Porous-fibrous metallic material for sound-absorbing structures of aircraft GTE

Farafonov D.P., Migunov V.P., Degovets M.L., Alyoshina R.Sh.
Farafonov D.P., Migunov V.P., Degovets M.L., Alyoshina R.Sh. Porous-fibrous metallic material for sound-absorbing structures of aircraft GTE // Proceedings of VIAM. 2016. No. 4. DOI: 10.18577/2307-6046-2016-0-4-1-1. URL: https://viam-works.ru/en/journal/2016/4/1
Abstract

The article presents the results of VIAM efforts aimed at creating an effective sound-absorbing material made of metal fibers for high-temperature sound-absorbing structures of aviation gas turbine engines (SAS). Porous fibrous metal material (PFMM) is one of the most challenging materials for SAS. Their high level of the absorption properties, which are almost self-contained under stream sound pressure, can provide noise reduction within a wide frequency range of the sound vibrations. In addition to high acoustic efficiency of the sound absorbing materials for aircraft gas turbine engines they have to possess high heat and corrosion resistance, high strength with low specific weight. The results of VIAM studies show that with the help of the metal fibers it is possible to create the sound-absorbing material with the characteristics named above. Research is executed within implementation of the complex scientific direction 15.7. «Metal porous-fibrous materials for sound-proof struct

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Migunov V.P., Lomberg B.S. Poristovoloknistye metallicheskie materialy dlya zvukopogloshhayushhih i uplotnitelnyh konstrukcij [Poristovoloknistye metal materials for sound-proof and sealing designs] / V kn.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 270–275.
  3. Migunov V.P., Farafonov D.P., Degovets M.L. Poristovoloknistyj material sverhnizkoj plotnosti na osnove metallicheskih volokon [Porous fibrous material of ultralow density on the basis of metal fibers] // Aviacionnye materialy i tehnologii. 2012. №4. S. 38–41.
  4. Farafonov D.P., Migunov V.P. Izgotovlenie poristovoloknistogo materiala sverhnizkoj plotnosti dlya zvukopogloshhajushhih konstrukcij aviacionnyh dvigatelej [Manufacturing of porous fibrous material of ultralow density for sound-proof designs of aircraft engines] // Aviacionnye materialy i tehnologii. 2013. №4. S. 26–30.
  5. Sobolev A.F., Ushakov V.G., Filippova R.D. Zvukopogloshhayushhie konstrukcii gomogennogo tipa dlya kanalov aviacionnyh dvigatelej [Sound-proof designs of homogeneous type for channels of aircraft engines] // Akusticheskij zhurnal. 2009. T. 55. №6. S. 749–759.
  6. Haleckij Yu.D. Effektivnost kombinirovannyh glushitelej shuma aviacionnyh dvigatelej [Efficiency of the combined silencers of noise of aircraft engines] //Akusticheskij zhurnal. 2012. T. 58. №4. S. 556–562.
  7. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Litejnye konstrukcionnye splavy na osnove alyuminida nikelya [Cast structural alloys on the basis of nickel aluminide] // Dvigatel. 2010. №4. S. 24–25.
  8. Kablov E.N., Buntushkin V.P., Povarova K.B., Bazyleva O.A., Morozova G.I., Kazanskaya N.K. Malolegirovannye legkie zharoprochnye vysokotemperaturnye materialy na osnove intermetallida Ni3Al [The low-alloyed easy heat resisting high-temperature materials on the basis of Ni3Al intermetallic compound] // Metally. 1999. №1. S. 58–65.
  9. Kablov E.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye polifunkcionalnye vysokotemperaturnye pokrytiya dlya nikelevyh splavov, uplotnitelnyh metallicheskih voloknistyh materialov i berillievyh splavov [Modern multifunctional high temperature coatings for nickel alloys, sealing metal fibrous materials and beryllium alloys] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://www.viam-works.ru (accessed: July 30, 2015).
  10. Farafonov D.P., Degovets M.L., Serov M.M. Issledovanie svojstv i tehnologicheskih parametrov polucheniya metallicheskih volokon dlya istiraemyh uplotnitelnyh materialov aviacionnyh GTD [The investigation of the properties and technological parameters producing metallic fibers for abradable sealing materials of aircraft GTE] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №7. St. 02 Available at: http://viam-works.ru (accessed: July 30, 2015). DOI: 10.18577/2307-6046-2014-0-7-2-2.
  11. Fei W., Kuiry S.C., Seal S. Inhibition of Metastable Alumina Formation on Fe–Cr–Al–Y Alloy Fibers at High Temperature Using Titania Coating // Oxidation of Metals. 2004. V. 62. №1–2.
  12. P. 29–44.
  13. Leprince G., Alperine S., Vandenbulke L., Walder A. New high temperature-resistant NiCrAl and NiCrAl+Hf felt materials // Materials Science and Engineering: A. 1989. V. 120–121. part 2.
  14. P. 419–425.
  15. Solntsev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. SiC–Si3N4–SiO2 high temperature coatings for metal fibers sealing materials // Glass and ceramics. 2011. V. 68. №5–6. P. 194–196.
  16. Solntsev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytiya dlya uplotnitelnyh materialov iz metallicheskih volokon [High-temperature thin-film coverings for sealing materials from metal fibers] // Aviacionnye materialy i tehnologii. 2012. №1. S. 30–36.
  17. Migunov V.P., Farafonov D.P., Degovets M.L., Stupina T.I. Uplotnitelnye materialy dlya protochnogo trakta GTD [Sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 94–97.
  18. Migunov V.P., Farafonov D.P. Issledovanie osnovnyh ekspluatacionnyh svojstv novogo klassa uplotnitelnyh materialov dlya protochnogo trakta GTD [Research of the main operational properties of new class of sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.