Abstract

The analysis of imported materials for the manufacture of air conditioning ducts has been carried out and, based on it, the basic minimum requirements for the Russian materials being developed are determined. Сompositions for flexible and rigid SCR elements were selected, and technological parameters for the manufacture of GRP for rigid SCR elements were investigated and worked out. A new domestic glass fiber reinforced plastic for the manufacture of rigid elements of air ducts SKV was developed. The study of its properties is carried out.

Reference list
  1. Kablov E.N. VIAM. Napravlenie glavnogo udara [Direction of main attack] // Nauka i zhizn. 2012. №6. S. 14–18.
  2. Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova [Armor for «Buran». Materials and technologies of VIAM for ISS «Energiya–Buran» / gen. ed. by E.N. Kablov]. M.: Nauka i zhizn, 2013. 128 s.
  3. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  4. Kablov E.N., Kirillov V.N., Zhirnov A.D., Starcev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PCM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  5. Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.E. i dr. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PCM] // Dokl. IX Mezhdunar. nauch. konf. po gidroaviacii «Gidroaviasalon–2012». M., 2012. S. 122–123. 6. Prognozy razvitiya mirovogo rynka grazhdanskoj aviacii [Forecasts of development of the world market of civil aviation] // Tehnicheskaya informaciya. 2003. Vyp. 3–4. S. 6.
  6. Global Market Forecast [Electronic resource]. Available at: http://www.airbus.com (accessed: November 17, 2017).
  7. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM]// Trudy VIAM: ehlektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: November 17, 2017). DOI 10.18577/2307-6046-2014-0-4-6-6.
  8. Veshkin E.A., Postnov V.I., Strelnikov S.V., Abramov P.A., Satdinov R.A. Opyt primeneniya tehnologicheskogo kontrolya polufabrikatov PKM [Experience of application of technological control of semi-finished products of PCM] // Izvestiya Samarskogo nauchnogo centra RAN. 2014. T. 16. №6 (2). S. 393–398.
  9. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  10. Gurit: official site. Available at: http://www.mobile.gurit.com (accessed: November 17, 2017).
  11. Hexcel: official site. Available at: http://www.hexcel.com (accessed: November 17, 2017).
  12. Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Fenolformaldegidnye svjazuyushhie novogo pokoleniya dlya materialov interera [Phenolformaldehyde binding new generation for interior materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
  13. Veshkin E.A., Postnov V.I., Zastrogina O.B., Satdinov R.A. Tehnologiya uskorennogo formovaniya trehslojnyh sotovyh panelej samoleta [Technology of the accelerated formation of three-layered cellular panels of airplane] // Izvestiya Samarskogo nauchnogo centra RAN. 2013. №4–4. S. 799–805.
  14. Veshkin E.A., Abramov P.A., Postnov V.I., Strel'nikov S.V. Vliyanie tehnologii podgotovki preprega na svojstva PKM [Influence of technology of preparation of prepreg on PCM properties] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №9. S. 8–14.
  15. Satdinov R.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. Vozduhovody nizkogo davleniya iz PKM v letatelnyh apparatah [РСМ low-pressure air ducts in aircraft] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8. St. 08. Available at: http://www.viam-works.ru (accessed: November 17, 2017). DOI: 10.18577/2307-6046-2016-0-8-8-8.
  16. Satdinov R.A., Istyagin S.E., Veshkin E.A. Analiz temperaturno-vremennyh parametrov rezhimov otverzhdeniya PKM s zadannymi harakteristikami [Analysis of the temperature-time parameters mode curing PCM with specified characteristics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №3. St. 09. Available at: http://www.viam-works.ru (accessed: November 17, 2017). DOI: 10.18577/2307-6046-2017-0-3-9-9.
  17. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2016. №2. St. 07. Available at: http://www.viam-works.ru (accessed: November 17, 2017). DOI 10.1857/2307-6046-2016-0-2-7-7
  18. Postnov V.I., Strelnikov S.V., Makrushin K.V., Veshkin E.A. Semipreg dlya polimernyh osnastok [Semipreg for polymeric equipments] // Sistemy upravleniya zhiznennym ciklom izdelij aviacionnoj tehniki: aktualnye problemy, issledovaniya, opyt vnedreniya i perspektivy razvitiya: tez. dokl. V Mezhdunar. nauch.-praktich. konf. Ulyanovsk, 2016. S. 186–188.
  19. Satdinov R.A., Veshkin E.A., Postnov V.I., Abramov P.A. Rol antiadgezionnyh pokrytij v tehnologicheskom processe formovaniya PKM [The role of anti-adhesive coatings in the technological process of PCM molding] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4 (40). St. 10. Available at: http://www.viam-works.ru (accessed: November 17, 2017). DOI: 10.18577/2307-6046-2016-0-4-10-10.