Trends in alloying and microalloying of nickel-based single crystal superalloys (review)

Shein E.A.
Shein E.A. Trends in alloying and microalloying of nickel-based single crystal superalloys (review) // Proceedings of VIAM. 2016. No. 3. DOI: 10.18577/2307-6046-2016-0-3-2-2. URL: https://viam-works.ru/en/journal/2016/3/2
Abstract

Review of modern single crystal Ni-based alloys is presented, including their chemical composition, structure and properties. The influence of addition agents on the structure stability, formation of undesired phases and toughening mechanism as well as rare earth metals influence on the structure and high temperature properties of superalloys are shown.

Reference list
  1. Kablov E.N. Fiziko-himicheskie i tehnologicheskie osobennosti sozdaniya zharoprochnyh splavov, soderzhashhih renij [Physical and chemical and technological features of creation of the hot strength alloys, containing reny] // Vestnik Moskovskogo universiteta. Ser. 2.: Himiya. 2005. №3. S. 155–167.
  2. Kablov E.N. Zharoprochnye konstrukcionnye materialy [Heat resisting constructional materials] // Litejnoe proizvodstvo. 2005. №7. S. 2–7.
  3. Petrushin N.B., Svetlov I.L., Ospennikova O.G. Litejnye zharoprochnye nikelevye splavy [Cast heat resisting nickel alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №5. S. 15–19.
  4. Kuznecov V.P., Lesnikov V.P., Konakova I.P., Petrushin N.V., Muboyadzhyan S.A. Struktura i fazovyj sostav monokristallicheskogo splava VZhM4 s gazocirkulyacionnym zashhitnym pokrytiem [Structure and phase composition of VZhM4 single-crystal alloy with gas circulating protecting cover] // MiTOM. 2011. №3. S. 28–32.
  5. Kablov E.N., Demonis I.M., Petrushin N.V. Materials and Technologies for New Generation Aeroengines / In: 4th European Conference for Aerospace Sciences. Saint Petersburg. 2011.
  6. Petrushin N.B., Ospennikova O.G., Visik E.M., Rassohina L.I., Timofeeva O.B. Zharoprochnye nikelevye splavy nizkoj plotnosti [Heat resisting nickel alloys of low density] // Litejnoe proizvodstvo. 2012. №6. S. 5–11.
  7. Kablov E.N., Petrushin N.V., Elyutin E.S. Monokristallicheskie zharoprochnye splavy dlya gazoturbinnyh dvigatelej [Single-crystal hot strength alloys for gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 38–52.
  8. Tolorajya V.N., Orehov N.G., Lomberg B.S. Korrozionnostojkie zharoprochnye splavy dlya krupnogabaritnyh monokristal'nyh turbinnyh lopatok [Corrosion-resistant hot strength alloys for large-size single-crystal turbine blades] // MiTOM. 2003. №1. S. 30–32.
  9. Gerasimov V.V., Visik E.M., Kolyadov E.V. Ob osvoenii tehnologii polucheniya krupnogabaritnyh lityh lopatok s monokristallicheskoj strukturoj [About development of technology of receiving large-size cast blades with single-crystal structure] // Litejnoe proizvodstvo. 2014. №3. S. 29–32.
  10. Sidorov V.V., Rigin V.E., Goryunov A.V., Min P.G. Innovacionnaya tehnologiya proizvodstva zharoprochnogo splava ZhS32-VI s uchetom pererabotki vseh vidov othodov v usloviyah sertificirovannogo serijnogo proizvodstva FGUP «VIAM» [The innovation technology of high temperature GS32-VI alloy production considering the recycling of all scrap appearance at certificated quantity production of FGUP «VIAM»] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 01. Available at: http://www.viam-works.ru (accessed: February 15, 2015). DOI: 10.18577/2307-6046-2014-0-6-1-1.
  11. Min P.G., Sidorov V.V. Rafinirovanie othodov zharoprochnogo nikelevogo splava ZhS32-VI ot primesi kremniya v usloviyah vakuumnoj indukcionnoj plavki [Refining of scraps of Ni-base superalloy ZhS32-VI to eliminate silicon impurity under conditions of vacuum induction melting] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 01. Available at: http://www.viam-works.ru (accessed: February 15, 2015). DOI: 10.18577/2307-6046-2014-0-9-1-1.
  12. Kablov E.N., Tolorajya V.N., Demonis I.M., Orehov N.G. Napravlennaya kristallizaciya zharoprochnyh nikelevyh splavov [The directed crystallization of heat resisting nickel alloys] // Tehnologiya legkih splavov. 2007. №2. S. 60–70.
