Manufacturing of CFRP test samples with different porosity for its evaluation by non-destructive testing

Boychuk A.S., Chertishchev V.Yu., Dikov I.A.
Boychuk A.S., Chertishchev V.Yu., Dikov I.A. Manufacturing of CFRP test samples with different porosity for its evaluation by non-destructive testing // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-11-11. URL: https://viam-works.ru/en/journal/2017/1/11
Keywords
porosity, autoclave molding, infusion.
Abstract

Test of ways of obtaining special CFRP specimens with different porosity by autoclave molding and infusion method are observed in this paper. For infusion method these results were obtained by low compression, air pumping-in to binder, lower binder input and addition of pore-forming agent. For autoclave molding these results were obtained without external pressure and molding at heat chamber with vacuum slide into the bag to 0,03–0,05 at.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M., 2002. S. 23–47.
  3. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  4. Merkulova Yu.I., Muhametov R.R. Nizkovyazkoe epoksidnoe svyazuyushhee dlya pererabotki metodom vakuumnoj infuzii [Development of a low-viscosity epoxy binder for processing by vacuum infusion] // Aviacionnye materialy i tehnologii. 2014. №1. S. 39–41. DOI: 10.18577/2071-9140-2014-0-1-39-41.
  5. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  6. Dushin M.I., Hrulkov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Out-of-autoclave formation carbon plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  7. Lin L., Luo M., Tian H.T., Li X.M., Guo G.P. Experimental investigation on porosity of carbon fiber-reinforced composite using ultrasonic attenuation coefficient // 17th World Conference on Nondestructive Testing. Shanghai, China. October 25–28, 2008. Available at: http://www.ndt.net/article/ wcndt2008/papers/222.pdf (accessed: June 11, 2016).
  8. Daniel I.M., Wooh S.C., Komsky I. Quantitative Porosity Characterization of Composite Materials by Means of Ultrasonic Attenuation Measurements // Journal of Nondestructive, Evaluation. 1992. Vol. 1L. No. L. Available at: http://link.springer.com/article/10.1007/BF00566012 (дата обращения: 11.07.2016).
  9. Ding S., Jin S., Luo Z., Liu H., Chen J., Lin L. Investigations on relationship between porosity and ultrasonic attenuation efficient in CFRP laminates based on RMVM // 7th International Symposium on NDT in Aerospace. Мo.5.A.1. Available at: https://www.ndt-aerospace.com/Portals/aerospace2015/BB/mo5a1.pdf (accessed: June 11, 2016).
  10. Dominguez N., Mascaro B. Ultrasonic Non-Destructive Inspection of Localised Porosity in Composite Materials // ECNDT. 2006. Tu.2.1.4. Available at: https://www.ndt-aerospace.com/Portals/aerospace2015/BB/mo5a1.pdf (accessed: June 11, 2016).
  11. Hillger W., Elze S. Determination of porosity in aerospace structures by ultrasonic pulse echo technique // 8 th ECNDT. Barcelona. 2002. Available at: http://www.dlr.de/fa/Portaldata/17/Resources/dokumente/institut/2002/u2002_2.pdf (accessed: June 11, 2016).
  12. Bojchuk A.S. Nerazrushayushhij kontrol detalej i konstrukcij aviacionnoj tehniki iz polimernyh kompozicionnyh materialov pri ispolzovanii ultrazvukovyh fazirovannyh reshetok [Non-destructive testing of details and designs of aviation engineering from polymeric composite materials when using the ultrasonic phased grids] // Tez. dokl. 19-j Vseros. nauch.-tehnich. konf. po nerazrushayushhemu kontrolyu i tehnicheskoj diagnostike. Samara, 2011. S. 289–291.
  13. Bojchuk A.S., Generalov A.S., Dalin M.A., Stepanov A.V. Kontrol tehnologicheskih i ekspluatacionnyh narushenij sploshnosti ploskih panelej iz polimernyh kompozicionnyh materialov pri ispolzovanii ultrazvukovyh fazirovannyh reshetok [Control of technological and operating disturbances of continuity of flat panels from polymeric composite materials when using the ultrasonic phased grids] // Tez. dokl. Vseros. konferencii po ispytaniyam i issledovaniyam materialov «TestMat 2012». M.: VIAM, 2012. S. 6.
  14. Bojchuk A.S., Generalov A.S., Stepanov A.V. Yuhackova O.V. Nerazrushayushhij kontrol PKM s ispolzovaniem ultrazvukovyh fazirovannyh reshetok [Non-destructive testing of PKM with use of the ultrasonic phased grids] // Promyshlennye ASU i kontrollery. 2013. №2. S. 54–58.
  15. Boychuk A.S., Stepanov A.V, Kosarina E.I., Generalov A.S. Primenenie tehnologii ultrazvukovyh fazirovannyh reshetok v nerazrushayushhem kontrole detalej i konstrukcij aviacionnoj tehniki, izgotavlivaemyh iz PKM [Application of ultrasonic phased lattice technique for nondestructive testing of aviation FRP parts structures] // Aviacionnye materialy i tehnologii. 2013. №2. S. 41–46.