Preparation of carbon fibers to interphase coating deposition for ceramic matrix composites
Valueva M.I., Zelenina I.V., Khaskov M.A., Gulyaev A.I. Preparation of carbon fibers to interphase coating deposition for ceramic matrix composites // Proceedings of VIAM. 2017. No. 10. DOI: 10.18577/2307-6046-2017-0-10-9-9. URL: https://viam-works.ru/en/journal/2017/10/9
Keywords
reinforced fillers, carbon fiber, surface coating, surface coating removal, interphase coating, ceramic matrix composite.
Abstract
The comparative results of surface coating removal from the carbon fiber, which determine the efficiency of interphase coating deposition and ceramic matrix composite manufacturing, are discussed. The physical-chemical and thermal analysis, tensile strength measurements and microstructure of carbon fillers with surface coating and after its removal were carried out. It was shown, that the most optimal method from technological point of view is the surface coating removal by annealing of carbon fiber at static air atmosphere at 400°С.
Reference list
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. inform. materialov. 3-e izd., pererab. i dop. [Tendencies and reference points of innovative development of Russia: collection of information materials. 3rd ed., rev. and add.]. M.: VIAM, 2015. 720 s.
- Haskov M.A., Shestakov A.M., Sorokin O.Yu., Gulyaev A.I., Davydova E.A., Sulyanova E.A., Sinyakov S.D. Termoanaliticheskie issledovaniya formirovaniya interfaznogo pokrytiya na osnove sistem polikarbosilan–oligosilazan–Rolivsan [Thermoanalytical researches of forming of interphase covering on the basis of systems polycarbosilane-oligoclase-Rolivsan] // Tez. dokl. III Vseros. nauch.-tehnich. konf. «Materialy i tehnologii novogo pokoleniya dlya perspektivnyh izdelij aviacionnoj i kosmicheskoj tehniki» (Moskva, 17 iyulya 2017 g.). M.: VIAM, 2017. S. 1–14. Available at: https://conf.viam.ru/conf/250/proceedings (accessed: September 10, 2017).
- Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
- Sorokin O.Yu. K voprosu o mehanizme vzaimodejstviya uglerodnyh materialov s kremniem (obzor) [On the issue of the mechanism of interaction between carbon materials and Si melt (review)] //Aviacionnye materialy i tehnologii. 2015. №1. S. 65–70. DOI: 10.18577/2071-9140-2015-0-1-65-70.
- Lebedeva Yu.E., Popovich N.V., Orlova L.A. Zashhitnye vysokotemperaturnye pokrytiya dlya kompozicionnyh materialov na osnove SiC [Protective high temperature coatings for composite materials on the basis of SiC] // Trudy VIAM: elektron. nauch.-tehnich. zhurnal. 2013. №2. St. 06. Available at: http://www.viam-works.ru (accessed: August 01, 2017).
- Meleshko A.I., Polovnikov S.P. Uglerod, uglerodnye volokna, uglerodnye kompozity [Carbon, carbon fibers, carbon composites]. M.: SAJNS-PRESS, 2007. 192 s.
- Baklanova N.I. Interfejsnye pokrytiya na armiruyushhih uglerodnyh i karbidokremnievyh voloknah dlya kompozitov s keramicheskoj matricej: avtoref. dis. ... dokt. him. nauk [The interface coverings on reinforcing carbon and carborundum fibers for composites with ceramic matrix: thesis, Dr. Sci. (Tech.)]. Novosibirsk, 2010. 40 s.
- Tkachenko L.A., Shaulov A.Yu., Berlin A.A. Zashhitnye zharoprochnye pokrytiya uglerodnyh materialov // Neorganicheskie materialy. 2012. T. 48. №3. S. 261–271.
- Zajcev B.N., Baklanova N.I., Zima T.M. Issledovanie metodom atomno-silovoj mikroskopii poverhnostno-modificirovannyh uglerodnyh volokon [Research by method of nuclear and power microscopy of the surface modified carbon fibers] // Neorganicheskie materialy. 2008. T. 44. №6. S. 682–688.
- Baklanova N.I., Zima T.M., Utkin A.V., Titov A.T. Mikrostrukturnye osobennosti
- TaC-pokrytij na uglerodnyh voloknah [Microstructural features of TaC-coatings on carbon fibers]// Neorganicheskie materialy. 2011. T. 47. №7. S. 812–817.
