The review of FRP volume porosity definition with ultrasonic non-destructive technique (review)
Dikov I.A., Boychuk A.S. The review of FRP volume porosity definition with ultrasonic non-destructive technique (review) // Proceedings of VIAM. 2017. No. 2. DOI: 10.18577/2307-6046-2017-0-2-10-10. URL: https://viam-works.ru/en/journal/2017/2/10
Keywords
FRP, CFRP, porosity, ultrasonic testing, ultrasonic fluctuation, attenuation coefficient, sound velocity, backscattering noise.
Abstract
The FRP porosity reduces structural strength, as known. At present FSUE «VIAM» specialists develop the automated ultrasonic testing method of aircraft wing porosity. Main ways of FRP volume porosity definition with use of ultrasonic non-destructive technique are observed in this paper. They are based on using ultrasonic waves attenuation coefficient, longitudinal ultrasonic wave velocity, backscattering noise energy, back-wall echo monitoring. Ultrasound scattering mechanism in FRP is described. Empiric curves for attenuation coefficient, ultrasonic wave velocity, backscattering noise energy vs pore quantity obtained by different authors are shown.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Savin S.P. Primenenie sovremennykh polimernykh kompozitsionnykh materialov v konstruktsii planera samoletov semeystva MS-21 [Application of modern polymeric composite materials in design of glider of airplanes of MS-21 family] // Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk. 2012. T. 14. №4 (2). S. 686–693.
- Kablov E.N. Aviatsionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M.: VIAM, 2002. S. 23–47.
- Kablov E.N. Konstruktsionnye i funktsionalnye materialy – osnova ekonomicheskogo i nauchno-tekhnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
- Dushin M.I., Khrulkov A.V., Karavaev R.Yu. Parametry, vliyayushchie na obrazovanie poristosti v izdeliyakh iz polimernykh kompozitsionnykh materi-alov, izgotavlivaemykh bezavtoklavnymi metodami (obzor) [The parameters influencing formation of porosity in products from polymeric composite materials, made by bezavtoklavny methods (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2015. №2. St. 11. Available at: http://www.viam-works.ru (accessed: August 01, 2016). DOI: 10.18577/2307-6046-2015-0-2-10-10.
- Void Content of Reinforce Plastic: ASTM D 2734-09. Standard by ASTM International. 2009. 3 p.
- Ulf Schnars, Rudolf Henrich. Applications of NDT Methods on Composite Structures in Aerospace Industry // Airbus Operations GmbH. Bremen. Available at: http://www.ndt.net/article/cdcm2006/papers/ schnars.pdf (accessed: August 01, 2016).
- Dushin M.I., Donetskiy K.I., Karavaev R.Yu. Ustanovlenie prichin obrazovaniya po-ristosti pri izgotovlenii PKM [Establishment of the reasons of formation of porosity when manufacturing PСM] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №6 (42). St. 08. Available at: http://www.viam-works.ru (accessed: August 01, 2016). DOI: 10.18577/2307-6046-2016-0-6-8-8.
- Merkulova Yu.I., Muhametov R.R. Nizkovyazkoe epoksidnoe svyazuyushhee dlya pererabotki metodom vakuumnoj infuzii [Development of a low-viscosity epoxy binder for processing by vacuum infusion] // Aviacionnye materialy i tehnologii. 2014. №1. S. 39–41. DOI: 10.18577/2071-9140-2014-0-1-39-41.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Dushin M.I., Hrulkov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Out-of-autoclave formation carbon plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
- GOST R 56682–2015. Kompozity polimernye i metallicheskie. Metod opredeleniya obema matritsy, armiruyushchego napolnitelya i pustot [GOST P 56682-2015. Composites polymeric and metal. Method of scoping of the matrix, reinforcing filler and emptiness]. M.: Standartinform, 2016. 24 s.
- Shanshan Ding, Shijie Jin, Zhongbing Luo, Huan Liu, Jun Chen, Li Lin. Investigations on rela-tionship between porosity and ultrasonic attenuation coefficient in CFRP laminates based on RMVM // 7th International Symposium on NDT in Aerospace. Mo.5.A.1. Available at: https://www.ndt-aerospace.com/Portals/aerospace2015/BB/mo5a1.pdf (accessed: August 01, 2016).
