Researches of the technological properties of metal-powder compositions of VT6 and VT20 titanium alloys obtained by induction melting and gas atomization

Knyazev A. E., Nerush S.V., Alishin M.I., Kuko I.S.
Knyazev A. E., Nerush S.V., Alishin M.I., Kuko I.S. Researches of the technological properties of metal-powder compositions of VT6 and VT20 titanium alloys obtained by induction melting and gas atomization // Proceedings of VIAM. 2017. No. 11. DOI: 10.18577/2307-6046-2017-0-11-6-6. URL: https://viam-works.ru/en/journal/2017/11/6
Keywords
metal-powder compositions, titanium alloys VT6 and VT20, technological properties, induction melting, gas atomization.
Abstract

This article presents the researches of the technological properties of metal-powder compositions of VT6 and VT20 titanium alloys obtained by induction melting and gas atomization. Researches of chemical composition, gas porosity, surface morphology and other technological properties of metal-powder compositions of VT6 and VT20 titanium alloys were conducted. Work is performed within development of technology of receiving the fine-dispersed of metal-powder compositions of VT6 and VT20 titanium alloys for enhancing of their use in the additive technologies.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
  4. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  5. Kablov E.N. Materialy i tehnologii VIAM v konstrukciyah perspektivnyh dvigatelej razrabotki OAO «Aviadvigatel» [Materials and VIAM technologies in designs of perspective engines of development of JSC Aviadvigatel] // Permskie aviacionnye dvigateli: inform. byul. 2014. №31. S. 43–47.
  6. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  7. Inozemcev A.A., Bashkatov I.G., Koryavcev A.S. Titanovye splavy v izdeliyah razrabotki OAO «Aviadvigatel» [Titanium alloys in products of development of JSC «Aviadvigatel»] // Sovremennye titanovye splavy i problemy ih razvitiya. M.: VIAM, 2010. S. 43–46.
  8. Magerramova L.A., Nozhnickij Yu.A., Vasilev B.E., Kinzburskij B.C. Primenenie additivnyh tehnologij dlya izgotovleniya detalej perspektivnyh gazoturbinnyh dvigatelej [Application of the additive technologies for manufacturing of details of perspective gas turbine engines] // Tehnologiya legkih splavov. 2015. №4. S. 7–13.
  9. Zlenko M.A., Nagajcev M.V., Dovbysh V.M. Additivnye tehnologii v mashinostroenii. Posobie dlya inzhenerov [The additive technologies in mechanical engineering]. M.: NAMI, 2015. S. 34–44.
  10. Shejhaliev Sh.M., Shemyakina O.A. Novosti poroshkovoj metallurgii. NETRAMM i RST [News of powder metallurgy. NETRAMM and RST] // Zhurnal Vesna. 2016. №6. S. 1–4.
  11. Дудихин Д.В., Сапрыкин А.А. Способы получения сферических порошков для аддитивных лазерных технологий [Ways of receiving spherical powders for the additive laser technologies] // MASTER’S JOURNAL. 2016. №1. С. 51–55.
  12. Mancevich N.M. Issledovatelskaya baza polucheniya metallicheskih poroshkov dlya additivnyh tehnologij [Research base of receiving metal powders for the additive technologies]. M.: ATOMJeKSPO, 2015. C. 6–8.
  13. Dovbysh V. M., Zabednov P.V., Zlenko M.A. Additivnye tehnologii i izdeliya iz metalla [The additive technologies and metal wares]. M.: NAMI, 2015. S. 29–31.
  14. Gu D.D., Meiners W., Meiners W., Wissenbach K., Poprawe R. Laser Additive Manufacturing of Metallic Components: Materials, Processes, and Mechanisms // International Materials Reviews. 2012. Vol. 57. P. 137–164.
  15. ASTM B213. Standard Test Methods for Flow Rate of Metal Powders Using the Hall Flowmeter Funnel.
  16. Knjazev A.E. Proizvodstvo granul titanovogo splava Ti–6Al–4V [Production of granules of Ti-6Al-4V titanium alloy] // Tehnologiya legkih splavov. 2010. №4. S. 46–48.