Gluing materials in the design of blades of helicopters

Lukina N.F., Dement’eva L.A., Petrova A.P., Anikhovskaya L.I.
Lukina N.F., Dement’eva L.A., Petrova A.P., Anikhovskaya L.I. Gluing materials in the design of blades of helicopters // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-7-7. URL: https://viam-works.ru/en/journal/2016/7/7
Keywords
highly elastic phenolic and rubber adhesives, high-strength epoxy adhesives, adhesive bond, adhesive binding, bond prepreg, composite material, fibreglass, mechanical characteristics.
Abstract

Application experience of highly elastic phenolic and rubber adhesives VK-3, VK-25, VK-50, liquid phenolic rubber adhesive VK-32-200B as glue intermediate layer and high-strength epoxy film adhesives VK-36P and VK-51 for blades manufacturing of main and tail helicopter propellers is shown. The main mechanical characteristics and purpose of adhesives are presented. Ways of development in the field of new adhesive materials application in helicopter equipment and technical efficiency in helicopters design are shown. The work is executed within implementation of the complex scientific direction 15.1. «Multifunction adhesive systems» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen ed. by E.N.Kablov]. M.: VIAM, 2012. 520 s.
  3. Batizat V.P., Anihovskaya L.I., Dementeva L.A. Klei dlya skleivaniya konstrukcij iz metallov i kompozicionnyh materialov [Glues for pasting of designs from metals and composite materials] // Aviacionnaya promyshlennost. 1983. №11. S. 15–17.
  4. Anihovskaya L.I., Petrova A.P., Batizat D.V. Vysokoelastichnyj plenochnyj klej VK-50 [Highly elastic film VK-50 glue] // Klei. Germetiki. Tehnologii. 2016 (v pechati).
  5. Karimova S.A., Pavlovskaya T.G., Petrova A.P. Podgotovka poverhnosti alyuminievyh splavov s primeneniem anodnogo oksidirovaniya [Surface preparation of aluminum alloys using anodic oxidation] // Klei. Germetiki. Tehnologii. 2014. №1. S. 34–38.
  6. Petrova A.P., Lukina N.F. Primenenie adgezionnyh gruntov i sistem modifikacii poverhnosti pri skleivanii [Application of adhesive soil and systems of updating of surface when pasting] // Klei. Germetiki. Tehnologii. 2013. №9. S. 24–28.
  7. Petrova A.P., Lukina N.F. Vliyanie adgezionnyh gruntov na resursnye harakteristiki kleevyh soedinenij [Influence of adhesive soil on resource characteristics of glued joints] // Klei. Germetiki. Tehnologii. 2015. №11. S. 20–23.
  8. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  9. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  10. Sharova I.A., Petrova A.P. Obzor po materialam mezhdunarodnoj konferencii po kleyam i germetikam (WAC-2012, Franciya) [Review of world adhesive and sealant conference (WAC-2012, France] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 06. Available at: http://www.viam-works.ru (accessed: January 25, 2016).
  11. Petrova A.P., Donskoj A.A., Chalyh A.E., Shherbina A.A. Kleyashhie materialy. Germetiki: spravochnik [Gluing materials. Hermetics: directory]. SPb.: Professional, 2008. S. 589.
  12. Lukina N.F., Dementeva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] // Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  13. Petrova A.P., Lukina N.F., Dementeva L.A., Avdonina I.A., Tyumeneva T.Yu., Zhadova N.S. Klei dlya aviacionnoj tehniki [Glues for aviation engineering] // RZhH. 2010. T. LIV. №1. C. 46–52.
  14. Kablov E.N., Minakov V.T., Anihovskaya L.I. Klei i materialy na ih osnove dlya remonta konstrukcij aviacionnoj tehniki [Glues and materials on their basis for repair of designs of aviation engineering] // Aviacionnye materialy i tehnologii. 2002. Vyp.: Remontnye tehnologii v aviastroenii. S. 61–65.
