Research of the process of extrusion of continuous high-melting fibers
Zimichev A.M., Varrik N.M., Sumin А.V. Research of the process of extrusion of continuous high-melting fibers // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-6-6. URL: https://viam-works.ru/en/journal/2017/1/6
Keywords
aluminum oxide, sol-gel method, continuous fiber.
Abstract
The ceramic fibers are priority subject to develop for their use as a main component of heat-shielding and heat-insulating materials for high-temperature purpose. This work investigates features of the process of formation of continuous alumina fiber by sol-gel method and also formation of inclusions in high-density fiberizing solutions during evaporation. It is established that existence of the second liquid phase in forming solution can interfere with the formation process.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
- Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
- Savenkova A.V., Chursova L.V., Eliseev O.A., Glazov P.A. Germetiki aviacionnogo naznacheniya [Hermetics of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 40–43.
- Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: May 16, 2016).
- Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova [Armor for «Buran». Materials and VIAM technologies for ISS of «Energiya–Buran» / gen. ed. by E.N. Kablov]. M.: Nauka i zhizn, 2013. 128 s.
- Kablov E.N., Shhetanov B.V. Voloknistye teploizolyacionnye i teplozashhitnye materialy: svojstva, oblasti primeneniya [Fibrous heatinsulating and heat-protective materials: properties, scopes] // Fundamentalnye problemy vysokoskorostnyh techenij: sb. tez. dokl. Mezhdunar. nauch.-tehnich. konf. Zhukovskij, 2004. S. 95–96.
- Overhead high power transmission cable comprising fiber reinforced aluminum matrix composite wire: pat. 6180232 US; publ. 30.01. 01. 13 p.
- Ruggles-Wrenn M.B., Szymczak N.R. Effect of Steam Environment on Compressive Creep Behavior of Nextel 720/alumina Ceramic Composite at 1200°C // Сomposites: Part A. 2008. Vol. 39. P. 1829–1837.
- Methods of producing a ceramic matrix composite: pat. 7153379 US; publ. 26.12.06. 7 p.
- Varrik N.M., Ivahnenko Yu.A., Maksimov V.G. Oksid-oksidnye kompozicionnye materialy dlya gazoturbinnyh dvigatelej (obzor) [Oxide-oxide composites for gas-turbine engines (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 03. Available at: http://www.viam-works.ru (accessed: October 16, 2016). DOI: 10.18577/2307-6046-2014-0-8-3-3.
- Balinova Yu.A., Kirienko T.A., Zimichev A.M. Reologiya vodnyh rastvorov sistemy «oksihlorid alyuminiya–polivinilovyj spirt», modificirovannyh bornoj kislotoj i ee solyami dlya keramicheskih voloknistyh materialov [Rheology of aqueous solutions of system « aluminum oxychloride -polyvinyl alcohol», modified by boric acid and its salts for ceramic fibrous materials] // Ogneupory i tehnicheskaya keramika. 2012. №11–12. S. 24–26.
- Kirienko T.A., Balinova Yu.A. Fiziko-himicheskie svojstva mnogokomponentnyh rastvorov dlya keramicheskih materialov, soderzhashhih polivinilovyj spirt [Physical and chemical properties of multicomponent solutions for ceramic materials containing polyvinyl alcohol] // Aviacionnye materialy i tehnologii. 2014. №1. S. 34–38. DOI: 10.18577/2071-9140-2014-0-1-34-38.
- Kirienko T.A., Balinova Yu.A. Vliyanie atmosfernoj vlazhnosti na reologiju tonkih sloev koncentrirovannyh vodnyh rastvorov sistemy «neorganicheskie soli–organicheskij polimer» [Influence of atmospheric humidity on a rheology of thin layers of the concentrated water solutions of system «inorganic salts–organic polymer»] // Aviacionnye materialy i tehnologii. 2014. №2. S. 56–58. DOI: 10.18577/2071-9140-2014-0-2-56-58.
- Zimichev A.M., Varrik N.M., Sumin A.V. Niti iz tugoplavkih oksidov dlya uplotnitelnoj teploizolyacii [Threads of refractory oxides for sealing thermal insulation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 05. Available at: http://www.viam-works.ru (accessed: October 16, 2016). DOI: 10.18577/2307-6046-2015-0-6-5-5.