USA, Houston, 2013. 18 p.
  34. Igie U., Pilidis P., Foufilas D. at al. Industrial Gas Turbine Performance: Compressor Fouling and On-Line Washing // Journal of turbomachinery. 2014. Vol. 136. Issue 10. 13 p.
  35. Wilkinson P., Shark L. Automatic monitoring of gas turbine air intakes using colour imaging techniques, Insight: Non-Destructive Testing and Condition Monitoring // Insigh – Non-Destructive Testing and Condition Monitoring. 2004. Vol. 46. No. 2. P. 94–97.
  36. Docenko G.N. Razrabotka principov ochistki detalej aviacionnoj tehniki ot nagaropodobnyh zagryaznenij biotehnologicheskim metodom: avtoref. dis. … kand. tehn. nauk [Development of principles of cleaning of details of aviation engineering from nagaropodobny pollution by biotechnological method: thesis of cand. tech. sci.]. M., 2000. 37 s.
  37. Mihajlov D.A., Nedashkovskij A.P., Ivchenko T.G. Tehnologicheskie osobennosti vosstanovleniya lopatok kompressora GTD s primeneniem funkcionalno-orientirovannyh pokrytij [Technological features of recovery of compressor blades of GTD using function-oriented coverings] // Progressivnye tehnologii i sistemy mashinostroeniya. 2014. №1 (47). S. 213–224.
  38. Volkov D.I., Tolkachev A.V. Snyatie nagara s napravlyayushhih apparatov gazoturbinnogo dvigatelya s ispolzovaniem vibroabrazivnoj obrabotki [Removal of deposit from directing devices of the gas turbine engine with use vibro abrasive machining] // Sborka v mashinostroenii, priborostroenii. 2015. №1 (174). S. 32–35.
  39. Makeev R.I., Tolkachev A.V. Vibropolirovalnaya obrabotka v sovremennom tehnologicheskom processe [Vibropolirovalny processing in modern technological process] // Uprochnyayushhie tehnologii i pokrytiya. 2006. №4 (16). S. 49–50.
  40. Leontev V.A., Zimchihis S.D., Kondratyuk E.V., Zamkovoj V.E. Vosstanovlenie rabotosposobnosti GTD s primeneniem novyh tehnologij i materialov [Recovery of operability of GTD using new technologies and materials] // Vestnik dvigatelestroeniya. 2006. №4. S. 99–103.
  41. Available at: http://www.agd-russia.ru (accessed: April 15, 2016).
  42. Plankovskij S.I., Golovin I.I., Sirenko F.F. Analiz sushhestvuyushhih metodov ochistki poverhnosti lopatok turbin v gazoturbinnyh dvigatelyah [The analysis of existing methods of surface cleaning of blades of turbines in gas turbine engines] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2013. №6 (103). S. 8–14.
  43. 43 Available at: https://www.karcher.ru/ru/professional/ochistka-sukhim-ldom.html (accessed: March 17, 2016).
  44. 43 Available at: http://www.elmemesser.ru/ru_RU/use-cases/industry/dry-ice (accessed: March 22, 2016).
  45. Vejko V.P., Kishalov A.A., Mutin T.Yu. i dr. Perspektivy industrialnyh primenenij lazernoj ochistki materialov [Perspectives of industrial applications of laser cleaning of materials] // Nauchno-tehnicheskij vestnik informacionnyh tehnologij, mehaniki i optiki. 2012. №3 (79). S. 50–54.
  46. Shulov V.A., Engelko V.I., Gromov A.N. i dr. Primenenie silnotochnyh impulsnyh elektronnyh puchkov dlya vosstanovleniya ekspluatacionnyh svoistv lopatok gazoturbinnyh dvigatelei [Application of high-current pulse electronic bunches for recovery of operational properties of blades of gas-turbine engines] // Izvestiya vuzov. Poroshkovaya metallurgiya i funkcionalnye pokrytiya. 2014. №1. S. 43–49.
  47. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  48. Nochovnaya N.A., Ivanov V.I., Alekseev E.B., Kochetkov A.S. Puti optimizacii ekspluatacionnyh svojstv splavov na osnove intermetallidov titana [Ways of optimization of operational properties of alloys on the basis of titanium intermetallic compound] // Aviacionnye materialy i tehnologii. 2012. №S. S. 196–206.
  49. Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Povyshenie prochnostnyh harakteristik zharoprochnyh psevdo-α-titanovyh splavov [Strengthening of high-temperature near-α-titanium alloys] // Aviacionnye materialy i tehnologii. 2014. №S5. C. 73–80. DOI: 10.18577/2071-9140-2014-0-S5-73-80.
  50. Horev A.I., Nochovny N.A., Yakovlev A.L. Mikrolegirovanie redkozemelnymi metallami titanovykh splavov [Microalloying rare earth metals of titanium alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 206–212.
  51. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  52. Kablov E.N. Tendentsii i orientiry innovatsionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials. 3rd ed.]. M.: VIAM, 2015. 720 s.
  53. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstrukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  54. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.