Localization of positions of impurity of carbon in crystal structures of polymorphic updatings of Nb5Si3 according to atomistic computer modeling

Marchenko E.I., Kuzmina N.A., Eremin N.N.
Marchenko E.I., Kuzmina N.A., Eremin N.N. Localization of positions of impurity of carbon in crystal structures of polymorphic updatings of Nb5Si3 according to atomistic computer modeling // Proceedings of VIAM. 2017. No. 3. DOI: 10.18577/2307-6046-2017-0-3-4-4. URL: https://viam-works.ru/en/journal/2017/3/4
Keywords
niobium-silicon natural composite materials, atomistic computer simulations, interaction potentials, diffusion, atoms of implementation.
Abstract

The method of atomistic computer modeling was developed consistent model of interatomic potentials, which allowed us to reproduce the crystal structures of three polymorphic modifications of niobium silicide (α-Nb5Si3, β-Nb5Si3, γ-Nb5Si3) with an error no more than 0,6%, as well as to calculate some physical properties. To assess the energy of the entering admixture of carbon atoms in the structure were further developed pair potentials interatomic Si–C, Nb–C and C–C. Two independent methods (Mott–Littleton and simulation in over the cell) first identified the energetically most favorable positions for the impurity atoms of carbon in the investigated structures.

Reference list
  1. Urusov V.S., Eremin N.N. Atomisticheskoe kompyuternoe modelirovanie struktury i svojstv neorganicheskih kristallov i mineralov, ih defektov i tverdyh rastvorov [Atomistic computer modeling of structure and properties of inorganic crystals and minerals, their defects and solid solutions]. M.: GEOS, 2012. 428 s.
  2. Available at: http://www.ras.ru/news/shownews.aspx?id=824e2453-383e-4d9e-b78d-87c9f7bf16ee (accessed: 31.01.2017).
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N., Svetlov I.L., Efimochkin I.Yu. Vysokotemperaturnye Nb-Si-kompozity [High-temperature Nb-Si-composites] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 164–173.
  5. Timofeyeva O.B., Kolodochkina V.G., Shvanova N.F., Neiman A.V. Issledovanie mikrostruktury vysokotemperaturnogo estestvenno kompozicionnogo materiala na osnove niobija, uprochnennogo intermetallidami silicida niobiya [The microstructure analysis of niobium-based high-temperature natural composite material reinforced with niobium silicide intermetallics] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 60–64. DOI: 10.18577/2071-9140-2015-0-1-60-64.
  6. Shchetanov B.V., Efimochkin I.Yu., Paegle S.V., Karachevtsev F.N. Issledovanie vysokotemperaturnoj prochnosti in-situ-kompozitov na osnove Nb, armirovannyh monokristallicheskimi voloknami α-Al2O3 [Study of high-temperature strength of Nb–Si–Ti in-situ-composites reinforced by single-crystal α-Al2O3] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 53–59. DOI: 10.18577/2071-9140-2016-0-3-53-59.
  7. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  8. Kocherzhinskij Yu.A., Yupko L.M., Shishkin E.A. Diagramma sostoyaniya Nb–Si [Chart of condition of Nb–Si] // Izv. AN SSSR. Metally. 1980. №1. C. 206–211.
  9. Aronsson B. The crystal structure of Mo5 Si3 and W5 Si3 // Acta Chemica Scandinavica. 1955. No. 9. P. 1107–1110.
  10. Schachner H., Cerwenka E., Nowotny H.N. Neue Silizide vom M5Si3-Typ mit D 88-Struktur // Journal of the American Ceramic Society. 1982. Vol. 65. P. 260–265.
  11. Schachner H., Cerwenka E., Nowotny H. Neue Silizide vom M5Si3-Typ mit D 88-Struktur // Monatshefte fuer Chemie und verwandte Teile anderer Wissenschaften. 1954. Vol. 85. P. 245.
  12. Kablov E.N., Kuzmina N.A., Eremin N.N., Svetlov I.L., Nejman A.V. Atomnye modeli struktury silicidov niobiya v in-situ kompozitah Nb–Si [Nuclear models of structure of silicides of niobium in in-situ Nb–Si composites] // Zhurnal strukturnoj himii. 2017. №3. T. 58. C. 564–570.
  13. Kuzmina N.A., Eremin N.N., Marchenko E.I., Svetlov I.L. i dr. Puti diffuzii primesej vnedreniya v silicide niobiya Nb5Si3 razlichnyh polimorfnyh modifikacij [Ways of diffusion of impurity of implementation in silicide of Nb5Si3 niobium of different polymorphic updatings] // Kristallografiya. 2017. №4 (v pechati).
  14. Muromcev N.A., Kuz'mina N.A., Marchenko E.I., Eremin N.N., Yakushev D.A. Teoreticheskij kristallohimicheskij analiz pustot v kristallicheskih strukturah polimorfnyh modifikacij Nb5Si3 [Theoretical crystal chemical analysis of emptiness in crystal structures of polymorphic updatings of Nb5Si3] // Mineraly: stroenie, svojstva, metody issledovaniya: sb. tez. dokl. VIII Vseros. molodezhnoj nauchnoj konferencii, Ekaterinburg. 2016. S. 100–101.
  15. Gale G.D., Gale J.D. GULP: A computer program for the symmetry adapted simulation. Journal of the Chemical Society // Faraday Transactions. 1997. Vol. 93. P. 629–637. DOI: 10.1039/A606455H.
  16. Mott N.F., Littleton M.J. Conduction in polar crystals. I. Electrolytic conduction in solid salts // Transactions of the Faraday Society. 1938. Vol. 34. P. 485–495.
  17. Momma and Izumi F. VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data // Journal of Applied Crystallography. 2011. Vol. 44. P. 1272–1276.
  18. Khaenko B.V., Sivak O.P. Structure of the ordering of niobium monocarbide // Soviet Physics, Crystallography = Kristallografiya. 1990. Vol. 35. P. 653–655.
  19. Merz K.M., Adamsky R.F. Synthesis of the wurtzite form of silicon carbide. Reference // Journal of the American Chemical Society. 1959. Vol. 81 (1). P. 250–251.
  20. Li C.L., Kuo J.L., Wang B.A. et al. A new layer compound Nb4SiC3 predicted from first-principles theory // Journal of Physics D Applied Physics. 2009. Vol. 42. No. 7. P. 075404–075409.