  13. Chubin Yang, Lin Liu, Xinbao Zhao, Yafeng Li, Jun Zhang, Hengzhi Fu. Dendrite morphology and evolution mechanism of nickel-based single crystal super alloys grown along the 001> and 011> orientations // Progress in Natural Science: Materials International. 2012. №22. P. 407–413.
  14. Fu Wang, Dexin Ma, Jun Zhang, Andreas Bührig-Polaczek. Investigation of segregation and density profiles in the mushy zone of CMSX-4 superalloys solidified during downward and upward directional solidification processes // Journal of Alloys and Compounds. 2015. №620. P. 24–30.
  15. Lee J.S., Gu J.H., Jung H.M., Kim E.H., Jung Y.G., Lee J.H. Directional Solidification Microstructure Control in CM247LC Superalloy //Materials Today: Proceedings. 2014. №1. P. 3–10.
  16. Gerasimov V.V., Visik E.M., Kolyadov E.V. Vzaimosvyaz formy fronta kristallizacii so strukturoj zharoprochnyh splavov v processe napravlennoj kristallizacii [The relationship shape of the crystallization front with the structure of heat-resistant alloys in the process of crystallization] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 02. Available at: http://www.viam-works.ru (accessed: February 15, 2015). DOI: 10.18577/2307-6046-2014-0-6-2-2.
  17. Simmonds S., D’Souza N., Ryder K.S., Dong H. Analysis of surface scale on the Ni-based superalloy CMSX-10N and proposed mechanism of formation // IOP Conf. Series: Materials Science and Engineering. 2011. №27.
  18. Xiong Jichun, Li Jiarong, Liu Shizhong. Surface Recrystallization in Nickel Base Single Crystal Superalloy DD6 // Chinese Journal of Aeronautics. 2010. №23. P. 478–485.
  19. Li Zhonglin, Xiong Jichun, Xu Qingyan, Li Jiarong, Liu Baicheng. Deformation and recrystallization of single crystal nickel-based superalloys during investment casting // Journal of Materials Processing Technology. 2015. №217. P. 1–12.
  20. Guang Xie, Jian Zhang, Lang-hong Lou. Effect of cyclic recovery heat treatment on surface recrystallization of a directionally solidified superalloy // Progress in Natural Science: Materials International. 2011. №21. P. 491–495.
  21. F. Wang, D.X. Ma, J. Zhang, S. Bogner, A. Bührig-Polaczek. A high thermal gradient directional solidification method for growing superalloy single crystals // Journal of Materials Processing Technology. 2014. V. 214. P. 3112–3121.
  22. Reed R.C. The Superalloys Fundamentals and Applications. Cambridge University Press. 2006. 390 p.
  23. Kupkovits R.A., Smith D.J., Neu R.W. Influence of minimum temperature on the thermomechanical fatigue of a directionally-solidified Ni-base superalloy // Procedia Engineering. 2010. №2. P. 687–696.
  24. Filippini M. Notched fatigue strength of single crystals at high temperature // Procedia Engineering. 2011. №10. P. 3787–3792.
  25. Amaro R.L., Antolovich S.D., Neu R.W., Staroselsky A. On thermo-mechanical fatigue in single crystal Ni-base superalloys // Procedia Engineering. 2010. №2. P. 815–824.
  26. Okazaki M., Sakaguchi M., Yamagishi S. Subcritical Crack Growth on Crystallographic Planes in a Ni-base Superalloy: Relevance to Orientations // Procedia Engineering. 2013. №55. P. 677–684.
  27. Xianfeng Ma, Huiji Shi, Jialin Gu, Guofeng Chen, Oliver Luesebrink, Harald Harders In-situ observations of the effects of orientation and carbide on low cycle fatigue crack propagation in a single crystal superalloy // Procedia Engineering. 2010. №2. P. 2287–2295.
  28. Leidermark D., Moverare J., Segersäll M., Simonsson K., Sjöström S., Johansson S. Evaluation of fatigue crack initiation in a notched singlecrystal superalloy component // Procedia Engineering. 2011. №10. P. 619–624.
  29. Johansson S., Moverare J., Leidermark D., Simonsson K., Kanesund J. Investigation of localized damage in single crystals subjected to thermalmechanical fatigue (TMF) // Procedia Engineering. 2010. №2. P. 657–666.
  30. Fu B., Zhang J., Harada H. Interaction between crack and twins in TMS-82 superalloy during thermomechanical fatigue process // Progress in Natural Science: Materials International. 2013. №23. P. 508–513.