  15. Anihovskaya L.I., Minakov V.T. Klei i kleevye prepregi dlya perspektivnyh izdelij aviakosmicheskoj tehniki [Glues and glue prepregs for perspective products of aerospace equipment] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubilejnyj nauch.-tehnich. sb. M.: MISiS–VIAM, 2002. S. 315–326.
  16. Lukina N.F., Dementeva L.A., Petrova A.P., Tyumeneva T.Yu. Svojstva kleev i kleyashhih materialov dlya izdelij aviacionnoj tehniki [Properties of glues and gluing materials for products of aviation engineering] // Klei. Germetiki. Tehnologii. 2009. №1. S. 14–24.
  17. Dementeva L.A., Lukina N.F., Serezhenkov A.A., Kucevich K.E. Osnovnye svojstva i naznachenie PKM na osnove kleevyh prepregov [The main properties and PCM assignment on the basis of glue prepregs] // Konstrukcii i tehnologiya polucheniya izdelij iz nemetallicheskih materialov»: sb. tez. dokl. XIX Mezhdunarodnoj nauch.-tehnich. konf. / ONPP «Tehnologiya». Obninsk, 2010. S. 11–12.
  18. Lukina N.F., Dementeva L.A., Petrova A.P., Kirienko T.A., Chursova L.V. Kleevye svyazuyushhie dlya detalej iz PKM sotovoj konstrukcii [Glue binding for details from PKM of cellular design] // Klei. Germetiki. Tehnologii. 2016 (v pechati).
  19. Dementeva L.A., Serezhenkov A.A., Bocharova L.I., Anihovskaya L.I., Lukina N.F. Kompozicionnye materialy kleevye na osnove steklyannyh i uglerodnyh napolnitelej [Composite materials glue on the basis of glass and carbon fillers] // Klei. Germetiki. Tehnologii. 2009. №1. S. 24–27.
  20. Lukina N.F., Chursova L.V. Laboratoriya «Klei i kleevye prepregi» – dostizheniya i perspektivy [Laboratory «Glues and glue prepregs» – achievements and perspectives] // Kleyashhie materialy aviacionnogo naznacheniya: sb. dokl. konf. M.: VIAM, 2013. S. 1–5.
  21. Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Adhesive prepregs and layered materials on their basis] // Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
  22. Prepreg i izdelie, vypolnennoe iz nego: pat. 2427594 Ros. Federaciya [Prepreg and the product which has been executed of it: pat. 2427594 Rus. Federation]; opubl. 23.07.13.
  23. Lukina N.F., Dement’eva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidel’nikov V.V., Kutsevich K.E. Adhesive prepregs and composite materials on their basis // Russian Journal of General Chemistry. 2011. T. 81. №5. С. 1022–1024.
  24. Dementeva L.A., Serezhenkov A.A., Bocharova L.I., Lukina N.F., Kucevich K.E., Petrova A.P. Svojstva kompozicionnyh materialov na osnove kleevyh prepregov [Properties of composite materials on the basis of glue prepregs] // Klei. Germetiki. Tehnologii. 2012. №6. S. 19–24.
  25. Morozov B.B. Primenenie polimernyh kompozicionnyh materialov v izdeliyah razrabotki OKB Suhogo [Application of polymeric composite materials in products of development of Sukhoi Design Bureau] // Kleyashhie materialy aviacionnogo naznacheniya: sb. dokl. konf. M.: VIAM, 2013. S. 31–36.
  26. Hrychev Yu.I., Shkodinova E.P., Dementeva L.A. Razrabotka tehnologicheskogo processa izgotovleniya radioprozrachnogo obtekatelya iz kleevyh prepregov tipa KMKS-2m.120 [Development of technological process of manufacturing of radio transparent fairing from glue prepregs of the KMKS-2M.120 type] // Kleyashhie materialy aviacionnogo naznacheniya: sb. dokl. konf.. M.: VIAM, 2013. S. 43–47.