- Lin L., Luo M., Tian H.T., Li X.M., Guo G.P. Experimental investigation on porosity of carbon fiber-reinforced composite using ultrasonic attenuation coefficient // 17th World Conference on Nondestructive Testing, October 25–28, 2008. China, Shanghai. Available at: http://www.ndt.net/
- article/wcndt2008/papers/222.pdf (accessed: August 01, 2016).
- Methods and apparatus for porosity measurement: United States Patent US 7,389,693 B2; Appl. No.: 11/355,217; US 2007/0186655 A1; publ. 16.08.07.
- Francis A. Reed, Thomas J. Batzinger, Robert W. Reed and Staffan Jonsson. Porosity Measure-ment in Composites Using Ultrasonic Attenuation Methods // Review of Progress in Quantitative Nondestructive Evaluation. 1993. Vol. 12. P. 1265–1272.
- Jeong H., Hsu D.K. Experimental analysis of porosity-induced ultrasonic attenuation and velocity change in carbon composites // Ultrasonics. 1995. Vol. 33. No. 3. P. 195–203.
- Daniel I.M., Wooh S.C. and Komsky I. Quantitative Porosity Characterization of Composite Materials by Means of Ultrasonic Attenuation Measurements // Journal of Nondestructive Evaluation. 1992. Vol. 11. No. 1. P. 1–8.
- Nerazrushayushchiy control [Non-destructive testing: the directory in the 7th vol.]: spravochnik v 7 t. / pod obshch. red. V.V. Klyueva. M.: Mashinostroenie, 2004. T. 3: Ultrazvukovoy kontrol / I.N. Er-molov, Yu.V. Lange. 864 s.
- Hughes M.S., Handley S.M., Miller J.G. and Madaras E.I. A Relationship between frequency dependent ultrasonic attenuation and porosity in composite laminates // Review in Progress in Quantitative Nondestructive Evaluation. 1987. P. 1037–1044.
- Karabutov A.A., Podymova N.B., Belyaev I.O. Issledovanie vliyaniya poristosti na zatukhanie ultrazvuka v ugleplastikovykh kompozitakh metodom lazerno-ultrazvukovoy spektroskopii [Research of influence of porosity on ultrasound attenuation in ugleplastikovy composites method of laser and ultrasonic spectroscopy] // Akusticheskiy zhurnal. 2013. T. 59. №6. C. 714–721.
- Murashov V.V. Opredelenie poristosti ugleplastikov v avia-kostruktsiyakh lazerno-akusticheskim sposobom ultrazvukovogo kontrolya [Determination of porosity ugleplastikov in aviadesigns in the laser and acoustic way of ultrasonic control] // Aviatsionnaya promyshlennost. 2011. №3. C. 33–37.
- Murashov V.V., Rumyantsev A.F. Diagnostika sostava i svoystv polimernykh kompozitov v detalyakh i konstruktsiyakh [Diagnostics of structure and properties of polymeric composites in details and designs] // Kontrol. Diagnostika. 2008. №8. S. 13–17.
- Dominguez N., Mascaro B. Ultrasonic Non-Destructive Inspection of Localised Porosity in Composite Materials // ECNDT 2006-9th European Conference on NDT 2006. Germany, Berlin. Available at: http://www.ndt.net/article/ecndt2006/doc/Tu.2.1.4.pdf (accessed: August 01, 2016).
- Je-Woong Park et al. Ultrasonic Influence of Porosity Level on CFRP Composite Laminates Using Rayleigh Probewaves // Acta Mechanica Solida Sinica. 2008. Vol. 21. No. 4. P. 298–307. DOI: 10.1007/s10338-008-0834-1.
- Im K.H. et al. On fiber direction and porosity content using ultrasonic pitch-catch technique in CFRP composite solid laminates // 18th International Conference on Composite Materials. 2011. Available at: http://iccm central.org/Proceedings/ICCM18proceedings/data/2.%20Oral%20Presentation/Aug25 (Thursday)/Th04%20Numerical%20Methods%20in%20Composite%20Materials/Th04-6-AK0992.pdf (accessed: August 01, 2016).
- Carsten Brandt, Peter Maa. A State Space Approach for the Non-Destructive Evaluation of CFRP with Ultrasonic Testing // 7th International Symposium on NDT in Aerospace. Mo.3.A.1. 2015. Available at: http://www.ndt.net/article/aero2015/papers/Mo_3_A_1_Brandt_v2.pdf (accessed: August 01, 2016).