  31. Staroselsky A., Cassenti Brice N. Creep, plasticity, and fatigue of single crystal superalloy // International Journal of Solids and Structures. 2011. №48. P. 2060–2075.
  32. Giraud R., Hervier Z., Cormier J., Gilles Saint-martin, Hamon F., Milhet X., Mendez J. Strain Effect on the γʹ Dissolution at High Temperatures of a Nickel-Based Single Crystal Superalloy // Metallurgical and materials transactions A. 2013. №44A. P. 131–146.
  33. Samal M.K., Ghosh S. Evaluation of Creep Deformation and Mechanical Properties of Nickel-based Superalloys through FE Analysis Based on Crystal Plasticity Models // Procedia Engineering. 2013. №55. P. 342–347.
  34. Haofang Sun, SuguiTian, NingTian, HuichenYu, Xianlin Meng Microstructure heterogeneity and creep damage of DZ125 nickel-based superalloy //Progress in Natural Science: Materials International. 2014. №24. P. 266–273.
  35. Wang L., Wang D., Liu T., Li X.W., Jiang W.G., Zhang G. Effect of minor carbon additions on the high-temperature creep behavior of a single-crystal nickel-based superalloy //Materials Characterization. 2015. №104. P. 81–85.
  36. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: February 15, 2015).
  37. Davis J.R. ASM specialty handbook: nickel, cobalt, and their alloys // ASM International. 2000. 421 p.
  38. Yu P., Wang W., Wang F. Influence of cyclic frequency on oxidation behavior of K38 superalloy with yttrium additions at 1273 K // Journal of Rare Earths. 2011. №2. P. 119–123.
  39. Shi Z., Liu S., Han M., Li J. Influence of yttrium addition on high temperature oxidation resistance of single crystal superalloy // Journal of Rare Earths. 2013. V. 31. №8. P. 795–799.
  40. Lia X.L., Heb S.M., Zhoua X.T., Zoua Y., Lia Z.J., Lib A.G., Yua X.H. Effects of rare earth yttrium on microstructure and properties of Ni–16Mo–7Cr–4Fe nickel-based superalloy // Materials Characterization. 2014. №95. P. 171–179.
  41. Song X., Wang L., Liu Y., Hui-ping M.A. Effects of temperature and rare earth content on oxidation resistance of Ni-based superalloy // Progress in Natural Science: Materials International. 2011. V. 21. №3. P. 227–235.
  42. Improved low sulfur nickel-base single crystal superalloy with ppm addition of lanthanum and yttrium: pat 2012036494 JP; publ. 23.02.12.
  43. Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah dlya lopatok gazovyh turbin (Prodolzhenie) [Reny in heat resisting nickel alloys for blades of gas turbines (Continuation)] // Materialovedenie. 2000. №3. S. 38–43.
  44. Shishkareva L.M., Kuz'mina N.A. Obzor metodik opredeleniya kachestva struktury monokristallicheskih otlivok zharoprochnyh splavov [Review of methods for determining the quality of the structure of single-crystal superalloy castings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №1. St. 06. Available at: http://www.viam-works.ru (accessed: February 15, 2015). DOI: 10.18577/2307-6046-2014-0-1-6-6.
  45. Mottura A., Reed R.C. What is the role of rhenium in single crystal superalloys? /In: MATEC Web of Conferences. 2014. V. 14. №01001. DOI: 10.1051/matecconf/20141401001.
  46. Liu B., Raabe D., Roters F., Arsenlis A. Interfacial dislocation motion and interactions in single-crystal superalloys // Acta Materialia. 2014. №79. P. 216–233.
  47. Zheng-Guang Liu, Chong-Yu Wang, Tao Yu G. Influence of Re on the propagation of a Ni/Ni3Al interface crack by molecular dynamics simulation // Modelling and Simulation in Materials Science and Engineering. 2013. V. 21. №4. DOI: 10.1088/0965-0393/21/4/045009.
  48. Du J.P., Wang C.Y., Yu T. Construction and application of multi-element EAM potential (Ni–Al–Re) in γ/γʹ Ni-based single crystal superalloys // Modelling and Simulation in Materials Science and Engineering. 2013. V. 21. №1. DOI: 10.1088/0965-0393/21/1/015007.
  49. Guoqing Zu, Lirong Liu, Tao Jin, Zhuangqi Hu. Effect of Ti on microstructural evolution of Re containing single crystal superallys // Procedia Engineering. 2012. №27. P. 969–975.
  50. Zhenxue Shi, Jiarong Li, Shizhong Liu. Effect of long term aging on microstructure and stress rupture properties of a nickel-based single crystal superalloy // Progress in Natural Science: Materials International. 2012. №22. P. 426–432.
