Identificationof the reasons of porosity formation when manufacturing compo-sites

Dushin M.I., Donetskiy K.I., Karavaev R.Y.
Dushin M.I., Donetskiy K.I., Karavaev R.Y. Identificationof the reasons of porosity formation when manufacturing compo-sites // Proceedings of VIAM. 2016. No. 6. DOI: 10.18577/2307-6046-2016-0-6-8-8. URL: https://viam-works.ru/en/journal/2016/6/8
Keywords
out-of-autoclave molding, infusion, moisture.
Abstract

It is known that porosity in polymeric composite materials (PCM) exerts a considerable impact on strength properties of the products working in the conditions of bending, compression and shearing load. Now in Federal state unitary enterprise «All-Russian scientific research institute of aviation materials» the works on creation of pore-free PCM produced by methods of autoclave and out-of-autoclave molding are conducted according to the strategic directions of development of materials and technologies of their processing for the period up to 2030 (13.2. «Structural PCM») [1]. The purpose of this work is the identification of main sources of porosity formation when manufacturing PCM by different methods. It is established on the tested flat samples collected from humidified prepregs molded in the autoclave or under vacuum that the main source of porosity formation is the moisture containing in binding and reinforcing fillers. Results of the study of feasibility of carbon plastics produ

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Mihajlin Yu.A. Konstrukcionnye polimernye kompozicionnye materialy [Constructional polymeric composite materials]. SPb.: Nauchnye osnovy i tehnologi. 2008. 822 s.
  3. Brautman L. Razrushenie i ustalost [Destruction and fatigue]. M.: Mir, 1978. 153 s.
  4. Void Content of Reinforced Plastic: ASTM D 2734-09. Standard by ASTM International. 2009. 3 p.
  5. Tavares S.S., Michaud V., Manson J.A.E. Through thickness air permeability of prepregs during cure // Composites: Part A. 2009. V. 40. P. 1587–1596.
  6. Thomas S., Nutt S.R. In situ estimation of though-thickness resin flow using ultrasound // Compos. Sci. Technol. 2008. 68:3093-8.
  7. Tavares S.S., Michaud V., Manson J.A.E. Assessment of semi-impregnated fabrics in honeycomb sandwich structures // Composites: Part A. 2010. V. 41. P. 8–15.
  8. Jackson K., Crabtree M. Autoclave guality composites tooling for composite from vacuum bag only processing // 47th International SAMPLE symposium. 2002. P. 800–807.
  9. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  10. Donetskij K.I., Kogan D.I., Hrulkov A.V. Svojstva polimernyh kompozicionnyh materialov, izgotovlennyh na osnove pletenyh preform [Properties of the polymeric composite materials made on the basis of braided preforms] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 05. Available at: http://www.viam-works.ru (accessed: January 14, 2015). DOI: 10.18577/2307-6046-2014-0-3-5-5.
  11. Donetskij K.I., Hrulkov A.V., Kogan D.I., Belinis P.G., Lukyanenko Yu.V. Primenenie obemno-armiruyushhih preform pri izgotovlenii izdelij iz PKM [Use of three-dimensional reinforcing preforms during the production of polymer composite products] // Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
  12. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  13. Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.Je., Ilin V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PCM] // Sb. dokl. IX Mezhdunar. nauch. konf. po gidroaviacii «Gidroaviasalon-2012». 2012. S. 122–123.
  14. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  15. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  16. Wood J.R., Bader M.G. Void control for polymer-matrix composites (1) theoretical and experimental methods for determining the growth and collapse of gas bubbles // Compos. Manuf. 1994. V. 5 (3). P. 139–147.
  17. Wood J.R., Bader M.G. Void control for polymer-matrix composites (1) theoretical and experimental evaluation of a diffusion model for the growth and collapse of gas bubbles // Compos. Manuf. 1994. V. 5 (3). P. 149–158.
  18. Liu L., Zhang B., Wang D., Wu Z. Effects of cure cycle on void content and mechanical properties of composite laminates // Compos. Struct. 2006. V. 73. P. 303–309.
