Aspects of mechanical properties of metal matrix composites reinforced with continuous unidirectional fibers (review)
UDC
669.018.95:621.775.8
DOI
10.18577/2307-6046-2017-0-1-5-5
Article PDF (Russian)
(581.46 KB)
How to cite
Grishina O.I., Serpova V.M. Aspects of mechanical properties of metal matrix composites reinforced with continuous unidirectional fibers (review) // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-5-5. URL: https://viam-works.ru/en/journal/2017/1/5
Keywords
metal matrix composites, continuous fibers, mechanical properties, control methods.
Abstract
Control of elastic-plastic behavior of metal matrix composites reinforced with continuous fibers is the most important task of defining performance of both material and structural elements. The paper discusses methods of control, which together provide a complete understanding of fracture mechanism, strength and elastic characteristics of the metal matrix composites reinforced with continuous unidirectional fibers. It is shown that the behavior of material when applying the load specifically depends on technological defects arising during manufacture.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N. Razrabotki VIAM dlya gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
- Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-loaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. 2011. №SP2. S. 13–19.
- Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizatsii v resursosberegayushchej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 01. Available at: http://www.viam-works.ru (accessed: June 18, 2016).
- Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
- Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
- Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
- Vildeman V.E., Sokolkin Yu.V., Tashkinov A.A. Mehanika neuprugogo deformirovaniya i razrusheniya kompozicionnyh materialov [Mechanics of not elastic deformation and destruction of composite materials]. M.: Nauka–Fizmatlit, 1997. 288 s.
- Kristensen L.M. Vvedenie v mehaniku kompozitov [Introduction in mechanics of composites]. M.: Mir, 1982. 334 s.
- Brautman L., Krok R. Kompozicionnye materialy [Composite materials]. M.: Mir, 1978. T. 1: Poverhnosti razdela v metallicheskih kompozitah. 438 s.
- Zirconium Diffusion Barrier in Titanium-Silicon Carbide Composite Materials: pat. 3717443 US; publ. 20.02.73.
- Brautman L., Krok R. Kompozicionnye materialy [Composite materials]. M.: Mashinostroenie, 1978. T. 8: Analiz i proektirovanie konstrukcij. Ch. 2. 264 s.
- Tamuzh V.P., Tetere G.A. Problemy mehaniki kompozitnyh materialov [Problems of mechanics of composite materials] // Mehanika kompozitnyh materialov. 1979. №1. S. 34–45.
- Shaterina M.A. Tehnologiya konstrukcionnyh materialov [Technology of constructional materials]. M.: Politehnika, 2005. 597 s.