  51. Li P., Li Q.Q., Jin T., Zhou Y.Z., Li J.G., Sun X.F., Zhang Z.F. Effect of Re on low-cycle fatigue behaviors of Ni-based single-crystal superalloys at 900°C // Materials Science & Engineering A. 2014. V. 603. P. 84–92.
  52. Yu X.X., Wang C.Y., Zhang X.N., Yan P., Zhang Z. Synergistic effect of rhenium and ruthenium in nickel-based single-crystal superalloys // Journal of Alloys and Compounds. 2014. №582.
  53. P. 299–304.
  54. Matuszewski K., Rettig R., Singer R.F. The effect of Ru on precipitation of topologically close packed phases in Re – containing Ni-base superalloys: Quantitative FIB-SEM investigation and 3D image modeling / In: MATEC Web of Conferences. 2014. V. 14. №09001. DOI: 10.1051/matecconf/20141409001.
  55. Jing-yang Chen, Qiang Feng, La-mei Cao, Zu-qing Sun. Influence of Ru addition on microstructure and stress-rupture property of Ni-based single crystal superalloys // Progress in Natural Science: Materials International. 2010. №20. P. 61–69.
  56. Chatterjee D., Hazari N., Das N. Influence of Ru Addition on Microstructure, Creep and Rupture Properties of Nickel-based DS Superalloy // Procedia Engineering. 2013. №55. P. 51–57.
  57. Medvedeva N.I., Ivanovskii A.L. Ab-initio study of Re and Ru effect on stability of TCP nanoparticles in Ni-based superalloys // Nanosystems: physics, chemistry, mathematics. 2014. №5.
  58. P. 486–493.
  59. Shi Q., Huo J., Cao L., Li J., Ding X., Zheng Y., Feng Q. Compositional effect on TCP phase formation in Ru-containing Ni-based single crystal superalloys / In: MATEC Web of Conferences. 2014. V. 14. №01002. DOI: 10.1051/matecconf/20141401002.
  60. Kamal Nayan Goswami, Mottura A. Can slow-diffusing solute atoms reduce vacancy diffusion in advanced high-temperature alloys? // Materials Science & Engineering A. 2014. №617. P. 194–199.
  61. Nobuyasu Tsuno, Satoshi Takahashi. Creep deformation behaviour of Rhenium free Ni-based single crystal superalloys LSC-15 / In: MATEC Web of Conferences. 2014. V. 14. №20002. DOI: 10.1051/matecconf/20141420002.
  62. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Nestesnennyj misfit v zharoprochnyh monokristallicheskih nikelevyh splavah [Unembarrassed misfit in heat resisting single-crystal nickel alloys] // Zavodskaya laboratoriya. Diagnostika materialov. 2011. T. 77. №11. S. 36–38.
  63. Nairong Sun, Lanting Zhang, Zhigang Li, Aidang Shan. The effect of microstructure on the creep behavior of a low rhenium-containing single crystal nickel-based superalloy // Materials Science and Engineering. A. 2014. №606. P. 175–186.
  64. Creep-resistant, Rhenium-free nickel base superalloy: pat. 20140119941 US; publ. 05.01.14.
  65. Jacqueline Wahl, Harris K. New single crystal superalloys – overview and update /MATEC Web of Conferences. 2014. V. 14. №17002. DOI: 10.1051/matecconf/20141417002.
  66. Monokristallicheskij splav na osnove Ni dlya lopatok turbin [Single-crystal alloy on the basis of Ni for blades of turbines]: pat. 2518838 Ros. Federaciya; opubl. 10.06.14.
  67. High strength Ni-based superalloy, and gas turbine using the same: pat. 2014074208 JP; publ. 04.24.14.
  68. Ni-based superalloy: pat. 2013053327 JP; publ. 03.21.13.
  69. Low rhenium single crystal superalloy for turbine blade and vane: pat. 2013119668 JP; publ. 06.17.13.
  70. Rhenium-free single crystal superalloy for turbine blade and vane application: pat. 2013108166 JP; publ. 06.06.13.
  71. Ni-based single crystal superalloy: pat. 8771440 US; publ. 07.08.14.
  72. Yoshihiro Kondo, Yuusuke Kubo, Nobuhiro Miura, Yoshinori Murata, and Akira Yoshinari. Creep properties of a new Re free single crystal Ni-based superalloy, NKH71 /In: MATEC Web of Conferences. 2014. 14. №20003. DOI: 10.1051/matecconf/20141420003.