- Utkin A.V., Matvienko A.A., Titov A.T., Baklanova N.I. Formirovanie i issledovanie mnogoslojnogo ZrO2-pokrytiya na karbidokremnievyh voloknah dlya SiC/SiC-kompozitov [Forming and research of multi-layer ZrO2-covering on carborundum fibers for SiC/SiC-composites] // Neorganicheskie materialy. 2011. T. 47. №10. S. 1176–1181.
- Uglerodnye volokna / pod red. S.M. Simamury [Carbon fibers / ed. by S.M. Simamura]. M.: Mir, 1987. 304 s.
- Morgan P. Carbon fibers and their composites. USA: CRC Press, 2005. 1131 p.
- Kondrashova I.A., Cheblakova E.G., Evteeva E.E. Obrabotka uglerodnogo volokna dlya dalnejshej ekspluatacii v tehnologicheskih processah [Processing of carbon fiber for further operation in technological processes] // Evrazijskij Soyuz Uchenyh (ESU). Tehnicheskie nauki. 2015. №3 (12). S. 36–38.
- Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Park S.-J. Carbon Fiber. Korea: Springer, 2015. 330 p.
- Available at: https://www.tohotenax.com/ru/produkci%d1%8f/uglerodn%d1%8be-volokna-tenax%c2%ae/zzgut%d1%8b-tenax%c2%ae/ (accessed: September 10, 2017).
- Cuj Syuj, Guseva R.I., Li Vej, Chzhan Linyuni, Gao Yuj. Analiz sostoyaniya poverhnosti vysokoprochnyh kompozicionnyh materialov s uglerodnym voloknom i issledovanie ih mehanicheskih harakteristik [The analysis of surface condition of high-strength composite materials with carbon fiber and research of their mechanical characteristics] // Uchenye zapiski Komsomol'skogo-na-Amure gosudarstvennogo tehnicheskogo universiteta. 2011. №IV-1 (8). S. 4–8.
- Urvanov S.A. Modificirovanie uglerodnogo volokna uglerodnymi nanostrukturami: avtoref. dis. ... kand. him. nauk [Modifying of carbon fiber by carbon nanostructures: thesis, PhD (Tech.)]. M., 2016. 20 s.
- Kern F., Gadow R. Liquid phase process for protective ceramic layers on carbon fibers // Surface and Coatings Technology. 2002. Vol. 151–152. P. 418–423.
- Available at: http://rus-carbon.ru/main/catalog/CarbonTk.aspx (accessed: September 10, 2017).
- Orlov M.R. Strategicheskie napravleniya razvitiya Ispytatelnogo centra FGUP «VIAM» [Strategic directions of development of the Test center FSUE «VIAM»] // Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
- Erasov V.S. Vizualizaciya processov ispytaniya i eksperimentalnyh dannyh v 3D-prostranstve [Visualization of mechanical testing processes and experimental data processing via 3D-presentation] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 22–28. DOI: 10.18577/2071-9140-2014-0-s4-22-28.
- Gulyaev A.I., Shurtakov S.V. Kolichestvennyj analiz mikrostruktury granichnogo sloya «volokno–matrica» v ugleplastikah [Quantitative analysis of fiber–matrix interface microstructure in carbon composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurnal. 2016. №7. St. 08. Available at: http://www.viam-works.ru (accessed: August 01, 2017). DOI: 10.18577/2307-6046-2016-0-7-8-8.
- Nefedov N.I., Haskov M.A., Petrova A.P., Buznik V.M. Issledovanie termicheskih svojstv ftorparafinov i gidrofobnyh pokrytij na ih osnove [Study of the thermal properties of fluorinated paraffins and hydrophobic coatings on their base] // Trudy VIAM: elektron. nauch.-tehnich. zhurnal. 2017. №2. St. 11. Available at: http://www.viam-works.ru (accessed: September 11, 2017). DOI: 10.18577/2307-6046-2017-0-2-11-11.
- Kablov E.N. Materialy – osnova lyubogo dela [Materials are the base of any business] // Delovaya slava Rossii. 2013. №2 (40). S. 4–9.
- Kablov E.N. Materialy novogo pokoleniya [Materials of new generation] // Zashhita i bezopasnost. 2014. №4. S. 28–29.
- Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.