Alternation of structure of selective laser melted aluminum alloy AK9ch during heat treatment

Ryabov D.K., Zaysev D.V., Dynin N.V., Ivanova A.O.
Ryabov D.K., Zaysev D.V., Dynin N.V., Ivanova A.O. Alternation of structure of selective laser melted aluminum alloy AK9ch during heat treatment // Proceedings of VIAM. 2016. No. 9. DOI: 10.18577/2307-6046-2016-0-9-3-3. URL: https://viam-works.ru/en/journal/2016/9/3
Keywords
AK9ch alloy, SLM, heat treatment, additive manufacturing.
Abstract

Development of 3D-printing technologies made it possible to prepare half-finished product and components from metal powders including those from aluminum alloys. These technologies allow procuring complex products with high improved material efficiency. However the high crystallization speed during selective laser sintering causes manufacture of structures that are not typical for classical casting technologies. The research results of the microstructure changes of AK9ch material during various kinds of heat treatment (annealing, solution treatment), the results of the optical microscopy and TEM studies are introduced. The work is carried out under the realization of integrated research area 10.3. «Technologies of atomization for producing high quality metallic powders for additive manufacturing and powders for brazing» («The strategic directions of development of materials and technologies for their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: March 01, 2016).
  5. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. Issledovanie svojstv splava EP648, poluchennogo metodom selektivnogo lazernogo splavleniya metallicheskih poroshkov [A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 02. Available at: http://www.viam-works.ru (accessed: July 19, 2016). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  6. Thijs L., Kempen K., Kruth J.-P., Van Humbeeck J. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder // Acta Mater. 2013. Vol. 61. P. 1809–1819.
  7. Bremen S., Meiners W., Diatlov A. Selective Laser Melting // Laser Technik Journal. 2012. No. 9 (2). P. 33–38.
  8. Sercombe T., Schaffer G. Rapid manufacturing of aluminum components // Science. 2003. Vol. 301 (5637). P. 1225–1227.
  9. Guan K., Wang Z.M., Gao M. et al. Effects of processing parameters on tensile properties of selective laser melted 304 stainless steel // Materials & Design. 2013. Vol. 50. P. 581–586.
  10. Illarionov E'.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tekhnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
  11. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  12. Buchbinder D. et al. Rapid Manufacturing of Aluminium Parts for serial Production via Selective Laser Melting // Proc. of International User’s Conference on Rapid Prototyping-Tooling & Manufacturing «Euro-uRapid 2007». Germany, Frankfurt/Main. Dec. 3–4, 2007.
  13. Read N., Wang W., Essa K. et al. Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development // Materials & Design. 2015. Vol. 65. P. 417–424.
  14. Ryabov D.K., Kolobnev N.I. Izmenenie mehanicheskih svojstv splava 1913 pri dvuhstupenchatom iskusstvennom starenii [Change of mechanical properties of alloy 1913 at two-level artificial aging] // Aviacionnye materialy i tehnologii. 2013. №4. S. 3–7.
  15. Kempen K., Thijs L., Van Humbeeck J., Kruth J.P. Mechanical Properties of AlSi10Mg Produced by Selective Laser Melting // Phys. Procedia. 2012. Vol. 39. P. 439–446.
  16. Manfredi D., Calignano F., Krishnan M. et al. From Powders to Dense Metal Parts: Characterization of a Commercial AlSiMg Alloy Processed through Direct Metal Laser Sintering // Materials. 2013. Vol. 6 (3). P. 856–869.
  17. Olakanmi E.O. Selective laser sintering/melting (SLS/SLM) of pure Al, Al–Mg, and Al–Si powders: Effect of processing conditions and powder properties // J. Mater. Process. Tech. 2013. Vol. 213. P. 1387–1405.18. Weingartena C. Formation and reduction of hydrogen porosity during selective lasermelting of AlSi10Mg // Journal of Materials Processing Technology. 2015. V. 221. P. 112–120.
  18. Weingartena C. Formation and reduction of hydrogen porosity during selective lasermelting of AlSi10Mg // Journal of Materials Processing Technology. 2015. Vol. 221. P. 112–120.
  19. Prashanth K.G., Scudino S., Klauss H.J. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment // Materials Science&Engineering A. 2014. V. 590. P. 153–160.