High-gradient directional solidification of intermetallic Ni–Al–Ta alloy based on Ni3Al, strengthened by TaC-phase
UDC
669:018.44:669.245
DOI
10.18577/2307-6046-2017-0-3-1-1
Article PDF (Russian)
(1011.16 KB)
How to cite
Petrushin N.V., Elyutin E.S., Raevskih A.N., Treninkov I.A. High-gradient directional solidification of intermetallic Ni–Al–Ta alloy based on Ni3Al, strengthened by TaC-phase // Proceedings of VIAM. 2017. No. 3. DOI: 10.18577/2307-6046-2017-0-3-1-1. URL: https://viam-works.ru/en/journal/2017/3/1
Keywords
Ni3Al
Abstract
Directional solidification of process of experimental intermetallic Ni3Al-based alloy of quaternary system Ni–7Al–13,5Ta–0,07С (wt. %) has been investigated. Phase composition of the alloy is γʹ+γ+MC. Directionally solidified as cylindrical bars of Ni3Al-based alloy were successfully grown with a Bridgman process by slow directional solidification (R=6 mm/h) with high thermal gradient (G=12°C/mm). Studied macrosegregation elements and influence macrosegregation on the physicochemical and structural parameters of directionally solidified intermetallic Ni3Al-based alloy (solidus temperature, liquidus temperature, γ- and γ′-lattice parameters and γ/γ′-lattice misfit).
Reference list
- Kablov E.N., Buntushkin V.P., Bazyleva O.A. Konstrukcionnye zharoprochnye materialy na osnove soedineniya Ni3Al dlya detalej goryachego trakta GTD [High-temperature structural materials based on Ni3Al compounds for details hot gas path of GTE] // Tehnologiya legkih splavov. 2007. №2. S. 75−80.
- Povarova K.B., Buntushkin V.P., Kazanskaya N.K., Drozdov A.A., Bazyleva O.A. Osobo legkie zharoprochnye nanostrukturirovannye splavy na osnove Ni3Al dlya aviacionnogo dvigatelestroeniya i energeticheskogo mashinostroeniya [Particularly light high-temperature nanostructured alloys based on Ni3Al for aircraft engines and power machinery] // Voprosy materialovedeniya. 2008. №2 (54). S. 85–93.
- Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallic alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
- Arginbaeva E.G., Bazyleva O.A., Kolodochkina V.G., Khvatskij K.K. Vliyanie kristallograficheskoj orientacii na strukturu i fiziko-mehanicheskie svojstva intermetallidnogo splava na osnove Ni3Al [The influence of crystallographic oriental on structure, physical and mechanical properties of intermetallic alloys based on Ni3Al] // Aviacionnye materialy i tehnologii. 2013. №2. S. 3–7.
- Kablov E.N., Ospennikova O.G., Petrushin N.V. Novyj monokristallicheskij intermetallidnyj (na osnove γʹ-fazy) zharoprochnyj splav dlya lopatok GTD [New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
- Evgenov A.G., Lukina E.A., Korolev V.A. Osobennosti processa selektivnogo lazernogo sinteza primenitel'no k litejnym splavam na osnove nikelya i intermetallida Ni3Al [Features of process of the selection laser synthesis with reference to cast alloys on the basis of nickel and Ni3Al intermetallic compound] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2016. №5 (23). St. 01. Available at: http://www.materialsnews.ru (accessed: Octoober 10, 2016)
- Vigdorovich V.N., Volpyan A.E., Kurdyumov G.M. Napravlennaya kristallizaciya i fiziko-himicheskij analiz [The directed crystallization and the physical and chemical analysis]. M.: Himiya, 1976. 200 s.
- Petrushin N.V., Bronfin M.B., Chabina E.B., D'yachkova L.A. Fazovye prevrashheniya i struktura napravlenno zakristallizovannyh intermetallidnyh splavov sistemy Ni–Al–Re [Phase transformations and structure directionally crystallized intermetallidny alloys of Ni–Al–Re system] // Metally. 1994. №3. S. 85–93.
- Petrushin N.V., Monastyrskaya E.V. Primenenie napravlennoj kristallizacii k resheniyu problem razrabotki i optimizacii zharoprochnyh materialov [Application of the directed crystallization to the solution of problems of development and optimization of heat resisting materials] // Materialovedenie. 1998. №5. S. 2–10.
- Kurc V., Zam P.R. Napravlennaya kristallizaciya evtekticheskih materialov / per. s nem. V.A. Polskogo; pod red. Yu.N. Tarana [The directed crystallization of eutectic materials / trans. from Ger. by V.A.Polish; ed. by Yu.N.Ram]. M.: Metallurgiya, 1980. 274 s.
- Petrushin N.V., Chabina E.B., Nazarkin R.M. Konstruirovanie zharoprochnyh intermetallidnyh splavov na osnove γ'-fazy s vysokoj temperaturoj plavleniya. Chast 1 [Designing of heat resisting intermetallidny alloys on basis γ'-phases with high melting temperature. Part 1] // MiTOM. 2012. №2 (680). S. 32–38.
- Litye lopatki gazoturbinnyh dvigatelej. Splavy, tehnologii, pokrytiya. 2-e izd. / pod obshh. red. E.N. Kablova [Cast blades of gas turbine engines. Alloys, technologies, coverings. 2nd ed. / gen. ed. by E.N.Kablova]. M.: Nauka, 2006. 632 c.
- Petrushin N.V., Elyutin E.S., Nazarkin R.M. i dr. Segregaciya legiruyushhih elementov v napravlenno zakristallizovannyh zharoprochnyh nikelevyh splavah, soderzhashhih renij i rutenij [Segregation of doping elements in directionally crystallized heat resisting nickel alloys, containing reniye and ruthenium] // Voprosy materialovedeniya. 2015. №1 (81). S. 27–37.
- Petrushin N.V., Elyutin E.S., Nazarkin R.M. at al. Segregation of alloying elements in directionally solidified Re-Ru-containing Ni-base superalloys // Inorganic Materials: Applied Research. 2016. Vol. 7. P. 824–831.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Nash P., West D.R.F. Phase equilibria in the Ni–Ta–Al system // Metal Science. 1979. Vol. 13. Nо. 12. P. 670–676.
- Kablov E.N., Gerasimov V.V., Visik E.M. Tehnologicheskie osobennosti polucheniya monokristallicheskih obrazcov i turbinnyh lopatok iz vysokorenievyh zharoprochnyh splavov na ustanovkah UVNK-9 i VIAM-1790 [Technological features of receiving single-crystal samples and turbine blades from high-rhenium hot strength alloys on the installations UVNK-9 and VIAM-1790] //Aviacionnye materialy i tehnologii. Vyp. Vysokorenievye zharoprochnye splavy, tehnologiya i oborudovanie dlya proizvodstva splavov i lit'ya monokristallicheskih turbinnyh lopatok GTD. M.: VIAM. 2004. S. 91−97.
- Eliot R. Upravlenie evtekticheskim zatverdevaniem [Management of eutectic hardening]. M.: Metallurgiya, 1987. 352 s.