Heat-resistant putties on base silicone resins

Kondrashov E.K.
Kondrashov E.K. Heat-resistant putties on base silicone resins // Proceedings of VIAM. 2017. No. 10. DOI: 10.18577/2307-6046-2017-0-10-7-7. URL: https://viam-works.ru/en/journal/2017/10/7
Keywords
putty, heat resistance, internal stress, coating viscosity.
Abstract

The comparative rate analysis of thermo-oxidative destruction of the film-forming agent of various nature is carried out and necessity of applying polyorganosiloxanes for the development of heat-resistant putties is proved. The choice of the inorganic heat-resistant fillers providing the minimum internal stresses in coatings with putties taking into account influence of fillers on the rate of thermo-oxidative destruction polyorganosiloxanes is reasonable. Results of assessment of technological, physic-mechanical, rheological and dielectric properties of KO-0035, KO-0066, KO-0067, KO-0070 putties, and also their heat resistance when heating in isothermal conditions and in gas-dynamic flow are given.

Reference list
  1. Kondrashov E.K., Semenova L.V. Termostojkie lakokrasochnye pokrytiya [Heat-resistant paint coatings] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 316–322.
  2. Kondrashov E.K., Semenova L.V. Termookislitelnaya stabilnost nenapolnennyh i dispersno-napolnennyh polimernyh plenkoobrazuyushhih [Thermooxidizing stability of the unfilled and disperse filled polymeric film-forming] // Aviacionnye materialy i tehnologii. 2003. Vyp.: Lakokrasochnye materialy i pokrytiya. S. 36–41.
  3. Semenova L.V. Termostojkaya emal VE-63 [Heat-resistant VE-63 enamel] // Aviacionnye materialy i tehnologii. 2003. Vyp.: Lakokrasochnye materialy i pokrytiya. S. 41–44.
  4. Kondrashov E.K., Kuznecova V.A., Lebedeva T.A., Malova N.E. Antikorrozionnye, termoreguliruyushhie, termostojkie i vlagozashhitnye pokrytiya MKS «Buran» [Anticorrosion, temperature-controlled, heat-resistant and vlagozashchitny coatings of ISS «Buran»] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 137–141.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevostyanov V.G. Vysokotemperaturnye konstrukcionnye kompozicionnye materialy na osnove stekla i keramiki dlya perspektivnyh izdelij aviacionnoj tehniki [High-temperature constructional composite materials on the basis of glass and ceramics for perspective products of aviation engineering] // Steklo i keramika. 2012. №4. S. 7–11.
  7. Sanzharovskij A.T. Fiziko-mehanicheskie svojstva polimernyh i lakokrasochnyh pokrytij [Physicomechanical properties of polymer and paint coatings]. M.: Himiya, 1975. 264 s.
  8. Kondrashov E.K., Vladimirskij V.N., Bejder E.Ya. Erozionnostojkie lakokrasochnye pokrytiya [Erosion resistance paint coatings]. M.: Himiya, 1989. 136 s.
  9. Chebotarevskij V.V., Kondrashov E.K. Tehnologiya lakokrasochnyh pokrytij v mashinostroenii [Technology of paint coatings in mechanical engineering]. M.: Mashinostroenie, 1978. 296 s.
  10. Kiselev F.F., Krylov S.V. Adsorbcionnye processy na poverhnosti poluprovodnikov i dielektrikov. M.: Nauka, 1978. 255 s.
  11. Roginskij S.Z. Elektronnye yavleniya v geterogennom katalize [The electronic phenomena in heterogeneous catalysis]. M.: Nauka, 1975. 270 s.
  12. Golenko Yu.V., Kondrashov E.K., Starina A.I. Opredelenie reologicheskih svojstv pokrytiya emali FP-5105 [Definition of rheological properties of covering of FP-5105 enamel] // Oboronnaya tehnika. 1977. №7. S. 73–74.
  13. Golenko Yu.V., Kondrashov E.K., Starina A.I. Issledovanie reologicheskih svojstv lakokrasochnyh pokrytij pri realno dejstvuyushhih nagruzkah [Research of rheological properties of paint coatings at really actual loads] // Aviacionnaya promyshlennost. 1977. №5. S. 27–28.
  14. Buznik V.M., Kablov E.N., Koshurina A.A. Materialy dlya slozhnyh tehnicheskih ustrojstv arkticheskogo primeneniya [Materials for difficult engineering devices of the Arctic application] // Nauchno-tehnicheskie problemy osvoeniya Arktiki. M.: Nauka, 2015. S. 275–285.
  15. Kondrashov E.K., Malovа N.E. Lakokrasochnye pokrytiya na osnove sopolimerov triftorhloryetilena [Paint coatings based on copolymers of trifluorochloroethylene] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 39–44. DOI: 10.18577/2071-9140-2015-0-2-39-44.
  16. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti i ekspluatacii aviacionnoj tehniki [Quality control of materials is a security accreditation and operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.