  19. Liu L., Zhang B., Wu Z., Wang D. Effects of cure pressure induced voids on the mechanical strength of carbon/epoxy laminates // J. Mater. Sci. Technol. 2005. V. 21 (1). P. 87–91.
  20. Olivier P., Cottu J.P., Ferret B. Effects of cure cycle pressure and voids on some mechanical properties of carbon/epoxy laminates // Composites. 1995. V. 26 (7). P. 509–515.
  21. Huang H., Talreja R. Effects of void geometry on elastic properties of unidirectional fiber reinforced composites // Composites Science and Technology. 2005. V. 65. P. 1964–1981.
  22. Costa M.L., Almeida S.F.M., Rezende M.C. The influence of porosity on the interlaminar shear strength of carbon/epoxy and carbon/bismaleimide fabric laminates // Composites Science and Technology. 2001. V. 61. P. 2101–2108.
  23. Grunenfelder L.K., Nutt S.R. Void formation in composite prepregs – effect of dissolved moisture // Composites Science and Technology. 2010. V. 70. Р. 2304–2309.
  24. Kardos J.L., Dudukovic M.P., Dave R. Void growth and resin transport during processing of thermosetting-matrix composites // Adv. Polym. Sci. 1986. V. 80. P. 102–123.
  25. Boey F.Y.C., Lye S.W. Void reduction in autoclave processing of thermoset composites part 1: high pressure effects on void reduction // Composites. 1992. V. 23 (4). P. 261–265.
  26. Hayward J.S., Harris B. Effect of process variables on the quality of RTM mouldings // SAMPE J. 1990. V. 26 (3). P. 39–46.
  27. Dushin M.I., Hrulkov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Out-of-autoclave formation coal plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  28. Lundstrom T.S., Gebart B.R., Lundemo C.Y. Void formation in RTM // The 49th annual conference. Session 16-F. Composite Institute of the Society of the Plastics Industry. 1992.
  29. Patel N., Lee L.J. Effect of fiber mat architecture on void formation and removal in liquid composite molding // Polym. Compos. 1995. V. 16 (5). P. 386–399.
  30. Patel N., Rohatgi V., Lee L.J. Modeling of void formation and removal in liquid composite molding. Part II. Model development // Polym. Compos. 1996. V. 17 (1). P. 104–114.
  31. Chen Y.T., Davis H.T., Macosko C.W. Wetting of fiber mats for composite manufacturing: I. Visualization experiments. AlChE // J. Polym. Compos. 1995. V. 41 (10). P. 2261–2273.
  32. Patel N., Rohatgi V., Lee L.J. Micro scale flow behavior and void formation mechanism during impregnation through a unidirectional stitched fiberglass mat // Polym. Eng. Sci. 1995. V. 35 (10). P. 837–851.
  33. Rohatgi V., Patel N., Lee L.J. Experimental investigation of flow induced microvoids during impregnation of unidirectional stitched fiberglass mat // Polym. Compos. 1996. V. 17 (2). P. 161–170.
  34. Ruiz E., Achim V., Bread J., Chatel S., Trouchu F. A fast numerical approach to reduce voud formation in liquid composite molding // The 8th International Conference on Flow Processes in Composite Materials (FPCM8). Douai. 2006. P. 251–260.
  35. Bread J., Henzel Y., Trouch F., Gauvin R. Analysis of dynamic flow through porous media. Part I: Comparison between saturated and unsaturated flows in fibrous reinforcements // Polymer Composites. 2003. V. 24. №3. P. 409–421.
  36. Lee G.W., Lee K.J. Mechanism of void formation in composite processing with woven fabrics // Polymer and Polymer Composites. 2003. V. 11. №7. P. 563–570.
  37. Hayward J.S., Harris B. Effect of vacuum assistance in resin transfer moulding // Compos. Manuf. 1990. V. 1 (33). P. 161–166.
  38. Lykov A.V. Teoriya sushki [Drying theory]. M.: Energiya, 1968. 472 s.
  39. High-performance infusion system for VARTM fabrication: pat. 6964561 США; publ. 15.11.05.
  40. Method for making composite structures: pat. 6630095 US; publ. 07.10.03.
  41. Method and device for producing fibre-reinforced components using an injection method: пат. 1181149 EU; publ. 10.12.03.
  42. Sposob izgotovleniya voloknistyh kompozitov vakuumnoj infuziej i ustrojstvo dlya osushhestvleniya sposoba: pat. 2480335 PU [Way of manufacturing of fibrous composites vacuum infusion and the device for implementation of way: pat. 2480335 PU]; opubl. 27.04.13.