Changes in the surface properties of titanium alloy VT20 in the chemical removal of operational carbon pollution

Nochovnaya N.A., Nikitin Ya.Yu., Grigorenko V.B., Kozlov I.A.
Nochovnaya N.A., Nikitin Ya.Yu., Grigorenko V.B., Kozlov I.A. Changes in the surface properties of titanium alloy VT20 in the chemical removal of operational carbon pollution // Proceedings of VIAM. 2017. No. 10. DOI: 10.18577/2307-6046-2017-0-10-5-5. URL: https://viam-works.ru/en/journal/2017/10/5
Keywords
chemical cleaning, operational pollution, carbon polution, surface properties, titanium alloy.
Abstract

For the first time investigated the influence of foreign and domestic chemical technologies removal of operational carbon pollution on the complex properties of the surface of the heat-resistant titanium alloy VT20. Visually, the gravimetric method, and using scanning electron microscopy and X-ray microanalysis of samples evaluated cleaning performance against carbon polution. The change in surface roughness, microhardness and surface activity of purified samples. It is established that when cleaning samples from carbon pollution chemically, an increase in the microhardness and a reduction in surface activity may occur, as compared to those for the initial samples. By its technological characteristics VPr16 solder picked possibility of reconditioning by soldering after the removal of carbon polution from the surface of titanium alloy VT20 chemical means.

Reference list
  1. Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Sostoyanie, problemy i perspektivy sozdaniya zharoprochnyh titanovyh splavov dlya detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 02. Available at: http://www.viam-works.ru (accessed: September 01, 2017).
  2. Shiryaev A.A., Nochovnaya N.A. Issledovanie struktury i himicheskogo sostava slitkov opytnogo vysokolegirovannogo titanovogo splava [Study of structure and chemical composition of pilot high-alloyed titanium alloy ingots] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 06. Available at: http://www.viam-works.ru (accessed: September 01, 2017). DOI: 10.18577/2307-6046-2015-0-9-6-6
  3. Alekseev E.B., Nochovnaya N.A., Panin P.V., Novak A.V. Tehnologicheskaya plastichnost, struktura i fazovyj sostav opytnogo titanovogo orto-splava, soderzhashhego 13% (po masse) alyuminiya [Technological plasticity, structure and phase composition of a pilot titanium ortho alloy with 13 wt. рct. aluminum] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 08. Available at: http://www.viam-works.ru (accessed: September 01, 2017). DOI: 10.18577/2307-6046-2015-0-12-8-8.
  4. Nochovnaia N.A., Panin P.V., Kochetkov A.S., Bokov K.A. Opyt VIAM v oblasti razrabotki i issledovaniia ekonomnolegirovannykh titanovykh splavov novogo pokoleniia [VIAM experience in the field of development and research of economically alloyed titanium alloys of new generation] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №9 (45). St. 05. Available at: http://www.viam-works.ru (accessed: September 01, 2017). DOI: 10.18577/2307-6046-2014-0-9-5-5.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N. Materialy kak osnova bezopasnosti [Materials as the base of safety] // Industriya. 2014. №16. S. 1–2.
  7. Kablov E.N. Chtoby sobrat samolet po atomam [To collect airplane on atoms] // Industriya. Inzhenernaya gazeta. 2015. №12. S. 1–2.
  8. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstrukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  9. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific and technical information. 3rd ed.]. M.: VIAM, 2015. 720 s.
  10. Huadong Y., Hong X. The Effect of Surface Roughness on Thermodynamic Performance Parameter of Axial Flow Compressor // Research Journal of Applied Sciences, Engineering and Technology. 2013. No. 5 (18). P. 4458–4463.
  11. Stepankov I.A. Kompleksnoe reshenie dlya ochistki kompressorov GTU: ochistitel Turbo-K i antifriz AF10 [The complex decision for cleaning of GTU compressors: cleaner of Turbo-K and AF10 antifreeze] // Turbiny i dizeli. 2015. №1. S. 54–55. Available at: http://www.turbine_diesel.ru (accessed: September 01, 2017).
  12. Malcev E.N. Razrabotka obobshhennogo metoda rascheta i proektirovaniya sistemy vlazhnoj ochistki protochnoj chasti GTD i sredstv ee realizacii: avtoref. dis. … kand. tehn. nauk [Development of the generalized method of calculation and design of system of wet cleaning of flowing part of GTD and means of its implementation: thesis, PhD (Tech.)]. Samara, 2013. 20 s.
  13. Docenko G.N. Razrabotka principov ochistki detalej aviacionnoj tehniki ot nagaropodobnyh zagryaznenij biotehnologicheskim metodom: avtoref. dis. … kand. tehn. nauk [Development of principles of cleaning of details of aviation engineering from nagaropodobny pollution by biotechnological method: thesis, PhD (Tech.)]. M., 2000. 37 s.
  14. Shulov V.A., Bycenko O.A., Teryaev D.A. i dr. Razrabotka tehnologicheskogo processa vosstanovleniya svojstv lopatok kompressora GTD iz zharoprochnoj stali EP866-Sh s primeneniem silnotochnyh impul'snyh elektronnyh puchkov [Development of technological process of recovery of properties of compressor blades of GTD from heat resisting EP866-Sh steel using high-current pulse electronic bunches] // Vzaimodejstvie izluchenij s tverdym telom: mater. 8-j Mezhdunar. konf. Minsk, 2009. S. 360–362.
  15. Enyia J.D., Li Y., Thank-God I., Igbong D.I. Industrial Gas Turbine On-line Compressor Washing for Power Generation. // Isaiah International Journal of Engineering Research and Technology. 2015. Vol. 4. Issue 08. P. 500–506.
  16. Kurz R., Brun K., Mokhatab S. Gas turbine compressor blade fouling mechanisms // Pipeline & Gas Journal. 2011. Vol. 238. No. 9 . P. 18–21.
  17. Maiwada B., Muaz N.I., Ibrahim S., Musa S.M. Impacts of Compressor Fouling On the Performance of Gas Turbine // International Journal of Engineering Science and Computing. 2016. Vol. 6. Issue 3. P. 2118–2125.